Synthesis and characterization of polyurethane foams derived of fully renewable polyester polyols from sorbitol

被引:35
作者
Furtwengler, Pierre [1 ]
Perrin, Remi [2 ]
Redl, Andreas [3 ]
Averous, Luc [1 ]
机构
[1] Univ Strasbourg, BioTeam ICPEES ECPM, UMR CNRS 7515, 25 Rue Becquerel, F-67087 Strasbourg 2, France
[2] Soprema, 14 Rue St Nazaire, F-67025 Strasbourg 1, France
[3] Tereos, ZI & Portuaire, BP 32, F-67390 Marckolsheim, France
关键词
Sorbitol; Esterification; Polyurethane; Polyester; Foam; OIL-BASED POLYOL; P-31; NMR-SPECTROSCOPY; POLYISOCYANURATE FOAMS; CATALYTIC PRODUCTION; RECENT PROGRESS; VEGETABLE-OILS; SUGAR ALCOHOLS; GLYCEROL; BIOMASS; PERFORMANCE;
D O I
10.1016/j.eurpolymj.2017.10.020
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
This work globally redesigns the conventional approach in obtaining polyurethane foams (PUF), from sorbitol. Fully biobased polyester polyols were synthesized from sorbitol, adipic or succinic acid and different renewable C2 to C12 diols as the first step towards the elaboration of PUF. Sorbitol-based polyester polyols were synthesized through a two-step esterification without catalyst. The absence of a catalyst limits some side reactions and focuses the reaction on the primary hydroxyl groups of the sorbitol, to obtain the linear molecular structure. The global yields of the corresponding esterifications were above 80%. Hydroxyl values and acid values of the corresponding linear biobased polyester polyols ranged from 440 to 683 mg KOH/g, and from 11 to 49 mg KOH/g, respectively. Acid values were decreased below 10 mg KOH/g by neutralization. PUF were prepared with polyols blends containing this biobased polyester polyol (up to 75 wt%) and a conventional fossil based polyol e.g., oxypropylated glycerol, which present a high fossil content. The fmal biobased content of the PUF ranged up to 28 wt% in contrast to 9 wt% for the reference. Then the addition of neat glycerol to the polyol blend increased the final biobased contents of the PUF foams up to 31 wt%. In contrast with the traditional approach consisting of modifying the catalyst content, the activation of the reactive foaming process was improved through initial polyols blends. The final biobased PUF foaming kinetic was similar to that of the polyether polyol, used as a reference. Finally, the effects of chemical and physical blowing agents (water vs. isopentane) were compared on the foaming rate and foam structure. The use of chemical blowing agent efficiently decreased the foam gel time of 33% and increased the foaming rate of 1 mm/s with biobased systems. Besides, the polyols architecture has a strong influence on the foam tack free time which varied from 50 to 235 s for the studied PUF.
引用
收藏
页码:319 / 327
页数:9
相关论文
共 52 条
[1]   Impact of the hard-segment concentration on highly resilient polyurethane foams based on palm olein polyol [J].
Adnan, Srihanum ;
Noor, Maznee T. I. Tuan ;
Ain, Nurul H. ;
Devi, Kosheela P. P. ;
Mohd, Norhisham S. ;
Kian, Yeong Shoot ;
Idris, Zainab B. ;
Campara, Irma ;
Schiffman, Christi M. ;
Pietrzyk, Karol ;
Sendijarevic, Vahid ;
Sendijarevic, Ibrahim .
JOURNAL OF APPLIED POLYMER SCIENCE, 2017, 134 (45)
[2]   Utilization of renewable bio-based resources, viz. sorbitol, diol, and diacid, in the preparation of two pack PU anticorrosive coatings [J].
Anand, Abhijeet ;
Kulkarni, Ravindra D. ;
Patil, Chandrashekhar K. ;
Gite, Vikas V. .
RSC ADVANCES, 2016, 6 (12) :9843-9850
[3]   Preparation and properties of eco-friendly two pack PU coatings based on renewable source (sorbitol) and its property improvement by nano ZnO [J].
Anand, Abhijeet ;
Kulkarni, R. D. ;
Gite, V. V. .
PROGRESS IN ORGANIC COATINGS, 2012, 74 (04) :764-767
[4]   Anisotropy of the stiffness and strength of rigid low-density closed-cell polyisocyanurate foams [J].
Andersons, J. ;
Kirpluks, M. ;
Stiebra, L. ;
Cabulis, U. .
MATERIALS & DESIGN, 2016, 92 :836-845
[5]   Biomass-Based Polyols through Oxypropylation Reaction [J].
Aniceto, Jose P. S. ;
Portugal, Ines ;
Silva, Carlos M. .
CHEMSUSCHEM, 2012, 5 (08) :1358-1368
[6]   Advanced biobased and rigid foams, based on urethane-modified isocyanurate from oxypropylated gambier tannin polyol [J].
Arbenz, Alice ;
Frache, Alberto ;
Cuttica, Fabio ;
Averous, Luc .
POLYMER DEGRADATION AND STABILITY, 2016, 132 :62-68
[7]   Synthesis and characterization of fully biobased aromatic polyols - oxybutylation of condensed tannins towards new macromolecular architectures [J].
Arbenz, Alice ;
Averous, Luc .
RSC ADVANCES, 2014, 4 (106) :61564-61572
[8]   P-31 NMR IN WOOD CHEMISTRY - A REVIEW OF RECENT PROGRESS [J].
ARGYROPOULOS, DS .
RESEARCH ON CHEMICAL INTERMEDIATES, 1995, 21 (3-5) :373-395
[9]   Technology development for the production of biobased products from biorefinery carbohydrates-the US Department of Energy's "Top 10" revisited [J].
Bozell, Joseph J. ;
Petersen, Gene R. .
GREEN CHEMISTRY, 2010, 12 (04) :539-554
[10]   Cell morphology and mechanical properties of rigid polyurethane foam [J].
Cameron Hawkins, Michelle ;
O'Toole, Brendan ;
Jackovich, Dacia .
JOURNAL OF CELLULAR PLASTICS, 2005, 41 (03) :267-285