Improvement of elevated-temperature strength and recrystallization resistance via Mn-containing dispersoid strengthening in Al-Mg-Si 6082 alloys

被引:76
作者
Li, Chen [1 ]
Liu, Kun [1 ]
Chen, X-Grant [1 ]
机构
[1] Univ Quebec Chicoutimi, Dept Appl Sci, Chicoutimi, PQ G7H 2B1, Canada
来源
JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY | 2020年 / 39卷
基金
加拿大自然科学与工程研究理事会;
关键词
Al-Mg-Si; 6082; alloy; Mn addition; Dispersoid precipitation; Elevated-temperature strength; Recrystallization resistance; MECHANICAL-PROPERTIES; HEAT-TREATMENT; CREEP RESISTANCE; ALUMINUM-ALLOY; MICROSTRUCTURE; BEHAVIOR; PRECIPITATION; DEFORMATION; EVOLUTION; SC;
D O I
10.1016/j.jmst.2019.08.027
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The precipitation behavior of Mn-containing dispersoids in Al-Mg-Si 6082 alloys with different Mn contents (0, 0.5 and 1.0 wt%) during various heat treatments (300-500 degrees C) was investigated. The effects of dispersoids on elevated-temperature strength and recrystallization resistance during hot-rolling and post-rolling annealing were evaluated. The results showed that the dispersoids in the Mn-containing alloys (0.5 and 1.0%) began to precipitate at 350 degrees C and reached the optimum conditions after 2-4h at 400 degrees C. However, the dispersoids coarsened with increasing holding time at temperatures above 450 degrees C. After the peak precipitation treatment at 400 degrees C for 2 h, the yield strength at 300 degrees C increased from 28 MPa (base alloy free of Mn) to 55 MPa (alloy with 0.5% Mn) and 70 MPa (alloy with 1% Mn), respectively, demonstrating a significant dispersoid strengthening effect at elevated temperature. In addition, the dispersoids were thermally stable at 300 degrees C for up to 1000 h holding owing to its relative high precipitation temperature (350-400 degrees C), leading to the superior constant mechanical performance at elevated temperature during the long service life. During hot rolling and post-rolling annealing, the presence of a large amount of dispersoids results in the higher Zener drag P-z compared with base alloy and then significantly improved the recrystallization resistance. The alloy containing 0.5% Mn exhibited the highest recrystallization resistance among three experimental alloys studied during the post-rolling process, likely resulted from the lower coarsening rate of dispersoids and the lower dispersoids free zone. (C) 2020 Published by Elsevier Ltd on behalf of The editorial office of Journal of Materials Science & Technology.
引用
收藏
页码:135 / 143
页数:9
相关论文
共 33 条
[31]   The effect of Mn and Zr dispersoid-forming additions on recrystallization resistance in Al-Cu-Li AA2198 sheet [J].
Tsivoulas, D. ;
Prangnell, P. B. .
ACTA MATERIALIA, 2014, 77 :1-16
[32]   The effect of heat treatment on Mg2Si coarsening in aluminum 6105 alloy [J].
Usta, M ;
Glicksman, ME ;
Wright, RN .
METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2004, 35A (02) :435-438
[33]   Evolution of Elevated-Temperature Strength and Creep Resistance during Multi-Step Heat Treatments in Al-Mn-Mg Alloy [J].
Wang, G. S. ;
Liu, K. ;
Wang, S. L. .
MATERIALS, 2018, 11 (07)