Durability of glass-fiber-reinforced polymer composites in an alkaline environment

被引:2
|
作者
Cho, Eung Ha [1 ]
Mounts, Joshua L.
机构
[1] W Virginia Univ, Dept Chem Engn, Morgantown, WV 26506 USA
[2] Dow Engn Solut, S Charleston, WV 25303 USA
来源
JOURNAL OF VINYL & ADDITIVE TECHNOLOGY | 2007年 / 13卷 / 04期
关键词
D O I
10.1002/vnl.20127
中图分类号
O69 [应用化学];
学科分类号
081704 ;
摘要
This study investigated the aging of urethane and urethane-modified vinyl ester (UMVE) GFRPs (glass fiber reinforced polymers) when they were exposed to alkaline solution for six months under a sustained load of 34.5 MPa or 16-20% of their tensile strength. The second experiment exposed both types of GFRP to alkaline solution without load for 6 months. The final experiment determined the alkaline solution diffusion coefficients into GFRP and neat polymer resin samples by measuring the change in mass of each sample as a function of time. After the GFRP samples were aged for 6 months, their tensile strengths were measured and compared with that of non-aged samples to determine the aging effect. It was found that alkaline solution alone without sustained load did not significantly reduce or change the tensile strength of any GFRP sample. However, the presence of sustained load greatly increased the aging effect, particularly more for urethane GFRP than on UMVE GFRP. Urethane GFRP experienced a tensile strength reduction of 57.5%, while UMVE GFRP lost 27.3% of its original tensile strength. J. VINYL ADDIT. TECHNOL., 13:221-228, 2007. (c) 2007 Society of Plastics Engineers.
引用
收藏
页码:221 / 228
页数:8
相关论文
共 50 条
  • [1] Durability of glass-fiber-reinforced polymer nanocomposites in an alkaline environment
    Ravindran, N
    Cho, EH
    JOURNAL OF VINYL & ADDITIVE TECHNOLOGY, 2006, 12 (01): : 25 - 32
  • [2] Durability of carbon and glass fiber reinforced polymer composites
    Civil Engineering Institute, Zhengzhou University, Zhengzhou 450001, China
    不详
    Harbin Gongye Daxue Xuebao, 2009, 2 (150-154):
  • [3] DURABILITY CHARACTERISTICS OF POLYMER-MODIFIED GLASS-FIBER-REINFORCED CONCRETE - CLOSURE
    SOROUSHIAN, P
    TLILI, A
    YOHENA, M
    TILSEN, BL
    ACI MATERIALS JOURNAL, 1993, 90 (06) : 631 - 631
  • [4] Assessment of Glass-Fiber-Reinforced Polymer (GFRP)-Concrete Interface Durability Subjected to Simulated Seawater Environment
    Ma, Deliang
    Liu, Jie
    Wang, Libin
    Wang, Qiudong
    BUILDINGS, 2024, 14 (06)
  • [5] STRENGTH AND DURABILITY OF MIXED GLASS-FIBER-REINFORCED LAMINATES
    ANDERSONS, J
    LOMONOV, V
    MIKELSONS, M
    TAMUZS, V
    MECHANICS OF COMPOSITE MATERIALS, 1994, 30 (01) : 22 - 29
  • [6] Glass-fiber-reinforced wood/plastic composites
    Rizvi, Ghaus M.
    Serneralul, Harnid
    JOURNAL OF VINYL & ADDITIVE TECHNOLOGY, 2008, 14 (01): : 39 - 42
  • [7] "Brick-and-Mortar" Nanostructured Interphase for Glass-Fiber-Reinforced Polymer Composites
    De Luca, Francois
    Sernicola, Giorgio
    Shaffer, Milo S. P.
    Bismarck, Alexander
    ACS APPLIED MATERIALS & INTERFACES, 2018, 10 (08) : 7352 - 7361
  • [8] LOW-TEMPERATURE COMPRESSIVE STRENGTH OF GLASS-FIBER-REINFORCED POLYMER COMPOSITES
    DUTTA, PK
    JOURNAL OF OFFSHORE MECHANICS AND ARCTIC ENGINEERING-TRANSACTIONS OF THE ASME, 1994, 116 (03): : 167 - 172
  • [9] LONGITUDINAL COMPRESSION STRENGTH OF GLASS-FIBER-REINFORCED COMPOSITES
    KIM, RY
    CRASTO, AS
    JOURNAL OF REINFORCED PLASTICS AND COMPOSITES, 1994, 13 (04) : 326 - 338
  • [10] Numerical failure analysis of glass-fiber-reinforced composites
    Tanimoto, Y
    Nishiwaki, T
    Nemoto, K
    JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART A, 2004, 68A (01): : 107 - 113