ac susceptibility study on R(2)Fe(14)B single crystals (R=Y,Pr,Nd,Sm,Gd,Tb,Dy,Ho,Er,Tm)

被引:34
|
作者
Kou, XC [1 ]
Grossinger, R [1 ]
Hilscher, G [1 ]
Kirchmayr, HR [1 ]
deBoer, FR [1 ]
机构
[1] UNIV AMSTERDAM,VAN DER WAALS ZEEMAN INST,NL-1018 XE AMSTERDAM,NETHERLANDS
来源
PHYSICAL REVIEW B | 1996年 / 54卷 / 09期
关键词
D O I
10.1103/PhysRevB.54.6421
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The temperature dependence of the ac susceptibility chi=chi'+i chi('') has been measured on R(2)Fe(14)B single crystals with R=Y, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, and Tm as a function of temperature in the temperature interval from 4.2 to 300 K, as a function of the strength of the applied ac field (up to 800 A/m), as a function of frequency (ranging from 5 to 1000 Hz), as well as the dependence on the crystallographic orientation. A reversible rotation of magnetic moments, excited by applying the field perpendicular to the easy magnetization direction, is found to be the principal contribution to the susceptibility (chi'). The energy loss is fairly small in this case (chi('')approximate to 0) When the external field is applied parallel to the easy magnetization direction, domain-wall movement is the main contribution to the susceptibility (chi') and to the energy loss (chi('')) For Nd2Fe14B, a peak in chi('')(T) is detected at 135 K, the spin-reorientation temperature, in a 5 Hz held of 40 A/m applied along the [001] direction. This peak disappears upon increasing the frequency or upon changing the crystallographic orientation of the crystal. In addition, an anomaly in the temperature dependence of the susceptibility is detected around 220 K for R(2)Fe(14)B single crystals with R=Pr, Nd, Sm, Tb, and Dy. The presence of this anomaly depends on the crystallographic orientation. It can only be detected when the external field is applied parallel to the [001] direction. For all frequencies used, the temperature dependence of chi' is completely different from that of chi('') The chi' values are nearly independent of the frequency in our measuring range from 5 to 1000 Hz. However, the chi('') values increase with increasing frequency when the field is applied along the easy magnetization direction and decrease when the field is applied perpendicular to the easy magnetization direction.
引用
收藏
页码:6421 / 6429
页数:9
相关论文
共 50 条
  • [21] Crystal structures of R2Pd2Pb (R = Y, La, Ce, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, Tm, and Lu) compounds
    Melnyk, G
    Kandpal, HC
    Gulay, LD
    Tremel, W
    JOURNAL OF ALLOYS AND COMPOUNDS, 2004, 370 (1-2) : 217 - 222
  • [22] Crystal structures of R2Pd2Pb (R = Y, La, Ce, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, Tm, and Lu) compounds
    Tremel, W. (tremel@mail.uni-mainz.de), 1600, Elsevier Ltd (370): : 1 - 2
  • [23] Atomistic study of rare-earth compounds R2Fe17 (R=Y, Ce, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, Tm, Lu) and Nd2Fe17Nx
    Hao, SQ
    Chen, NX
    Shen, J
    MODELLING AND SIMULATION IN MATERIALS SCIENCE AND ENGINEERING, 2002, 10 (04) : 425 - 435
  • [24] CRYSTAL-STRUCTURE OF RGANI COMPOUNDS (R=CE,PR,ND,SM,GD,TB,DY,HO,ER,TM,YB,LU,Y)
    YARMOLYUK, YP
    GRYN, YN
    GLADYSHEVSKY, EI
    DOPOVIDI AKADEMII NAUK UKRAINSKOI RSR SERIYA A-FIZIKO-MATEMATICHNI TA TECHNICHNI NAUKI, 1979, (09): : 771 - 775
  • [25] Crystal structure of R5CuPb3 (R=Y, La, Ce, Pr, Nd, Sm, Gd, Tb, Dy, Ho, Er, Tm, Lu) compounds
    Gulay, LD
    Stêpieñ-Damm, J
    Wolcyrz, M
    JOURNAL OF ALLOYS AND COMPOUNDS, 2001, 319 (1-2) : 148 - 153
  • [26] Crystal structures of R(Ag,Pb)3 (R=Y, Sm, Gd, Tb, Dy, Ho, Er, Tm) compounds
    Gulay, LD
    Wolcyrz, M
    JOURNAL OF ALLOYS AND COMPOUNDS, 2001, 319 (1-2) : 218 - 220
  • [27] Crystal structure of RCuPb (R=Y, Sm, Gd, Tb, Dy, Ho, Er, Tm, Lu) compounds
    Gulay, LD
    Stepien-Damm, J
    Wolcyrz, M
    JOURNAL OF ALLOYS AND COMPOUNDS, 2001, 315 (1-2) : 169 - 173
  • [28] Physical properties of ternary compounds RNiPb (R=Y, Sm, Gd, Tb, Dy, Ho, Er and Tm)
    Gulay, LD
    Hiebl, K
    JOURNAL OF ALLOYS AND COMPOUNDS, 2002, 339 (1-2) : 46 - 53
  • [29] Magnetic properties and magnetocaloric effect of R2Fe14B compounds with R = Y, Pr, Nd, Sm, Gd, Tb, Dy, Ho and High-Magnetic field phase transitions in the compounds with R = Gd, Dy
    Elkhneny, Rana M.
    Aly, Samy H.
    Yehia, Sherif
    Khedr, Doaa M.
    CRYOGENICS, 2022, 127
  • [30] Anisotropic magnefization studies of R2CoGa8 single crystals (R = Gd, Tb, Dy, Ho, Er, Tm, Y, and Lu)
    Joshi, Devang A.
    Nagalakshmi, R.
    Dhar, S. K.
    Thamizhavel, A.
    PHYSICAL REVIEW B, 2008, 77 (17):