Glass-ceramic oxidation protection of higher manganese silicide thermoelectrics

被引:16
|
作者
Salvo, M. [1 ]
Smeacetto, F. [1 ]
D'Isanto, F. [1 ]
Viola, G. [1 ]
Demitri, P. [1 ]
Gucci, F. [2 ,3 ]
Reece, M. J. [2 ,3 ]
机构
[1] Politecn Torino, Dept Appl Sci & Technol, Corso Duca Abruzzi 24, I-10129 Turin, Italy
[2] Queen Mary Univ London, Sch Engn & Mat Sci, Mile End Rd, London E1 4NS, England
[3] Queen Mary Univ London, Nanoforce Technol Ltd, Mile End Rd, London E1 4NS, England
关键词
Glass-ceramic; Coating; Thermoelectric; Oxidation; HIGH-TEMPERATURES; MODULES; RESISTANCE;
D O I
10.1016/j.jeurceramsoc.2018.01.007
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
A higher manganese silicide (HMS) thermoelectric, with composition MnSi1.74, densified by spark plasma sintering, was successfully coated with a glass-ceramic, in order to be used at temperatures higher than 500 degrees C, Compositional changes in both the HMS substrate and the glass-ceramic coating are reviewed and discussed with respect to the electrical properties of the uncoated and coated HMS before and after thermal cycles from RT to 600 degrees C in air. The formation of a Si-deficient layer (MnSi) on the uncoated HMS surface is due to the reaction between the HMS and oxygen at 600 degrees C, thus contributing to a lower power factor in comparison with the as sintered HMS. Coated HMS samples (after thermal cycles RT-600 degrees C) show a lower electrical resistivity and a significantly higher power factor in comparison with the uncoated ones. The glass-ceramic coating is self-reparable at 600 degrees C, as demonstrated by the complete sealing of an induced scratch on its surface.
引用
收藏
页码:66 / 71
页数:6
相关论文
共 50 条
  • [31] Structure and properties of ferrite/glass-ceramic nanocomposites
    Yue, ZX
    Zhou, J
    Zhang, HG
    Li, LT
    Gui, ZL
    JOURNAL OF INORGANIC MATERIALS, 1999, 14 (03) : 375 - 379
  • [32] Flexural strength of glass-ceramic for structural applications
    Collini, Luca
    Carfagni, Gianni Royer
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2014, 34 (11) : 2675 - 2685
  • [33] Bulk higher manganese silicide thermoelectric materials and modules
    Zhou, Aijun
    Cui, Hengguan
    Li, Jingze
    Zhu, Tiejun
    Zhao, Xinbing
    2011 CHINESE MATERIALS CONFERENCE, 2012, 27 : 94 - 102
  • [34] Influence of MoO3 on boron aluminosilicate glass-ceramic coating for enhancing titanium high-temperature oxidation resistance
    Yu, Fang
    Gu, Dongguang
    Zheng, Yifeng
    Luo, Yali
    Li, Xueyan
    Chen, Han
    Guo, Lucun
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 729 : 453 - 462
  • [35] Effect of ZrB2 and ZrO2 on the erosion/corrosion behavior of glass-ceramic coating
    Ak, Aykut
    Karaahmet, Oguz
    Cicek, Bugra
    MATERIALS TODAY COMMUNICATIONS, 2023, 36
  • [36] Glass and glass-ceramic sealants for solid oxide fuel cells (SOFC)
    Lara, C
    Pascual, MJ
    Durán, A
    BOLETIN DE LA SOCIEDAD ESPANOLA DE CERAMICA Y VIDRIO, 2003, 42 (03): : 133 - 143
  • [37] Abrasion-resistant CMAS glass-ceramic coatings incorporated with B4C particles
    Copoglu, Nurullah
    Karaahmet, Oguz
    Cicek, Bugra
    SURFACE ENGINEERING, 2022, 38 (05) : 541 - 551
  • [38] Comparison of the properties of glass, glass-ceramic and ceramic materials produced from coal fly ash
    Erol, M.
    Kucukbayrak, S.
    Ersoy-Mericboyu, A.
    JOURNAL OF HAZARDOUS MATERIALS, 2008, 153 (1-2) : 418 - 425
  • [39] In vitro biocompatibility of a ferrimagnetic glass-ceramic for hyperthermia application
    Bretcanu, Oana
    Miola, Marta
    Bianchi, Claudia L.
    Marangi, Ida
    Carbone, Roberta
    Corazzari, Ingrid
    Cannas, Mario
    Verne, Enrica
    MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS, 2017, 73 : 778 - 787
  • [40] Bioactivity and Biocompatibility of a Novel Wollastonite Glass-Ceramic Biomaterial
    Saadaldin, Selma A.
    Dixon, S. Jeffrey
    Rizkalla, Amin S.
    Journal of Biomaterials and Tissue Engineering, 2014, 4 (11) : 939 - 946