Microstructure and mechanical properties of laser-deposited Ti65 near-alpha titanium alloy

被引:13
作者
He, Bo [1 ]
Sun, Junfeng [1 ]
Yang, Guang [1 ]
Li, Changfu [2 ]
Yi, Junzhen [2 ]
Li, Xiaodan [3 ]
Ni, Jiaqiang [3 ]
机构
[1] Shenyang Aerosp Univ, Sch Mechatron Engn, Shenyang 110136, Peoples R China
[2] Shenyang Aerosp Univ, Key Lab Fundamental Sci Natl Def Aeronaut Digital, Shenyang 110136, Peoples R China
[3] Shenyang Aircraft Corp, Shenyang 110850, Liaoning, Peoples R China
来源
APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING | 2022年 / 128卷 / 09期
关键词
Laser deposition; Ti65; Defect; Microstructure; Mechanical property; COOLING RATE; BEHAVIOR; DEFECTS; EVOLUTION;
D O I
10.1007/s00339-022-05955-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Ti65 titanium alloy samples were fabricated by laser deposition manufacturing (LDM) technology, and defects, microstructures and mechanical properties of the LDMed Ti65 samples were investigated. Results showed that there were pores and lack of fusion defects in the sample deposited with low-power laser, and an obvious crack appeared at the bottom of the sample. While in the sample deposited with high-power laser, the pores were much smaller and no other detected defects. After annealing, the defects of these samples did not change markedly. Widmanstatten microstructure was exhibited and no strengthening phases were precipitated in the low-power laser-deposited sample. Lamellar microstructure was exhibited, and Ti3Sn strengthening phases and tungsten-rich phases were presented in the high-power laser-deposited sample. After annealing, both of them changed to basketweave microstructures, but alpha lamellas of the high-power laser-deposited sample were coarsened more notably. The average strength and plasticity of the high-power laser-deposited sample were higher than those of the low-power laser-deposited sample by 6 MPa and 1.4%, respectively. After annealing, strength and plasticity of these samples were improved, and the average strength and plasticity of the high-power samples were still higher than those of the low-power samples by 22 MPa and 3.9%, respectively. The microhardnesses of the as-deposited and annealed samples deposited with high-power laser were greater than those of the corresponding samples deposited with low-power laser.
引用
收藏
页数:12
相关论文
共 39 条
[1]   Methodology for Studying Effect of Cooling Rate During Laser Deposition on Microstructure [J].
Amine, Tarak ;
Newkirk, Joseph W. ;
Liou, Frank .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2015, 24 (08) :3129-3136
[2]   Synthesis and characterization of nanorods for magnetic rotational spectroscopy [J].
Aprelev, Pavel ;
Gu, Yu ;
Burtovyy, Ruslan ;
Luzinov, Igor ;
Kornev, Konstantin G. .
JOURNAL OF APPLIED PHYSICS, 2015, 118 (07)
[3]   Effect of laser energy density on defects behavior of direct laser depositing 24CrNiMo alloy steel [J].
Cao, Lin ;
Chen, Suiyuan ;
Wei, Mingwei ;
Guo, Qian ;
Liang, Jing ;
Liu, Changsheng ;
Wang, Mei .
OPTICS AND LASER TECHNOLOGY, 2019, 111 :541-553
[4]   Relationship among Microstructure, Defects and Performance of Ti60 Titanium Alloy Fabricated by Laser Solid Forming [J].
Chen Jing ;
Zhang Rui ;
Zhang Qiang ;
Yang Jieqiong ;
Huang Weidong .
RARE METAL MATERIALS AND ENGINEERING, 2014, 43 (03) :548-552
[5]   Titanium alloy components fabrication by laser depositing TA15 powders on TC17 forged plate: Microstructure and mechanical properties [J].
Chi, Jiaxuan ;
Cai, Zhongyi ;
Zhang, Hepeng ;
He, Dongsheng ;
Zhang, Hongqiang ;
Wan, Zhandong ;
Peng, Peng ;
Guo, Wei .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2021, 818 (818)
[6]   Mechanical and electrochemical corrosion properties of titanium by laser melting deposition [J].
Di, Ruifeng ;
Qian, Zhu ;
Fang, Yan ;
Tantai, Fanliang ;
Tian, Hongfang ;
Lei, Jianbo .
APPLIED PHYSICS A-MATERIALS SCIENCE & PROCESSING, 2021, 127 (12)
[7]   Microstructure and mechanical properties of PM Ti600 alloy after hot extrusion and subsequent annealing treatment [J].
Ding, Chao ;
Shi, Qi ;
Liu, Xin ;
Zheng, Li ;
Li, Runxia ;
Hang, Zhengxiang ;
Yu, Baoyi ;
Wu, Wei .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2019, 748 :434-440
[8]   Formation and Elimination Mechanism of Lack of Fusion and Cracks in Direct Laser Deposition 24CrNiMoY Alloy Steel [J].
Guo, Qian ;
Chen, Suiyuan ;
Wei, Mingwei ;
Liang, Jing ;
Liu, Changsheng ;
Wang, Mei .
JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2020, 29 (10) :6439-6454
[9]   Blended elemental P/M synthesis and property evaluation of Ti-1100 alloy [J].
Hagiwara, M ;
Emura, S .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2003, 352 (1-2) :85-92
[10]   Structure and properties of Ti-6Al-4V titanium alloy products obtained by direct laser deposition and subsequent heat treatment [J].
Klimova-Korsmik, O. G. ;
Turichin, G. A. ;
Shalnova, S. A. ;
Gushchina, M. O. ;
Cheverikin, V. V. .
BEAM TECHNOLOGIES AND LASER APPLICATION, 2018, 1109