Sorption and Thermal Properties of Insulating Mortars with Expanded and Vitrified Small Ball

被引:3
作者
Fang, Ping [1 ]
Mukhopadhyaya, Phalguni [2 ]
Kumaran, Kumar [2 ]
Shi, Caijun [1 ]
机构
[1] Hunan Univ, Dept Civil Engn, Key Lab Bldg Safety & Energy Efficiency, Minist Educ, Changsha 410082, Hunan, Peoples R China
[2] Natl Res Council Canada, Inst Res Construct, Ottawa, ON K1A 0R6, Canada
关键词
expanded vitrified small hollow balls; expanded perlite particles; thermal insulating mortar; hygroscopic sorption properties; pore structure characteristics; LIGHTWEIGHT CONCRETE; PERLITE AGGREGATE; COMPRESSIVE STRENGTH; MINERAL ADMIXTURES; CONDUCTIVITY; DENSITY; CEMENT; RATIOS;
D O I
10.1520/JTE102678
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Expanded vitrified small hollow ball (EVSB), made from a special type of perlite mineral is one of the recently developed materials in China. It is widely used as a cementitious thermal insulating mortar for building envelope construction in hot-humid areas of southern China. However, EVSB is a porous material sensitive to environmental moisture. The thermal insulating property of the EVSB mortar is dependent on its moisture transport and storage characteristics. In this study, hygroscopic sorption properties of EVSB mortars have been investigated in comparison with those of normal expanded perlite particle (NEPP) mortars. The Brunauer, Emmett and Teller specific surface area and the Barrett, Joyner and Halenda pore size distribution, as well as the scanning electron microscope micromorphologies of the mortars were assessed. It was observed that EVSB mortars had lower moisture sorption capacity than NEPP mortars when the relative humidity (RH) was higher than 70% because of its lower total pore volume. The addition of water-repellent admixtures in the mortar decreased the moisture sorption capacity of EVSB mortars but still maintains the same physisorption isothermal characteristics. It is also evident that the thermal conductivity values of both NEPP and EVSB mortars increased rapidly when RH is above 90%. However, the increased rate of thermal conductivity of NEPP mortars was apparently higher than that of EVSB mortars. It is hoped that finding from this study will help to develop a better understanding of the in situ thermal performance of the EVSB mortar used for the building envelope construction in hot and humid areas of southern China.
引用
收藏
页码:210 / 218
页数:9
相关论文
共 22 条
[1]  
[Anonymous], 2004, ANN BOOK ASTM STAND, V4., P21
[2]  
[Anonymous], 2004, ANN BOOK ASTM STAND, V4., P155
[3]  
ASHWORTH T, 1991, AM SOC TEST MATER, V1116, P415, DOI 10.1520/STP16360S
[4]  
*ASTM INT, 2004, ANN BOOK ASTM STAND, P867
[5]   Water vapour sorption experiments on hardened cementitious materials - Part I: Essential tool for analysis of hygral behaviour and its relation to pore structure [J].
Baroghel-Bouny, Veronique .
CEMENT AND CONCRETE RESEARCH, 2007, 37 (03) :414-437
[6]   Characteristics and properties of lightweight concrete manufactured with cenospheres [J].
Blanco, F ;
García, P ;
Mateos, P ;
Ayala, J .
CEMENT AND CONCRETE RESEARCH, 2000, 30 (11) :1715-1722
[7]  
*BUILD MAT IND ASS, 2007, JCT10422007 BUILD MA
[8]   Effect of aggregate properties on the strength and stiffness of lightweight concrete [J].
Chi, JM ;
Huang, R ;
Yang, CC ;
Chang, JJ .
CEMENT & CONCRETE COMPOSITES, 2003, 25 (02) :197-205
[9]   An experimental research on the fluidity and mechanical properties of high-strength lightweight self-compacting concrete [J].
Choi, Yun Wang ;
Kim, Yong Jic ;
Shin, Hwa Cheol ;
Moon, Han Young .
CEMENT AND CONCRETE RESEARCH, 2006, 36 (09) :1595-1602
[10]   Thermal conductivity and compressive strength of expanded perlite aggregate concrete with mineral admixtures [J].
Demirboga, R ;
Gül, R .