Hardness studies and fracture behaviour on flux-grown YFeO3 single crystals

被引:15
作者
Bamzai, K
Kotru, PN
Wanklyn, BM
机构
[1] UNIV JAMMU,DEPT PHYS,JAMMU 180004,INDIA
[2] UNIV OXFORD,DEPT PHYS,CLARENDON LAB,OXFORD OX1 3PU,ENGLAND
关键词
D O I
10.1002/crat.2170310617
中图分类号
O7 [晶体学];
学科分类号
0702 ; 070205 ; 0703 ; 080501 ;
摘要
Results of Vickers' microhardness (H-v), fracture toughness (K-c), brittleness index (B-i) of (110) and (001) faces of flux-grown yttrium orthoferrite crystals: in the load range of 10-100 g, are given. The cracks are classified into Palmqvist and median types. The transition from Palmqvist to median type of cracks is shown to take place when the applied load exceeds 50 g. Application of the formula of NIHARA et al. for only median cracks leads to calculation of more precise values for fracture toughness and brittleness index than what was reported earlier (BAMZAI et al.) as an average value.
引用
收藏
页码:813 / 819
页数:7
相关论文
共 26 条
[1]  
BHATT DG, 1981, J AM CERAM SOC, V64, pC166
[2]   EVALUATION OF STRUCTURE AND HARDNESS OF PROCESSED PLASTICS BY VICKERS MICROHARDNESS TEST [J].
BOWMAN, J ;
BEVIS, M .
COLLOID AND POLYMER SCIENCE, 1977, 255 (10) :954-966
[3]  
BROOKES CA, 1975, J MATER SCI, V10, P2177
[4]  
CAHOON JR, 1971, METALL TRANS, V2, P1979
[5]   Crystal Growth and Magnetic Susceptibility of Some Rare-Earth Compounds Part 2 Magnetic Susceptibility Measurements on a Number of Rare-Earth Compounds [J].
Cashion, J. D. ;
Cooke, A. H. ;
Leask, M. J. M. ;
Thorp, T. L. ;
Wells, M. R. .
JOURNAL OF MATERIALS SCIENCE, 1968, 3 (04) :402-407
[6]  
DANIELS FW, 1949, T AM SOC METAL, V41, P419
[7]  
DAVISON JW, 1958, REP NAVAL RES LAB PR, V10
[8]  
EVANS AG, 1981, J AM CERAM SOC, V64, pC182
[9]   CRYSTALLOGRAPHIC STUDIES OF PEROVSKITE-LIKE COMPOUNDS .1. RARE EARTH ORTHOFERRITES AND YFEO3, YCRO3, YALO3 [J].
GELLER, S ;
WOOD, EA .
ACTA CRYSTALLOGRAPHICA, 1956, 9 (06) :563-568
[10]  
Hays C., 1973, Metallography, V6, P275, DOI 10.1016/0026-0800(73)90053-0