Dissolution behaviour of MgO based refractories in CaO-Al2O3-SiO2 slag

被引:28
|
作者
Huang, F. [1 ]
Liu, C. [1 ]
Maruoka, N. [2 ]
Kitamura, S. -Y. [2 ]
机构
[1] Univ Sci & Technol Beijing, Sch Met & Ecol Engn, Beijing 100083, Peoples R China
[2] Tohoku Univ, Inst Multidisciplinary Res Adv Mat, Aoba Ku, Sendai, Miyagi 9808577, Japan
基金
中国国家自然科学基金;
关键词
Dissolution; Refractory; MgO-C; MgO-Cr2O3; Slag; STAINLESS-STEEL SLAGS; DEGRADATION MECHANISMS; CORROSION; PARTICLES; OXIDE;
D O I
10.1179/1743281215Y.0000000003
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Magnesium oxide (MgO) based refractories are widely used in secondary refining processes, and their dissolution into refining slag is the primary cause of their shortened lifespan. The dissolution rate was investigated for sintered MgO and commercial MgO-C and MgO-Cr2O3 refractories in a synthesised 50CaO-45Al(2)O(3)-5SiO(2) liquid (mass-%) slag. The change in slag composition was measured after a refractory sample was placed into the molten slag that was stirred by flowing argon gas at 1773 K. The dissolution rate of the sintered MgO was above those of the MgO-C and MgO-Cr2O3 refractories under the same gas flowrate, although the dissolution rate of all samples increased as the gas flowrate was increased from 25 to 75 mL.min(-1). The slag containing 5 mass-% FeO considerably promoted the dissolution of the MgO-C refractory because of the oxidation of carbon by FeO. The dissolution of all the refractories was greatly affected by penetration of the liquid slag, with the mass transfer of MgO in the penetrating slag at lower gas flowrates likely being the rate controlling step. At high gas flowrates, Ar bubbles covered the surface and blocked the contact between the liquid slag and the solid phase, reducing the dissolution rate.
引用
收藏
页码:553 / 560
页数:8
相关论文
共 50 条
  • [1] Dissolution of MgO based refractories in CaO-Al2O3-MgO-SiO2 slag
    Wang, Huijun
    Caballero, Roberto
    Sichen, Du
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2018, 38 (02) : 789 - 797
  • [2] Dissolution and diffusion of TiO2 in the CaO-Al2O3-SiO2 slag
    Zhong-shan Ren
    Xiao-jun Hu
    Xin-mei Hou
    Xiang-xin Xue
    Kuo-chih Chou
    International Journal of Minerals, Metallurgy, and Materials, 2014, 21 : 345 - 352
  • [3] Deep learning revealed statistics of the MgO particles dissolution rate in a CaO-Al2O3-SiO2-MgO slag
    Chamasemani, Fereshteh Falah
    Lenzhofer, Florian
    Brunner, Roland
    SCIENTIFIC REPORTS, 2024, 14 (01):
  • [4] Dissolution and diffusion of TiO2 in the CaO-Al2O3-SiO2 slag
    Zhong-shan Ren
    Xiao-jun Hu
    Xin-mei Hou
    Xiang-xin Xue
    Kuo-chih Chou
    International Journal of Minerals Metallurgy and Materials, 2014, 21 (04) : 345 - 352
  • [5] Dissolution and diffusion of TiO2 in the CaO-Al2O3-SiO2 slag
    Ren, Zhong-shan
    Hu, Xiao-jun
    Hou, Xin-mei
    Xue, Xiang-xin
    Chou, Kuo-chih
    INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2014, 21 (04) : 345 - 352
  • [6] Effect of varying Al2O3 contents of CaO-Al2O3-SiO2 slags on lumped MgO dissolution
    Kim, Yelim
    Kashiwaya, Yoshiaki
    Chung, Yongsug
    CERAMICS INTERNATIONAL, 2020, 46 (05) : 6205 - 6211
  • [7] Corrosion of spinel clinker by CaO-Al2O3-SiO2 ladle slag
    Cho, MK
    Hong, GG
    Lee, SK
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2002, 22 (11) : 1783 - 1790
  • [8] Dissolution of CaO in SiO2-CaO-Al2O3 Slag in Si Production
    Folstad, Marit Buhaug
    Einarsrud, Kristian Etienne
    Tangstad, Merete
    METALS, 2024, 14 (02)
  • [9] SULFIDE CAPACITIES OF CAO-AL2O3-MGO AND CAO-AL2O3-SIO2 SLAGS
    HINO, M
    KITAGAWA, S
    BANYA, S
    ISIJ INTERNATIONAL, 1993, 33 (01) : 36 - 42
  • [10] Effect of Na2O on Dissolution Rate of Alumina in CaO-Al2O3-MgO-SiO2 Slag
    Shu, Qifeng
    Wang, Yanfei
    Li, Jiangling
    Liu, Yang
    Li, Pengfei
    Chou, Kuochih
    ISIJ INTERNATIONAL, 2015, 55 (11) : 2297 - 2303