Laboratory scale investigation to improve the productivity of stamp charge coke oven through optimisation of bulk density of coal cake

被引:23
作者
Dash, PS
Krishnan, SH
Sharma, R
Banerjee, PK
Haldar, SK
机构
[1] Tata Steel, Raw Mat & Cokemaking Res Grp, Res & Dev, Jamshedpur 831007, Jharkhand, India
[2] Tata Steel, Coke Plant, Jamshedpur 831001, Jharkhand, India
关键词
bulk density; coal cake stability; stamp charging; stamping energy; HGI; compressive strength; shear strength; specific gravity; ash; volatile matter;
D O I
10.2355/isijinternational.45.1577
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
In the recent past, it was realised that the gross coke yield was going down as a result of lower oven throughput in the stamp charged batteries of Tata Steel. The basic reason for this being the net reduction in the ash content of the coal blend used due to the incorporation of higher percentage of low ash imported coals and reduction in the ash content of captive coals through washing. The coals having higher ash content improves the bulk density, as the specific gravity of ash is higher than that of pure coal. Moreover, the ash components have affinity for water and pure coal repels water, which in case of pure coal, works against the holding together of the blend. Hence, lower the ash content, less is the bulk density of cake under identical stamping energy and lower the bulk density, less is the oven throughput. In order to maximise the oven throughput and productivity, a study was conducted in the laboratory mainly to assess the effect of various blend constituents and their ash content on the bulk density of coal charge. The effect of ash content on the coal cake stability has also been dealt with. This study, in short, is a useful tool for selecting the right type of coals and designing the optimum blend for stamp charging to achieve maximum throughput and productivity. In addition, studies were also carried out to assess the effect of addition of various binders on coal cake stability at lower moisture level which would also help in achieving higher throughput and productivity.
引用
收藏
页码:1577 / 1586
页数:10
相关论文
共 12 条
[1]  
BROSCHE H, 1925, BRENNST CHEM, V6, P33
[2]  
Bujnowska B., 1994, COKEMAKING INT, V6, P25
[3]   POSSIBILITIES OF TAR ADDITION TO COAL AS A METHOD OF IMPROVING COKE STRENGTH [J].
CHATTERJEE, A ;
PRASAD, HN .
FUEL, 1983, 62 (05) :591-600
[4]  
GURTOVNIK PF, 1982, COKE CHEM, V7, P24
[5]  
Kandler W., 1990, COKEMAKING INT, V1, P67
[6]  
KITAMURA M, 1982, 41 IR C P ISS WARR, P424
[7]   Application of binder in stamp charge coke making [J].
Krishnan, SH ;
Dash, RS ;
Guha, M ;
Kumar, D ;
Deshpande, DP .
ISIJ INTERNATIONAL, 2004, 44 (07) :1150-1156
[8]  
RAO PVT, 1994, TATA SEARCH, V1, P27
[9]  
Singh B. K., 1999, MONOGRAPHS STAMP CHA, P11
[10]  
SPENGLER H, 1991, COKEMAKING INT, V3, P25