Effect of target composition on the microstructural, mechanical, and corrosion properties of TiAlN thin films deposited by high-power impulse magnetron sputtering (Reprinted from Surface & Coatings Technology, vol 352, pg 330-337, 2018)

被引:3
作者
Chang, Chi-Lung [1 ,2 ]
Yang, Fu-Chi [2 ]
机构
[1] Ming Chi Univ Technol, Dept Mat Engn, New Taipei 24301, Taiwan
[2] Ming Chi Univ Technol, Ctr Thin Film Technol & Applicat, New Taipei 24301, Taiwan
关键词
High-power impulse magnetron sputtering (HiPIMS); TixAly alloy target; TiAlN coating; Hardness; Corrosion; AL-N COATINGS; TRIBOLOGICAL PROPERTIES; TI; OXIDATION; HIPIMS; GROWTH; BEHAVIOR; ENHANCEMENT; HYSTERESIS; STABILITY;
D O I
10.1016/j.surfcoat.2019.07.008
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Ti1-xAlxN thin films were deposited using reactive high-power impulse magnetron sputtering on silicon Si (100), tungsten carbide (WC-Co), and SUS304 substrates using three metallurgical TixAly alloy targets with Al/(Al + Ti) atomic ratios of 0.19, 0.36, and 0.57. A fixed duty cycle of 1% and a N-2/Ar ratio of 15.8% was used. The currentvoltage characteristics of the TixAly alloy targets were first investigated. Then, the microstructural evolution and the mechanical and corrosion properties of the as-deposited Ti1-xAlxN thin films were analysed by scanning electron microscopy, grazing incident X-ray diffractometry, X-ray photoelectron spectroscopy, transmission electron microscopy, nanoindentation, and anodic potentiodynamic polarisation tests. The power density of 1.86 kW/cm(2) achieved with the square-like power output wave obtained in the constant current mode was higher than the 1.37 kW/cm(2) power density obtained with the triangular-like power output wave. The deposition rates of the Ti1-xAlxN thin films increased from 13.4 to 28.6 nm/min with an increasing alloy target Al/(Al + Ti) atomic ratio due to the higher sputter yield of Al than Ti. The Al/(Al + Ti) atomic ratio of the alloy target determines the structure, which changed from a highly preferred TiN (111) orientation (Al/(Al + Ti) ratio = 0.19) to a nanocomposite structure (Al/(Al + Ti) ratio = 0.57). The nanoindentation results indicated that the highest hardness and elastic modulus values of the Ti1-xAlxN thin films were 33.3 GPa and 405.9 GPa, respectively, obtained using the Al/(Al + Ti) = 0.19 alloy target. In addition, the friction coefficients of the Ti1-xAlxN thin films were between 0.68 and 0.77. However, the potentiostatic polarisation measurements showed that the amorphous TiAlN films exhibited the highest corrosion resistance in 3.5% NaCl solution, as the corrosion resistance of the Ti1-xAlxN coatings increased as the Al/(Al + Ti) atomic ratio increased.
引用
收藏
页码:113 / 120
页数:8
相关论文
共 56 条
  • [1] Corrosion behavior of PVD-grown WC-(Ti1-xAlx)N films in a 3.5% NaCl solution
    Ahn, SH
    Yoo, JH
    Choi, YS
    Kim, JG
    Han, JG
    [J]. SURFACE & COATINGS TECHNOLOGY, 2003, 162 (2-3) : 212 - 221
  • [2] Hysteresis and process stability in reactive high power impulse magnetron sputtering of metal oxides
    Aiempanakit, Montri
    Kubart, Tomas
    Larsson, Petter
    Sarakinos, Kostas
    Jensen, Jens
    Helmersson, Ulf
    [J]. THIN SOLID FILMS, 2011, 519 (22) : 7779 - 7784
  • [3] On the deposition rate in a high power pulsed magnetron sputtering discharge
    Alami, J.
    Sarakinos, K.
    Mark, G.
    Wuttig, M.
    [J]. APPLIED PHYSICS LETTERS, 2006, 89 (15)
  • [4] Bandorf R., 2014, COMPREHENSIVE MAT PR, V4, P75
  • [5] An investigation of c-HiPIMS discharges during titanium deposition
    Barker, Paul Michael
    Konstantinidis, Stephanos
    Lewin, Erik
    Britun, Nikolay
    Patscheider, Joerg
    [J]. SURFACE & COATINGS TECHNOLOGY, 2014, 258 : 631 - 638
  • [6] Deposition of TiAlN coatings using reactive bipolar-pulsed direct current unbalanced magnetron sputtering
    Barshilia, Harish C.
    Yogesh, K.
    Rajam, K. S.
    [J]. VACUUM, 2008, 83 (02) : 427 - 434
  • [7] The effect of changing the magnetic field strength on HiPIMS deposition rates
    Bradley, J. W.
    Mishra, A.
    Kelly, P. J.
    [J]. JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2015, 48 (21)
  • [8] Abrasive wear behavior of high speed steel and hard metal coated with TiALN and TiCN
    Bressan, JD
    Hesse, R
    Silva, EM
    [J]. WEAR, 2001, 250 (PART 1) : 561 - 568
  • [9] Deposition rate enhancement in HiPIMS without compromising the ionized fraction of the deposition flux
    Capek, J.
    Hala, M.
    Zabeida, O.
    Klemberg-Sapieha, J. E.
    Martinu, L.
    [J]. JOURNAL OF PHYSICS D-APPLIED PHYSICS, 2013, 46 (20)
  • [10] Effects of nitrogen flow rates on the growth morphology of TiA1N films prepared by an rf-reactive sputtering technique
    Chakrabarti, K
    Jeong, JJ
    Hwang, SK
    Yoo, YC
    Lee, CM
    [J]. THIN SOLID FILMS, 2002, 406 (1-2) : 159 - 163