Phase Transition of AISI Type 304L Stainless Steel Induced By Severe Plastic Deformation via Cryo-Rolling

被引:5
|
作者
Shit, Gopinath [1 ]
Bhaskar, Pragna [1 ]
Ningshen, S. [1 ]
Dasgupta, A. [1 ]
Mudali, U. Kamachi [1 ]
Bhaduri, A. Kumar [1 ]
机构
[1] Indira Gandhi Ctr Atom Res, Kalpakkam 603102, Tamil Nadu, India
来源
关键词
304L Stainless Steel; Phase Transition; Corrosion; Microscopy; XRD; SPD; INDUCED MARTENSITIC-TRANSFORMATION; STRAIN; RESISTANCE; TENSILE;
D O I
10.1063/1.4980199
中图分类号
O469 [凝聚态物理学];
学科分类号
070205 ;
摘要
The phase transition induced by Severe Plastic Deformation (SPD) was confirmed in metastable AISI type 304L austenitic stainless steel (SS). SPD via cryo-rolling in liquid nitrogen (L-N-2) temperature is the adopted route for correlating the phase transition and corrosion resistance. The thickness of the annealed AISI type 304L SS at 1050 degrees C sheet was reduced step by step from 15% to 50% of its initial thickness. The phase changes and phase transformation are qualitatively analyzed by X-Ray Diffraction (XRD) method. During the process, the XRD of each Cryo-Rolled and annealed sample was analyzed and different phases and phase transitions are measured. The investigated AISI type 304L SS by SPD reveals a microstructure of gamma-austenite; alpha' - marternsite and epsilon-martensite formation depending on the percentage of cryo-rolling. The Vickers hardness (HV) of the samples is also measured. The corrosion rate of the annealed sheet and cryo rolled sample was estimated in boiling nitric acid as per ASTM A-262 practice-C test.
引用
收藏
页数:3
相关论文
共 50 条
  • [31] Liquid phase cladding of AlxCoCrFeNi high entropy alloys on AISI 304L stainless steel
    Fereidouni, Mohammad
    Khorrami, Mahmoud Sarkari
    Sohi, Mahmoud Heydarzadeh
    SURFACE & COATINGS TECHNOLOGY, 2020, 402
  • [32] Corrosion degradation of AISI type 304L stainless steel for application in nuclear reprocessing plant
    S. Ningshen
    M. Sakairi
    Journal of Solid State Electrochemistry, 2015, 19 : 3533 - 3542
  • [33] Nitriding behavior and corrosion properties of AISI 304L and 316L austenitic stainless steel with deformation-induced martensite
    Biehler, J.
    Hoche, H.
    Oechsner, M.
    SURFACE & COATINGS TECHNOLOGY, 2017, 324 : 121 - 128
  • [34] Comprehensive study of deuterium-induced effects in austenitic stainless steel AISI 304L
    Roehsler, Andreas
    Sobol, Oded
    Unger, Wolfgang E. S.
    Boellinghaus, Thomas
    INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2019, 44 (23) : 12228 - 12238
  • [35] Analysis of dissipated energy and temperature fields at severe notches of AISI 304L stainless steel specimens
    Rigon, D.
    Ricotta, M.
    Meneghetti, G.
    FRATTURA ED INTEGRITA STRUTTURALE, 2019, 13 (47): : 334 - 347
  • [36] Improvement of the corrosion behavior of AISI 304L stainless steel by deep rolling treatment under cryogenic cooling
    Khouloud Gharbi
    Naoufel Ben Moussa
    Amir Ben Rhouma
    Nabil Ben Fredj
    The International Journal of Advanced Manufacturing Technology, 2021, 117 : 3841 - 3857
  • [37] Improvement of the corrosion behavior of AISI 304L stainless steel by deep rolling treatment under cryogenic cooling
    Gharbi, Khouloud
    Ben Moussa, Naoufel
    Ben Rhouma, Amir
    Ben Fredj, Nabil
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2021, 117 (11-12): : 3841 - 3857
  • [38] Johnson-Mehl-Avrami-Kolmogorov (JMAK-type) Analysis of Deformation-Induced Martensitic Transformation in AISI 304L Stainless Steel
    Sohrabi, Mohammad Javad
    Mirzadeh, Hamed
    Sadeghpour, Saeed
    Mahmudi, Reza
    IRANIAN JOURNAL OF MATERIALS SCIENCE AND ENGINEERING, 2023, 20 (04) : 1 - 9
  • [39] A Study on Deformation Behavior of 304L Stainless Steel During and After Plate Rolling at Elevated Temperatures
    Pourabdollah, P.
    Serajzadeh, S.
    JOURNAL OF MATERIALS ENGINEERING AND PERFORMANCE, 2017, 26 (02) : 885 - 893
  • [40] A Study on Deformation Behavior of 304L Stainless Steel During and After Plate Rolling at Elevated Temperatures
    P. Pourabdollah
    S. Serajzadeh
    Journal of Materials Engineering and Performance, 2017, 26 : 885 - 893