Evidence for exceptional low temperature ductility in polycrystalline magnesium processed by severe plastic deformation

被引:141
|
作者
Figueiredo, Roberto B. [1 ,2 ,3 ]
Sabbaghianrad, Shima [2 ,3 ]
Giwa, Adenike [4 ]
Greer, Julia R. [4 ]
Langdon, Terence G. [2 ,3 ,5 ]
机构
[1] Univ Fed Minas Gerais, Dept Mat Engn & Civil Construct, BR-31270901 Belo Horizonte, MG, Brazil
[2] Univ Southern Calif, Dept Aerosp & Mech Engn, Los Angeles, CA 90089 USA
[3] Univ Southern Calif, Dept Mat Sci, Los Angeles, CA 90089 USA
[4] CALTECH, Div Engn & Appl Sci, Pasadena, CA 91125 USA
[5] Univ Southampton, Fac Engn & Environm, Mat Res Grp, Southampton SO17 1BJ, Hants, England
基金
美国国家科学基金会;
关键词
Ductility; Flow mechanisms; Grain boundary sliding; High-pressure torsion; Magnesium; HIGH-PRESSURE TORSION; GRAINED PURE MG; ROOM-TEMPERATURE; SINGLE-CRYSTAL; CREEP-BEHAVIOR; STRAIN-RATE; MICROSTRUCTURAL EVOLUTION; ELEVATED-TEMPERATURES; AZ31; ALLOY; HCP METALS;
D O I
10.1016/j.actamat.2016.09.054
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
An investigation was conducted to examine the mechanical behavior and microstructure evolution during deformation of ultrafine-grained pure magnesium at low temperatures within the temperature range of 296-373 K. Discs were processed by high-pressure torsion until saturation in grain refinement. Dynamic hardness testing revealed a gradual increase in strain rate sensitivity up to m approximate to 0.2. High ductility was observed in the ultrafine-grained magnesium including an exceptional elongation of similar to 360% in tension at room temperature and stable deformation in micropillar compression. Grain coarsening and an increase in frequency of grain boundaries with misorientations in the range 15 degrees-45 degrees occurred during deformation in tension. The experimental evidence, when combined with an analysis of the deformation behavior, suggests that grain boundary sliding plays a key role in low strain rate deformation of pure magnesium when the grain sizes are at and below similar to 5 mu m. (C) 2016 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:322 / 331
页数:10
相关论文
共 50 条
  • [41] Tensile flow behavior of AZ31 magnesium alloy processed by severe plastic deformation and post-annealing at moderately high temperatures
    Fong, Kai Soon
    Danno, Atsushi
    Tan, Ming Jen
    Chua, Beng Wah
    JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2017, 246 : 235 - 244
  • [42] On the Issue of the Improvement of Magnesium Plasticity by Cold Severe Plastic Deformation
    Komkova, D. A.
    Antonova, O. V.
    Volkov, A. Yu.
    PHYSICS OF METALS AND METALLOGRAPHY, 2018, 119 (11) : 1120 - 1126
  • [43] Magnetic Binary Supersaturated Solid Solutions Processed by Severe Plastic Deformation
    Stuckler, Martin
    Krenn, Heinz
    Pippan, Reinhard
    Weissitsch, Lukas
    Wurster, Stefan
    Bachmaier, Andrea
    NANOMATERIALS, 2019, 9 (01)
  • [44] New insight for mechanical properties of metals processed by severe plastic deformation
    Wang, Peng
    Xiang, Yuhai
    Wang, Xiaogui
    Liu, Zhanli
    Qu, Shaoxing
    Zhuang, Zhuo
    INTERNATIONAL JOURNAL OF PLASTICITY, 2019, 123 : 22 - 37
  • [45] The fundamentals of nanostructured materials processed by severe plastic deformation
    Yuntian T. Zhu
    Terence G. Langdon
    JOM, 2004, 56 : 58 - 63
  • [46] Impact of severe plastic deformation on kinetics and thermodynamics of hydrogen storage in magnesium and its alloys
    Edalati, Kaveh
    Akiba, Etsuo
    Botta, Walter J.
    Estrin, Yuri
    Floriano, Ricardo
    Fruchart, Daniel
    Grosdidier, Thierry
    Horita, Zenji
    Huot, Jacques
    Li, Hai-Wen
    Lin, Huai-Jun
    Revesz, Adam
    Zehetbauer, Michael J.
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2023, 146 : 221 - 239
  • [47] Microstructural stability of Cu processed by different routes of severe plastic deformation
    Gubicza, J.
    Dobatkin, S. V.
    Khosravi, E.
    Kuznetsov, A. A.
    Labar, J. L.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (03): : 1828 - 1832
  • [48] Microstructure of a metal-polymer composite processed by severe plastic deformation
    Sauvage, Xavier
    Malandain, Jean-Jacques
    Hohenwarter, A.
    NANOMATERIALS BY SEVERE PLASTIC DEFORMATION IV, PTS 1 AND 2, 2008, 584-586 : 306 - 309
  • [49] Severe plastic deformation (SPD) of biodegradable magnesium alloys and composites: A review of developments and prospects
    Kasaeian-Naeini, M.
    Sedighi, M.
    Hashemi, R.
    JOURNAL OF MAGNESIUM AND ALLOYS, 2022, 10 (04) : 938 - 955
  • [50] Achieving Exceptional Grain Refinement through Severe Plastic Deformation: New Approaches for Improving the Processing Technology
    Valiev, Ruslan Z.
    Langdon, Terence G.
    METALLURGICAL AND MATERIALS TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 2011, 42A (10): : 2942 - 2951