Corrosion of heating surfaces of power station boiler equipment made of steel 12X18H10T

被引:0
|
作者
Reformatskaya, II
Ryzhenkov, VA
Rodionova, IG
Ashcheulova, II
Yakushev, VV
Kiselev, VD
机构
[1] RF Karpov Inst Phys Chem, FGUP, GNTs, Moscow 103064, Russia
[2] Tech Univ, Moscow Power Inst, Moscow, Russia
[3] FGUP Bardin Cent Res Inst Ferrous Met, Moscow, Russia
来源
PROTECTION OF METALS | 2003年 / 39卷 / 06期
关键词
Stainless Steel; Inorganic Chemistry; Thermal Power; Heating Surface; Change Composition;
D O I
10.1023/B:PROM.0000007846.80803.b3
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The long-term operation of thermal power equipment made of 12X18HIOT steel at a temperature of greater than or equal to 550degreesC and higher changes its performance due to the changed composition of inside surfaces and bodies of tubes. To avoid deterioration of service characteristics during the operation, the thermal equipment is recommended to make of low-carbon chrome-nickel stainless steels or niobium-stabilized steels. Preservation of the equipment by octadecylamine should be carried out only at a working temperature below its thermodestruction temperature.
引用
收藏
页码:537 / 542
页数:6
相关论文
共 50 条
  • [1] Corrosion of Heating Surfaces of Power Station Boiler Equipment Made of Steel 12X18H10T
    I. I. Reformatskaya
    V. A. Ryzhenkov
    I. G. Rodionova
    I. I. Ashcheulova
    V. V. Yakushev
    V. D. Kiselev
    Protection of Metals, 2003, 39 : 537 - 542
  • [2] The effect of heatings on the corrosion resistance of 12X18H10T stainless steel
    Shubadeeva, LI
    Revyakina, OK
    Makarchuk, TB
    Gurvich, LY
    PROTECTION OF METALS, 1996, 32 (02): : 119 - 125
  • [3] The diagram of electrochemical equilibrium of 12X18H10T steel
    Tyurin, AG
    PROTECTION OF METALS, 2004, 40 (03): : 240 - 248
  • [4] The Diagram of Electrochemical Equilibrium of 12X18H10T Steel
    A. G. Tyurin
    Protection of Metals, 2004, 40 : 240 - 248
  • [5] The effects of deformations by rolling and uniaxial tension on the structure and the magnetic and mechanical properties of armco iron, steel 12X18H10T, and a steel 12X18H10T-Armco Iron-Steel 12X18H10T composite material
    Gorkunov, E. S.
    Zadvorkin, S. M.
    Kokovikhin, E. A.
    Tueva, E. A.
    Subachev, Yu V.
    Goruleva, L. S.
    Podkopytova, A. V.
    RUSSIAN JOURNAL OF NONDESTRUCTIVE TESTING, 2011, 47 (06) : 369 - 380
  • [6] The effects of deformations by rolling and uniaxial tension on the structure and the magnetic and mechanical properties of armco iron, steel 12X18H10T, and a steel 12X18H10T-Armco Iron-Steel 12X18H10T composite material
    E. S. Gorkunov
    S. M. Zadvorkin
    E. A. Kokovikhin
    E. A. Tueva
    Yu. V. Subachev
    L. S. Goruleva
    A. V. Podkopytova
    Russian Journal of Nondestructive Testing, 2011, 47 : 369 - 380
  • [7] Influence of high hydrostatic pressure on a structure of steel 12X18H10T
    Dobrikov, AO
    Domareva, AS
    METALLOFIZIKA I NOVEISHIE TEKHNOLOGII, 1999, 21 (05): : 49 - 53
  • [8] On the nature of the kink in the oxidation rate curves of 12X18H10T steel
    Kotenev, VA
    Zimina, TY
    PROTECTION OF METALS, 2002, 38 (06): : 570 - 574
  • [9] On the Nature of the Kink in the Oxidation Rate Curves of 12X18H10T Steel
    V. A. Kotenev
    T. Yu. Zimina
    Protection of Metals, 2002, 38 : 570 - 574
  • [10] INTERACTION OF ALUMINIZED 12X18H10T STEEL WITH MOLTEN ALKALI CARBONATES
    ELKINA, VI
    KUDYAKOV, VY
    ANFINOGENOV, AI
    SHAMANOVA, ND
    PANKRATOV, AA
    PERIN, SM
    ANTONOV, BD
    PROTECTION OF METALS, 1995, 31 (03): : 242 - 247