A study on the electrode characteristics of V-Ti alloy surface-modified by ballmilling process

被引:5
|
作者
Kim, SH [1 ]
Lee, SM [1 ]
Lee, PS [1 ]
Lee, JY [1 ]
机构
[1] Korea Adv Inst Sci & Technol, Dept Mat Sci & Engn, Hyperstructured Organ Mat Res Ctr, Taejon 305701, South Korea
关键词
D O I
10.1149/1.1374443
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
V-Ti alloys have not been used as anode material of Ni/MH batteries because of their inability to charge/discharge in KOH electrolyte. Ni, a catalyst for hydrogen absorption/desorption in KOH electrolyte, was added to V-Ti alloy as a catalyst by the ballmilling process. The discharge capacity varied with ballmilling conditions such as ballmilling time lund Ni content. In particular, increasing ballmilling time leads to an effective alloyed surface, but a decreasing number of interstitial sites for hydrogen storage in the V-Ti alloy by structural damage of the alloy. The nickel powder alone was ballmilled causing a change in shape from spherical to Rake-type and inducing strain, as measured by X-ray diffraction. Therefore. Ni powder had a large surface area that increased the contact area of surface alloying and high activity of the surface alloying reaction. Comparing the ballmilling condition for Rake Ni with that for sphere Ni, the optimum ballmilling time was decreased so that the number of interstitial sites for hydrogen storage was nearly unchanged. Because of such a large hydrogen storage capacity to be dischargeable electrochemically, the maximum discharge capacity was 439 mAh/g. (C) 2001 The Electrochemical Society.
引用
收藏
页码:A696 / A700
页数:5
相关论文
共 50 条
  • [21] Wear resistance of surface-modified TiNbSn alloy
    M. Hatakeyama
    N. Masahashi
    Y. Michiyama
    H. Inoue
    S. Hanada
    Journal of Materials Science, 2021, 56 : 14333 - 14347
  • [22] Wear resistant surface-modified aluminum alloy
    Osaka Univ, Osaka, Japan
    Mater Sci Forum, pt 3 (1655-1660):
  • [23] Wear resistant surface-modified aluminum alloy
    Nakata, K
    Hashimoto, T
    Lee, KC
    Matsuda, F
    ALUMINIUM ALLOYS: THEIR PHYSICAL AND MECHANICAL PROPERTIES, PTS 1-3, 1996, 217 : 1655 - 1660
  • [24] Wear resistance of surface-modified TiNbSn alloy
    Hatakeyama, M.
    Masahashi, N.
    Michiyama, Y.
    Inoue, H.
    Hanada, S.
    JOURNAL OF MATERIALS SCIENCE, 2021, 56 (25) : 14333 - 14347
  • [25] Surface-modified carbon black for As(V) removal
    Borah, Dipu
    Satokawa, Shigeo
    Kato, Shigeru
    Kojima, Toshinori
    JOURNAL OF COLLOID AND INTERFACE SCIENCE, 2008, 319 (01) : 53 - 62
  • [26] Nonhydrolytic surface synthesis of a heterobimetallic V-Ti alkoxide complex on silica
    Rice, GL
    Scott, SL
    CHEMISTRY OF MATERIALS, 1998, 10 (02) : 620 - 625
  • [27] REDOX CONVERSION OF PEROXIDASE ON SURFACE-MODIFIED GOLD ELECTRODE
    RAZUMAS, VJ
    GUDAVICIUS, AV
    KULYS, JJ
    JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1983, 151 (1-2): : 311 - 315
  • [28] INFRARED STUDY OF AMMONIA AND PYRIDINE ADSORPTION ON V-TI OXIDE
    MIYATA, H
    NAKAGAWA, Y
    ONO, T
    KUBOKAWA, Y
    CHEMISTRY LETTERS, 1983, (08) : 1141 - 1144
  • [29] Evaluation of surface-modified Ti-6Al-4V alloy by combination of plasma-carburizing and deep-rolling
    Tsuji, N.
    Tanaka, S.
    Takasugi, T.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2008, 488 (1-2): : 139 - 145
  • [30] LUMINESCENT PROPERTIES OF A SURFACE-MODIFIED CADMIUM SELENIDE ELECTRODE
    VANRYSWYK, H
    JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1985, 132 (01) : C11 - C13