Study of point-supported glass breakage behavior with varying point-covered areas under thermal loading

被引:5
|
作者
Lu, Wei [1 ]
Chen, Haodong [1 ]
Wang, Yu [2 ]
Duan, Qiangling [1 ]
Jiang, Lin [1 ]
Wang, Qingsong [1 ]
Sun, Jinhua [1 ]
机构
[1] Univ Sci & Technol China, State Key Lab Fire Sci, Hefei 230027, Anhui, Peoples R China
[2] Univ Edinburgh, BRE Ctr Fire Safety Engn, Sch Engn, Edinburgh EH9 3JL, Midlothian, Scotland
基金
中国博士后科学基金;
关键词
Point-supported glazing; Fire; Point-covered area; First breakage time; Stress field distribution; WINDOW GLASS; FRACTURE-BEHAVIOR; RADIANT EXPOSURE; FIRE CONDITIONS; CORNER FIRES; PERFORMANCE; SINGLE; TRANSMISSION; ENCLOSURE; FACADES;
D O I
10.1016/j.ijthermalsci.2018.05.045
中图分类号
O414.1 [热力学];
学科分类号
摘要
Point-supported glazing assemblies are widely used in modern buildings for aesthetic elegance, as well as for economic reasons. However, the formation of vents caused by glass breakage could aggravate ventilation controlled compartment fires. The point-covered area generally varies and may constitute potential fire hazards. Accordingly, it is necessary to investigate the fire performance and breakage mechanisms in various point covered areas. In this study, a total of 12 tests, including three various point-covered area glazing, were heated by a 200 x 200 mm(2) pool fire. The breakage time, glass surface and air temperatures, incident heat flux, and crack initiation and final fall out ratio were obtained. The critical conditions for the three aforementioned various point-covered area glazing were determined. The reference breakage times, t(r), which were calculated by assigning a failure probability of 0.1 to the two-parameter Weibull distribution were 119, 140, and 166 s. It was established that a relatively small point-covered area glazing can survive longer; the smaller the point-covered area was, the larger the final fallout ratio of glazing assemblies will be. Numerical simulations were performed to investigate the stress distribution on the glass pane, with breakage times well predicted. Accordingly, these results have implications on the fire resistance design for point-supported glazing assemblies.
引用
收藏
页码:65 / 75
页数:11
相关论文
共 23 条
  • [21] Study on behavior of waffle-type UHPC-GFRP composite slab under three-point loading
    Pang, Kun
    Zhou, Heying
    Wu, Chaolan
    Jiang, Haoting
    Zhang, Zhongya
    Yu, Yanjiang
    Zhang, Jiangtao
    CASE STUDIES IN CONSTRUCTION MATERIALS, 2023, 19
  • [22] Experimental Study of Static and Fatigue Behavior of CFRP-Balsa Sandwiches under Three-point Flexural Loading
    Zaharia, Sebastian Marian
    Morariu, Cristin Olimpiu
    Nedelcu, Anisor
    Pop, Mihai Alin
    BIORESOURCES, 2017, 12 (02): : 2673 - 2689
  • [23] Fatigue behavior of a Zr-based bulk metallic glass under uniaxial tension-tension and three-point bending loading mode
    Yue, Y.
    Wang, R.
    Ma, D. Q.
    Tian, J. F.
    Zhang, X. Y.
    Jing, Q.
    Ma, M. Z.
    Liu, R. P.
    INTERMETALLICS, 2015, 60 : 86 - 91