Densification of reactive lime from limestone

被引:39
作者
Bhattacharya, TK [1 ]
Ghosh, A [1 ]
Das, SK [1 ]
机构
[1] Cent Glass & Ceram Res Inst, Refractories Div, Kolkata 700032, W Bengal, India
关键词
sintering; microstructure; hydration resistance; reactivity of lime;
D O I
10.1016/S0272-8842(00)00101-2
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Sintering of lime from natural limestone was carried out by a single stage (from natural carbonate) and double stage (from limestone converted hydroxide) process in the temperature range 1500 to 1650 degreesC. In double stage process hydroxides were activated by three different techniques through pre-calcination and hydration. Different techniques employed are air-quenching the powder after precalcination, furnace cooling and water quenching of powder. The air quenching process showed better densification. Incorporation of hydroxide into carbonate powder up to an extent of 25 wt.% showed maximum densification. Hydration resistance was related to densification and grain size of sintered lime. (C) 2001 Elsevier Science Ltd and Techna S.r.l. All rights reserved.
引用
收藏
页码:455 / 459
页数:5
相关论文
共 13 条
[1]  
Boynton RS, 1980, CHEM TECHNOLOGY LIME, P18
[2]   EQUILIBRIUM PARTIAL-PRESSURE OF MG, SIO, CA, AND CO IN CARBON-CONTAINING DOLOMA REFRACTORIES [J].
BREZNY, B .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1976, 59 (11-1) :529-530
[3]  
Burke J.E., 1958, RECRYSTALIZATION SIN, P120
[4]  
CARR D, 1975, LIMESTONE DOLOMITE I, P759
[5]   INITIAL SINTERING OF ALUMINA AND HEMATITE [J].
COBLE, RL .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1958, 41 (02) :55-62
[6]  
DEKEYSER WL, 1951, B SOC CHIM BELG, V60, P516
[7]   SINTERING OF ACTIVATED CAO [J].
DEKEYSER, WL ;
WOLLAST, R ;
DUVIGNEAUD, PH .
JOURNAL OF MATERIALS SCIENCE, 1969, 4 (11) :989-+
[8]  
GROPYANOV VM, 1923, OGNEUPORY, V9, P11
[9]  
LANA LW, 1990, CERAM B, V69, P1184
[10]   SINTERING OF SODIUM CHLORIDE [J].
MORGAN, CS ;
HALL, LL ;
YUST, CS .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1963, 46 (11) :559-560