Development of etched SiO2@Pt@ZrO2 core-shell catalyst for CO and C3H6 oxidation at low temperature

被引:9
|
作者
Lee, Eun Jun [1 ]
Seo, Yaeun [1 ]
Park, Haney [1 ]
Kim, Min June [1 ]
Yoon, Dalyoung [3 ]
Choung, Jin Woo [3 ]
Kim, Chang Hwan [3 ]
Choi, Jungkyu [1 ]
Lee, Kwan-Young [1 ,2 ]
机构
[1] Korea Univ, Dept Chem & Biol Engn, 145 Anam Ro, Seoul 02841, South Korea
[2] Korea Univ, Super Ultra Low Energy & Emiss Vehicle SULEEV Ctr, 145 Anam Ro, Seoul 02841, South Korea
[3] Hyundai Motor Co, IFAT Inst Fundamental & Adv Technol, Energy & Environm Chem Syst Lab, R&D Div, 37 Cheoldobagmulgwan Ro, Uiwang Si 16082, Gyeonggi Do, South Korea
基金
新加坡国家研究基金会;
关键词
Simultaneous CO and hydrocarbon oxidation; Etched SiO2 @Pt@ZrO2; Thermal stability; THERMAL-STABILITY; SHELL; PERFORMANCE; ZRO2; NANOPARTICLES; SUPPORT; SPHERES; IMPACT; SIO2;
D O I
10.1016/j.apsusc.2021.151582
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In our previous study, we conducted CO oxidation with SiO2@Pd@CeO2 catalysts. However, the limit of the CeO2 shell thickness limited the thermal stability. So, in this study, thick ZrO2 shell was introduced to improve thermal stability. SiO2@Pt@ZrO2 catalysts were examined for the simultaneous oxidation of CO and hydrocarbons. SiO2@Pt@ZrO2 catalysts had improved thermal stability compared to Pt/SiO2 or Pt/ZrO2 after aging at 750 degrees C for 25 h. However, fresh SiO2@Pt@ZrO2 catalysts showed low oxidation activity because of the low gas accessibility due to the thick ZrO2 shell. Therefore, we proposed etched SiO2@Pt@ZrO2 catalysts for enhanced gas accessibility. The selective etching of SiO2 was adjusted by varying the KOH concentration. TEM images confirmed that the void space of the core-shell catalysts increased as the concentration of KOH increased. The exposed Pt surface area increased as the void space of the core-shell catalysts was increased. On the other hand, in excessively etched 3.2 M catalysts, the core-shell structure collapsed. Etched catalysts which maintain the core-shell structure improve thermal stability after hydrothermal aging. As a result, 1.6 M catalysts showed the best simultaneous oxidation of CO and hydrocarbons, and we confirmed that properly etched catalysts enhanced the oxidation activity and thermal stability.
引用
收藏
页数:8
相关论文
共 50 条
  • [21] The impact of CO and C3H6 pulses on PtOx reduction and NO oxidation in a diesel oxidation catalyst
    Arvajova, Adela
    Koci, Petr
    Schmeisser, Volker
    Weibel, Michel
    APPLIED CATALYSIS B-ENVIRONMENTAL, 2016, 181 : 644 - 650
  • [22] A highly loaded Ni@SiO2 core-shell catalyst for CO methanation
    Lakshmanan, Pandian
    Kim, Min Sik
    Park, Eun Duck
    APPLIED CATALYSIS A-GENERAL, 2016, 513 : 98 - 105
  • [23] Preparation, Characterization, and Kinetic Study of a Core-Shell Mn3O4@SiO2 Nanostructure Catalyst for CO Oxidation
    Xu, Jing
    Deng, Ya-Qing
    Zhang, Xiao-Man
    Luo, Yan
    Mao, Wei
    Yang, Xue-Jing
    Ouyang, Like
    Tian, Pengfei
    Han, Yi-Fan
    ACS CATALYSIS, 2014, 4 (11): : 4106 - 4115
  • [24] NiO@SiO2 core-shell catalyst for low-temperature methanation of syngas in slurry reactor
    Wang H.
    Zhang J.-F.
    Bai Y.-X.
    Wang W.-F.
    Tan Y.-S.
    Han Y.-Z.
    Ranliao Huaxue Xuebao/Journal of Fuel Chemistry and Technology, 2016, 44 (05): : 548 - 556
  • [25] Effect of hydrothermal reaction time and calcination temperature on properties of Au@CeO2 core-shell catalyst for CO oxidation at low temperature
    He, Beibei
    Zhao, Qingguo
    Zeng, Zhigang
    Wang, Xiaohong
    Han, Sheng
    JOURNAL OF MATERIALS SCIENCE, 2015, 50 (19) : 6339 - 6348
  • [26] Effect of Calcination Atmospheres on Catalytic Performance of Pt/Al2O3 for Oxidation of CO and C3H6
    Guo Miaoxin
    Wang Fengjun
    Wang Chengxiong
    Zhang Aimin
    Zhao Yunkun
    Du Junchen
    RARE METAL MATERIALS AND ENGINEERING, 2021, 50 (09) : 3056 - 3061
  • [27] Effect of Thermal Degradation on the CO, C3H6, and NO Oxidation Performance of Pt/Al2O3 with a Zoned Distribution of Pt
    Abedi, Ali
    Epling, William
    INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2014, 53 (14) : 5692 - 5700
  • [28] Evaluation of the oxidizing potential of Ru and Ru-Pt/ZrO2 catalysts for NO oxidation in the presence of C3H6 and O2
    Serrano-Sánchez, AM
    Steltenpohl, P
    González-Marcos, MP
    González-Marcos, JA
    González-Velasco, JR
    CHEMICAL PAPERS, 2004, 58 (01): : 41 - 47
  • [29] Preparation and application of core-shell Pt/TiO2 catalyst for ammonia oxidation process
    Xu, Xiao-Bo
    Pu, Xue-Ling
    Yuan, Shao-Jun
    Jiang, Wei
    Liang, Bin
    Journal of Molecular Catalysis, 2014, 28 (01): : 75 - 81
  • [30] CO Oxidation Activities of Ni and Pd-TiO2@SiO2 Core-Shell Nanostructures
    Do, Yeji
    Cho, Insu
    Park, Yohan
    Pradhan, Debabrata
    Sohn, Youngku
    BULLETIN OF THE KOREAN CHEMICAL SOCIETY, 2013, 34 (12): : 3635 - 3640