INFLUENCE OF PLASTIC DEFORMATION DURING EXTRUSION PROCESS ON HEAT RESISTANCE ALLOYS Fe40Al

被引:1
作者
Pasek, D. [1 ]
Cebulski, J. [1 ]
机构
[1] Silesian Tech Univ, Dept Mat Engn & Met, 8 Krasinskiego Str, PL-40019 Katowice, Poland
关键词
corrosion resistance; plastic deformation; alloys intermetallic phase matrix FeAl; Al2O3; extrusion; IRON ALUMINIDE; OXIDATION; MICROSTRUCTURE; FEAL;
D O I
10.1515/amm-2017-0336
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
The article presents the results of studies on the effects wrought on the corrosion resistance of the alloy matrix phase intermetallic FeAl. Researches were carried out on the Fe40Al5Cr0.2TiB alloy and involved the oxidation of the samples after the crystallization after plastic deformation made by extrusion. The tests were performed in an oven in air at 1100 degrees C for 100, 300 and 500 h. Determined to change the mass of the samples after corrosion research setting kinetics of corrosion processes, as well as an analysis of the microstructure of the alloy after the crystallization and after forming. The structure was examined using light microscopy and scanning electron microscopy and X-ray microanalysis with EDS chemical composition of the corrosion products. The test results revealed that plastic deformation during extrusion of intermetallic alloy led to structural changes, the effect of which was to improve the heat resistance at a temperature of 1100 degrees C.
引用
收藏
页码:2281 / 2286
页数:6
相关论文
共 50 条
[21]   Influence of Pre-Heat Treatment on the Deformation Behaviors, Microstructural Characteristics, and Mechanical Properties of a Continuously Cast Al-Cu-Mg Alloy during Continuous Extrusion Process [J].
Qin, Renbao ;
Chen, Wentian ;
Tang, Jie ;
Jiang, Fulin ;
Chen, Yonggang ;
Zhang, Hui .
MATERIALS, 2023, 16 (08)
[22]   Recent Developments in Plastic Deformation Behavior of Titanium and Its Alloys During the Rolling Process: A Review [J].
Ryu, Donghee ;
Kim, Yulhee ;
Nahm, Sahn ;
Kang, Leeseung .
MATERIALS, 2024, 17 (24)
[23]   B2 phase precipitation behavior in Ti-40Al-8Nb alloys during the hot deformation process [J].
Yang, Guang ;
Zuo, Junxian ;
Cheng, Liang ;
Wang, Yanli ;
Zhu, Bin ;
Han, Songsong ;
Bai, Wenpeng ;
Yu, Min .
INTERMETALLICS, 2022, 150
[24]   Influence of severe plastic deformation on dynamic strain aging of ultrafine grained Al-Mg alloys [J].
Zhao, Shiteng ;
Meng, Chenlu ;
Mao, Fengxin ;
Hu, Weiping ;
Gottstein, Guenter .
ACTA MATERIALIA, 2014, 76 :54-67
[25]   Structure of Al-Fe alloys prepared by different methods after severe plastic deformation under pressure [J].
Dobromyslov, A. V. ;
Taluts, N. I. .
PHYSICS OF METALS AND METALLOGRAPHY, 2017, 118 (06) :564-571
[26]   Influence of the Plastic Deformation Process on the Residual Stresses and Hardness of an Al-5Mg Alloy [J].
Samara, Fayez ;
Goanta, Viorel ;
Istrate, Bogdan ;
Alkisswani, Layth ;
Munteanu, Corneliu ;
Cosau, Roxana .
MATERIALS, 2024, 17 (14)
[27]   The Influence of Niobium Additions on Creep Resistance of Fe-27 at. % Al Alloys [J].
Dobes, Ferdinand ;
Dymacek, Petr ;
Friak, Martin .
METALS, 2019, 9 (07)
[28]   Severe Plastic Deformation of Fe-22Al-5Cr Alloy by Cross-Channel Extrusion with Back Pressure [J].
Lyszkowski, Radoslaw ;
Polkowski, Wojciech ;
Czujko, Tomasz .
MATERIALS, 2018, 11 (11)
[29]   How does surface integrity of nanostructured surfaces induced by severe plastic deformation influence fatigue behaviors of Al alloys with enhanced precipitation? [J].
Maurel, Pierre ;
Weiss, Laurent ;
Grosdidier, Thierry ;
Bocher, Philippe .
INTERNATIONAL JOURNAL OF FATIGUE, 2020, 140 (140)
[30]   An analysis to plastic deformation behavior of AZ31 alloys during accumulative roll bonding process [J].
Roostaei, Ali A. ;
Zarei-Hanzaki, A. ;
Parsa, M. H. ;
Fatemi-Varzaneh, S. M. .
JOURNAL OF MATERIALS SCIENCE, 2010, 45 (16) :4494-4500