Changes in the Inter- and Intra- Fibrillar Structure of Lyocell (TENCEL®) Fibers after KOH Treatment

被引:12
作者
Ozturk, Hale Bahar [1 ]
Abu-Rous, Mohammad [2 ]
MacNaughtan, Bill [3 ]
Schuster, K. Christian [2 ]
Mitchell, John R. [3 ]
Bechtold, Thomas [1 ]
机构
[1] Univ Innsbruck, Res Inst Text Chem & Text Phys, Christian Doppler Lab Text & Fiber Chem Cellulosi, Hoechsterstr 73, A-6850 Dornbirn, Austria
[2] Textile Innovat, A-4860 Lenzing, Austria
[3] Univ Nottingham, Sch Biol Sci, Div Food Sci, Loughborough, Leics, England
来源
UTILIZATION OF LIGNOCELLULOSIC MATERIALS | 2010年 / 294-II卷
关键词
cellulose; fibers; lyocell; structure; swelling; ALKALI-METAL HYDROXIDES; CELLULOSIC FIBERS; PORE STRUCTURE; SPLITTING TENDENCY; FINE-STRUCTURE; COTTON FIBERS; PART; CHROMATOGRAPHY; MERCERIZATION; MORPHOLOGY;
D O I
10.1002/masy.200900027
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Lyocell fibers were treated with KOH up to 8 M which was demonstrated to distribute homogeneously at the outer zones of fiber cross section compared to NaOH which accesses more deeply but less homogenously. Both NaOH and KOH solutions can be used to lower significantly the fibrillation of lyocell fibers. However, due to intrafibrillar swelling together with deep penetration ability of alkali seen for NaOH treatments results in great fiber tensile strength loss which is not observed for KOH treatments due to its inability to penetrate the fiber completely. The porous structure of fibers was studied by inverse size exclusion chromatography (ISEC) to identify mean pore diameter, total pore area and accessible pore volume (APV). Mean pore diameter of fibers decreased after KOH treatments which did not change after NaOH treatments. Wide angle X-ray diffraction analyses (WAXD) were applied to identify the crystallinity index and crystallite size. In general, fiber properties such as water retention value, carboxyl content using methylene blue sorption method, depth of color measured after dyeing with C.I Direct Red 81 and weight loss were distinctly different in the ranges up to 2 M, 2-5 M and 5 to 8 M KOH. KOH treatment suggests new possibilities for the pretreatment of lyocell fibers to lower fibrillation while slightly lowering elongation at break without a distinct loss in tensile strength and with less decrease in carboxyl content and weight loss without changing dyeing properties of fibers compared to NaOH treatment.
引用
收藏
页码:24 / +
页数:2
相关论文
共 50 条
[1]   A new method to visualize and characterize the pore structure of TENCEL® (Lyocell) and other man-made cellulosic fibres using a fluorescent dye molecular probe [J].
Abu-Rous, Mohammad ;
Varga, Ksenija ;
Bechtold, Thomas ;
Schuster, Kurt Christian .
JOURNAL OF APPLIED POLYMER SCIENCE, 2007, 106 (03) :2083-2091
[2]   Visualisation of the fibrillar and pore morphology of cellulosic fibres applying transmission electron microscopy [J].
Abu-Rous, Mohammad ;
Ingolic, Elisabeth ;
Schuster, Kurt Christian .
CELLULOSE, 2006, 13 (04) :411-419
[3]  
ANTWUORINEN O, 1958, PAPPERMACH TRA, V6, P313
[4]   EFFECT OF SCOURING BLEACHING, CAUSTIC MERCERIZATION, AND LIQUID-AMMONIA TREATMENT ON THE PORE STRUCTURE OF COTTON TEXTILE FIBERS [J].
BERTONIERE, NR ;
KING, WD .
TEXTILE RESEARCH JOURNAL, 1989, 59 (02) :114-121
[5]  
BREDERECK K, 2003, MELLIAND TEXTILBERIC, V1, P58
[6]  
BREDERECK K, 1992, MELLIAND TEXTILBERIC, V73, P652
[7]   AN EQUILIBRIUM THEORY FOR EXCLUSION CHROMATOGRAPHY OF BRANCHED AND LINEAR POLYMER CHAINS [J].
CASASSA, EF ;
TAGAMI, Y .
MACROMOLECULES, 1969, 2 (01) :14-+
[8]  
DARUWALLA EH, 1963, TEXT RES J, P33
[9]  
DEGUZMAN EV, 1988, Patent No. 283114
[10]  
DIMICK BE, 1976, THESIS LAWRANCE U WI