A practical methodology to select fretting palliatives: Application to shot peening, hard chromium and WC-Co coatings

被引:24
作者
Kubiak, K
Fouvry, S
Marechal, AM
机构
[1] Ecole Cent Lyon, CNRS, UMR 5513, Lab Tribol & Dynam Syst, F-69134 Ecully, France
[2] SNCF, F-94407 Vitry Sur Seine, France
关键词
fretting; fatigue; Cr; WC-Co; friction; cracking; wear;
D O I
10.1016/j.wear.2005.01.030
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Considered as a plague for numerous industrial assemblies, fretting, associated to slight oscillatory displacement, is encountered in all quasi-static contacts subjected to vibration. Depending on sliding conditions, cracking or wear damage can be observed. During the past three decades there has been a huge development in surface treatments. Thousands of new surface treatments and coatings are now available. The critical challenge is to evaluate such treatments against fretting loadings. To achieve this objective, a fast fretting methodology has been developed. It consists in quantifying the palliative friction, cracking and wear responses through a very small number of fretting tests. By defining quantitative variables. a normalized polar fretting damage chart approach is introduced. Applied to shot peening, chromium coatings and WC-Co coatings, it demonstrates the potential benefit of a thermal sprayed WC-Co coating. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:367 / 376
页数:10
相关论文
共 19 条
[1]   The effect of rapidly varying contact stress fields on fretting fatigue [J].
Araújo, JA ;
Nowell, D .
INTERNATIONAL JOURNAL OF FATIGUE, 2002, 24 (07) :763-775
[2]   CONTACT AND RUBBING OF FLAT SURFACES [J].
ARCHARD, JF .
JOURNAL OF APPLIED PHYSICS, 1953, 24 (08) :981-988
[3]   BASIS OF A COATING CHOICE METHODOLOGY IN FRETTING [J].
CARTON, JF ;
VANNES, AB ;
VINCENT, L .
WEAR, 1995, 185 (1-2) :47-57
[4]   A quantitative approach of Ti-6Al-4V fretting damage:: friction, wear and crack nucleation [J].
Fouvry, S ;
Duó, P ;
Perruchaut, P .
WEAR, 2004, 257 (9-10) :916-929
[5]   Quantification of fretting damage [J].
Fouvry, S ;
Kapsa, P ;
Vincent, L .
WEAR, 1996, 200 (1-2) :186-205
[6]   An energy description of wear mechanisms and its applications to oscillating sliding contacts [J].
Fouvry, S ;
Liskiewicz, T ;
Kapsa, P ;
Hannel, S ;
Sauger, E .
WEAR, 2003, 255 :287-298
[7]   Impact of contact size and geometry on the lifetime of a solid lubricant [J].
Fridrici, V ;
Fouvry, S ;
Kapsa, P ;
Perruchaut, P .
WEAR, 2003, 255 (7-12) :875-882
[8]   Effect of shot peening on the fretting wear of Ti-6Al-4V [J].
Fridrici, V ;
Fouvry, S ;
Kapsa, P .
WEAR, 2001, 250 :642-649
[9]  
HOEPPNER DW, 1992, AM SOC TEST MATER, V1159, P23, DOI 10.1520/STP25809S
[10]   LUBRICATED FRETTING WEAR OF A HIGH-STRENGTH EUTECTOID STEEL ROPE WIRE [J].
MCCOLL, IR ;
WATERHOUSE, RB ;
HARRIS, SJ ;
TSUJIKAWA, M .
WEAR, 1995, 185 (1-2) :203-212