Corrosion of heating surfaces of power station boiler equipment made of steel 12X18H10T

被引:0
|
作者
Reformatskaya, II
Ryzhenkov, VA
Rodionova, IG
Ashcheulova, II
Yakushev, VV
Kiselev, VD
机构
[1] RF Karpov Inst Phys Chem, FGUP, GNTs, Moscow 103064, Russia
[2] Tech Univ, Moscow Power Inst, Moscow, Russia
[3] FGUP Bardin Cent Res Inst Ferrous Met, Moscow, Russia
来源
PROTECTION OF METALS | 2003年 / 39卷 / 06期
关键词
Stainless Steel; Inorganic Chemistry; Thermal Power; Heating Surface; Change Composition;
D O I
10.1023/B:PROM.0000007846.80803.b3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The long-term operation of thermal power equipment made of 12X18HIOT steel at a temperature of greater than or equal to 550degreesC and higher changes its performance due to the changed composition of inside surfaces and bodies of tubes. To avoid deterioration of service characteristics during the operation, the thermal equipment is recommended to make of low-carbon chrome-nickel stainless steels or niobium-stabilized steels. Preservation of the equipment by octadecylamine should be carried out only at a working temperature below its thermodestruction temperature.
引用
收藏
页码:537 / 542
页数:6
相关论文
共 50 条
  • [31] Interaction of shock waves and energy cumulation under the quasi-spherical explosive loading of a 12X18H10T steel ball
    V. I. Zel’dovich
    B. V. Litvinov
    N. Yu. Frolova
    A. E. Kheifets
    A. K. Muzyrya
    A. Yu. Simonov
    Doklady Physics, 2011, 56 : 329 - 333
  • [32] RESISTANCE OF TITANIUM BT1-0 AND CHROME-NICKEL STEEL 12X18H10T IN THE TECHNOLOGICAL MEDIUM FOR DICHLOROETHANE REGENERATION
    VORONKOVA, IN
    CHERNYSH, GP
    KRYUCHEK, VG
    VOLYNSKU, VV
    KHIMIKO-FARMATSEVTICHESKII ZHURNAL, 1981, 15 (10): : 112 - 114
  • [33] INFLUENCE OF DEFORMATION RATE ON MARTENSITIC GAMMA-]ALPHA' TRANSFORMATION AND MECHANICAL-PROPERTIES OF NEUTRON-IRRADIATED 12X18H10T STEEL
    MAKSIMKIN, IP
    SADVAKASOV, DK
    FIZIKA METALLOV I METALLOVEDENIE, 1991, (09): : 202 - 205
  • [34] Changes in the structure and elemental composition of the aluminide coating oil 12X18H10T steel in the course of a long-term exposure to carbonate melt
    Antonov, BD
    Elkina, VI
    Pankratov, AA
    PROTECTION OF METALS, 1997, 33 (06): : 571 - 572
  • [35] Effect of quenching and tempering on the structure and mechanical properties of laminated composites "steel 12X18H10T - steel 5XB2C" obtained by explosive welding
    Prikhodko, E. A.
    Alkhimov, A. P.
    OBRABOTKA METALLOV-METAL WORKING AND MATERIAL SCIENCE, 2012, (01): : 96 - 99
  • [36] Evaluating the piercing conditions for 12X18H10T blanks in 140 mills on the basis of cyclic-shaping data
    Golubchik R.M.
    Merkulov D.V.
    Klempert E.D.
    Medvedev E.K.
    Titova S.V.
    Steel in Translation, 2009, 39 (03) : 262 - 266
  • [37] Replacing Forged 12X18H10T Steel Billet with Castings Obtained from Thin-Walled Metal-Shell Molds with Forced Cooling
    Chernyshov E.A.
    Romanov A.D.
    Romanova E.A.
    Myl’nikov V.V.
    Russian Engineering Research, 2024, 44 (03) : 339 - 342
  • [38] Effect of Stress Concentrators on the Strength of Pipes of Boiler Heating Surfaces Made of 12Cr1MoV and Cr18Ni12Ti Steel Grades.
    Zelenskii, V.G.
    Plotnikov, V.P.
    Teploenergetika, 1976, (10): : 20 - 22
  • [39] Corrosion and electrochemical properties of steel X18H10T in solutions of phosphoric acid at high temperatures
    Filimonov, EV
    Ayuyan, GA
    Shcherbakov, AI
    Pisarenko, TA
    PROTECTION OF METALS, 1999, 35 (06): : 595 - 597
  • [40] CORROSION CRACKING AND INTERGRANULAR CORROSION OF 12KH18N10T STEEL WELD JOINTS
    MELEKHOV, RK
    KOLIUSHKO, BF
    GIRNYI, SI
    MARCHAK, II
    SOVIET MATERIALS SCIENCE, 1990, 26 (05): : 534 - 539