Stabilization of defects by the presence of hydrogen in tungsten: simultaneous W-ion damaging and D-atom exposure

被引:21
作者
Hodille, E. A. [1 ]
Markelj, S. [2 ]
Schwarz-Selinger, T. [3 ]
Zaloznik, A. [2 ]
Pecovnik, M. [2 ]
Kelemen, M. [2 ,4 ]
Grisolia, C. [5 ]
机构
[1] Univ Helsinki, Dept Phys, POB 43, FI-00014 Helsinki, Finland
[2] Jozef Stefan Inst, Jamova Cesta 39, Ljubljana 1000, Slovenia
[3] Max Planck Inst Plasma Phys, Boltzmannstr 2, D-85748 Garching, Germany
[4] Jozef Stefan Int Postgrad Sch, Jamova Cesta 39, Ljubljana 1000, Slovenia
[5] CEA, IRFM, F-13108 St Paul Les Durance, France
关键词
tungsten; deuterium retention; damage stabilization; displacement damage; NRA; TDS; DENSITY-FUNCTIONAL THEORY; DEUTERIUM RETENTION; DIFFUSION; ADSORPTION; IRRADIATION; ABSORPTION; W(110); FILMS;
D O I
10.1088/1741-4326/aaec97
中图分类号
O35 [流体力学]; O53 [等离子体物理学];
学科分类号
070204 ; 080103 ; 080704 ;
摘要
The possible mutual influence and synergistic effect between defect production and the presence of hydrogen isotopes in the crystal lattice of tungsten is studied. For this purpose, we perform modeling of experimental data where polycrystalline tungsten samples were in one case sequentially irradiated by 10.8 MeV tungsten ions followed by low-energy deuterium exposure and in the other case simultaneously irradiated by tungsten ions, while exposed to deuterium atoms. Modeling of the measured deuterium depth profiles and thermal-desorption spectra for different irradiation temperatures is performed by the MHIMS (migration of hydrogen isotopes in materials) code. A model of trap creation due to tungsten ion irradiation during the deuterium atom exposures is implemented. In both experimental series, the deuterium desorption peaks corresponding to defects induced by tungsten irradiation are described by the same two de-trapping energies of 1.83 and 2.10 eV. The experiments give unambiguous proof that the presence of deuterium increases the overall trap density. The modeling reveals that the two trap concentrations are affected differently by the temperature and presence of deuterium: the concentration of the low-energy trap is significantly higher in the case of simultaneous exposure compared to sequential exposure, especially at high temperature (2.2 times higher at 1000K). The concentration of the high-energy trap is only weakly affected by the presence of hydrogen.
引用
收藏
页数:11
相关论文
共 57 条
  • [21] Simulations of atomic deuterium exposure in self-damaged tungsten
    Hodille, E. A.
    Zaloznik, A.
    Markelj, S.
    Schwarz-Selinger, T.
    Becquart, C. S.
    Bisson, R.
    Grisolia, C.
    [J]. NUCLEAR FUSION, 2017, 57 (05)
  • [22] Macroscopic rate equation modeling of trapping/detrapping of hydrogen isotopes in tungsten materials
    Hodille, E. A.
    Bonnin, X.
    Bisson, R.
    Angot, T.
    Becquart, C. S.
    Layet, J. M.
    Grisolia, C.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2015, 467 : 424 - 431
  • [23] Hodille E. A., 2018, COMMUNICATION
  • [24] Hydrogen in tungsten: Absorption, diffusion, vacancy trapping, and decohesion
    Johnson, Donald F.
    Carter, Emily A.
    [J]. JOURNAL OF MATERIALS RESEARCH, 2010, 25 (02) : 315 - 327
  • [25] Dislocation-core symmetry and slip planes in tungsten alloys: Ab initio calculations and microcantilever bending experiments
    Li, Hong
    Wurster, Stefan
    Motz, Christian
    Romaner, Lorenz
    Ambrosch-Draxl, Claudia
    Pippan, Reinhard
    [J]. ACTA MATERIALIA, 2012, 60 (02) : 748 - 758
  • [26] Investigating behaviors of H in a W single crystal by first-principles: From solubility to interaction with vacancy
    Liu, Yue-Lin
    Zhou, Hong-Bo
    Zhang, Ying
    [J]. JOURNAL OF ALLOYS AND COMPOUNDS, 2011, 509 (33) : 8277 - 8282
  • [27] Longhurst G. R., 2004, INEELEXT042004 BWXT
  • [28] A review of modelling and simulation of hydrogen behaviour in tungsten at different scales
    Lu, Guang-Hong
    Zhou, Hong-Bo
    Becquart, Charlotte S.
    [J]. NUCLEAR FUSION, 2014, 54 (08)
  • [29] Recent advances in modeling and simulation of the exposure and response of tungsten to fusion energy conditions
    Marian, Jaime
    Becquart, Charlotte S.
    Domain, Christophe
    Dudarev, Sergei L.
    Gilbert, Mark R.
    Kurtz, Richard J.
    Mason, Daniel R.
    Nordlund, Kai
    Sand, Andrea E.
    Snead, Lance L.
    Suzudo, Tomoaki
    Wirth, Brian D.
    [J]. NUCLEAR FUSION, 2017, 57 (09)
  • [30] Deuterium retention in tungsten simultaneously damaged by high energy W ions and loaded by D atoms
    Markelj, S.
    Schwarz-Selinger, T.
    Zaloznik, A.
    Kelemen, M.
    Vavpetic, P.
    Pelicon, P.
    Hodille, E.
    Grisolia, C.
    [J]. NUCLEAR MATERIALS AND ENERGY, 2017, 12 : 169 - 174