The Effects of Pressure and Temperature on Partial Discharge Degradation of Silicone Conformal Coatings

被引:23
作者
Emersic, Christopher [1 ]
Lowndes, Robert [2 ]
Cotton, Ian [1 ]
Rowland, Simon [1 ]
Freer, Robert [3 ]
机构
[1] Univ Manchester, Sch Elect & Elect Engn EEE, Manchester, Lancs, England
[2] Univ Manchester, Sch Mat, Manchester, Lancs, England
[3] Univ Manchester, Sch Mat, Ceram, Manchester, Lancs, England
关键词
Aerospace testing; Partial discharges; Coatings; Aircraft power systems; Power electronics; CIRCUIT BOARDS; AIRCRAFT;
D O I
10.1109/TDEI.2017.006466
中图分类号
TM [电工技术]; TN [电子技术、通信技术];
学科分类号
0808 ; 0809 ;
摘要
The partial discharge damage rates for silicone-coated printed circuit boards have been quantified in a series of experiments at pressures and temperatures relevant to the aerospace industry (down to 116 mbar, -55 degrees C to + 70 degrees C) and up to 6 kV. Surface cracking was observed, and damage magnitude was found to be non-linear with coating thickness, with thinner coatings experiencing relatively greater damage rates. This is attributed to higher surface electric fields for a given energisation voltage. Increasing temperature or reducing pressure increased the rate of damage. For coating thicknesses less than 100 mu m, reducing pressure to 116 mbar (1 mbar = 100 Pa) increased the relative crack growth rate by nearly an order of magnitude. Temperature change had the most profound influence on damage; low temperatures were observed to substantially reduce damage rate, with very little or no damage observed, whereas higher temperatures substantially increased damage rate, with the resulting magnitude of surface damage too large to quantify. Silicone coatings of thickness greater than 250 mu m showed no appreciable damage from partial discharge when aged at either low pressure or high temperature at voltages up to 6 kV. Corresponding damage-free surface electric fields are computed. No samples were observed to fail, indicating the robustness of high quality silicone coatings. Possible causes of crack formation in silicone are discussed.
引用
收藏
页码:2986 / 2994
页数:9
相关论文
共 13 条
[1]  
[Anonymous], 1992, MAT DEVICES SERIES
[2]  
Auckland D. W., 1993, IEEE C EL INS DIEL P
[3]  
Champion J. V., 2000, 8 INT C DIEL MAT MEA
[4]  
Cotton I., 2007, EL INS C EL MAN EXP
[5]   Higher voltage aircraft power systems [J].
Cotton, Ian ;
Nelms, Andrew ;
Husband, Mark .
IEEE AEROSPACE AND ELECTRONIC SYSTEMS MAGAZINE, 2008, 23 (02) :25-32
[6]   Degradation of Conformal Coatings on Printed Circuit Boards due to Partial Discharge [J].
Emersic, Christopher ;
Lowndes, Robert ;
Cotton, Ian ;
Rowland, Simon ;
Freer, Robert .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2016, 23 (04) :2232-2240
[7]   All-electric aircraft [J].
Howse, M .
POWER ENGINEER, 2003, 17 (04) :35-37
[8]   DEGRADING EFFECT OF HIGH-ALTITUDE CORONA ON ELECTRONIC-CIRCUIT BOARDS [J].
KARADY, GG ;
SIRKIS, MD ;
OLIVA, JR .
IEEE TRANSACTIONS ON ELECTRICAL INSULATION, 1991, 26 (06) :1216-1219
[9]   Thickness dependent dielectric strength of a low-permittivity dielectric film [J].
Kim, HK ;
Shi, FG .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 2001, 8 (02) :248-252
[10]  
Muhamedin F. L., 2015, TELKOMNIKA, V13, P1194