Hardness studies and fracture behaviour on flux-grown YFeO3 single crystals

被引:15
作者
Bamzai, K
Kotru, PN
Wanklyn, BM
机构
[1] UNIV JAMMU,DEPT PHYS,JAMMU 180004,INDIA
[2] UNIV OXFORD,DEPT PHYS,CLARENDON LAB,OXFORD OX1 3PU,ENGLAND
关键词
D O I
10.1002/crat.2170310617
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
Results of Vickers' microhardness (H-v), fracture toughness (K-c), brittleness index (B-i) of (110) and (001) faces of flux-grown yttrium orthoferrite crystals: in the load range of 10-100 g, are given. The cracks are classified into Palmqvist and median types. The transition from Palmqvist to median type of cracks is shown to take place when the applied load exceeds 50 g. Application of the formula of NIHARA et al. for only median cracks leads to calculation of more precise values for fracture toughness and brittleness index than what was reported earlier (BAMZAI et al.) as an average value.
引用
收藏
页码:813 / 819
页数:7
相关论文
共 26 条
[21]   THE FORMATION OF CRACKS AS A RESULT OF PLASTIC FLOW [J].
STROH, AN .
PROCEEDINGS OF THE ROYAL SOCIETY OF LONDON SERIES A-MATHEMATICAL AND PHYSICAL SCIENCES, 1954, 223 (1154) :404-414
[22]  
TABER D, 1970, REV PHYS TECHNOL, V1, P145
[23]  
Wanklyn B. M., 1969, Journal of Crystal Growth, V5, P323, DOI 10.1016/0022-0248(69)90033-5
[24]  
WESTBROOK JH, 58RL2033 GE RES LAB
[25]   PHYSICAL PROPERTIES AND ATOMIC ARRANGEMENTS IN CRYSTALS [J].
WOOSTER, WA .
REPORTS ON PROGRESS IN PHYSICS, 1953, 16 :62-82
[26]  
WYTT R, 1974, METALS CERAMICS POLY, pCH5