Thirty years of measured prestress at Swedish nuclear reactor containments

被引:34
作者
Anderson, P [1 ]
机构
[1] Lund Univ, Div Struct Engn, S-22100 Lund, Sweden
关键词
D O I
10.1016/j.nucengdes.2005.04.002
中图分类号
TL [原子能技术]; O571 [原子核物理学];
学科分类号
0827 ; 082701 ;
摘要
The main function of the reactor containment, i.e. to ensure tightness at a major internal accident, depends directly on the prestressing system. To secure that the prestress level is sufficient, the tendon force has been measured during the whole time of operation. The general results from these measurements show that the loss of prestress 30 years after tensioning is between 5 and 10%. This is much lower loss than predicted initially at the design stage. More advanced and today commonly used models for predicting prestress loss show better agreement with the results. The main reasons for the relatively low loss are assumed to be: (1) the confirmed slow drying process of the concrete and (2) the high concrete age at the initial tensioning. The results also indicate that the temperature has a major influence on the loss of prestress. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:2323 / 2336
页数:14
相关论文
共 21 条
  • [1] ACI, 1992, ACI MAN CONCR PRACT, V209, P1
  • [2] ALWIS WAM, 2001, P CONCREEP 6, P803
  • [3] Average force along unbonded tendons: a field study at nuclear reactor containments in Sweden
    Anderson, P
    Berglund, LE
    Gustavsson, J
    [J]. NUCLEAR ENGINEERING AND DESIGN, 2005, 235 (01) : 91 - 100
  • [4] Ashar H., 1997, JOINT WANO OECD NEA, P337
  • [5] BAZANT ZP, 1995, MATER STRUCT, V28, P357
  • [6] BHAL NS, 1995, INDIAN CONCRETE J, V69, P499
  • [7] Furr H.L., 1967, ACI J, V64, P288
  • [8] Gopalakrishnan K.S., 1969, American Concrete Institute, V66, P1008
  • [9] Hansen TC., 1966, J Am Concr Inst, V63, P267
  • [10] HILL H, 1995, 9513 NRC