Control of degradation rate of bioabsorbable magnesium by anodization and steam treatment

被引:35
作者
Hiromoto, Sachiko [1 ]
Yamamoto, Akiko
机构
[1] Natl Inst Mat Sci, Int Ctr Mat Nanoarchitecton, Tsukuba, Ibaraki 3050044, Japan
来源
MATERIALS SCIENCE & ENGINEERING C-MATERIALS FOR BIOLOGICAL APPLICATIONS | 2010年 / 30卷 / 08期
关键词
Bioabsorbable magnesium; Culture medium; Anodization; Autoclaving; Degradation rate; Corrosion; PURE MAGNESIUM; CORROSION-RESISTANCE; SPECTROPHOTOMETRIC DETERMINATION; ABSORBABLE METAL; ALLOY; BEHAVIOR; SURFACE; MG; BIODEGRADATION; PRECIPITATION;
D O I
10.1016/j.msec.2010.06.001
中图分类号
TB3 [工程材料学]; R318.08 [生物材料学];
学科分类号
0805 ; 080501 ; 080502 ;
摘要
The control of degradation rate of bioabsorbable magnesium devices is crucial for their biomedical applications. In this study, the influence of anodizing voltages and autoclaving on the degradation behavior of anodized pure magnesium was examined by immersion tests in a culture medium for 14 d. The anodization and autoclaving varied the morphology of surface film. Porous films were formed at 7 V and 100 V. and non-porous films were formed at 2 V and 20 V. The microscopic appearance of the anodized films did not change by autoclaving. The degradation rate on Day 1 was the highest and subsequently decreased to a quasi-steady state within the initial 3-5 d. The 7 V- and 100 V-anodized specimens showed the highest and the lowest quasi-steady degradation rate, respectively. The autoclaving significantly retarded the degradation of the anodized specimens. These facts revealed that anodization and autoclaving are useful for the control of the degradation rate of magnesium and its alloys. The porous anodized films showed local corrosion, whereas the non-porous anodized film formed at 20 V did not show apparent local corrosion. The local corrosion was prevented by autoclaving. These results suggest that the occurrence of local corrosion depends on the porous morphology of surface film. (C) 2010 Elsevier B.V. All rights reserved.
引用
收藏
页码:1085 / 1093
页数:9
相关论文
共 38 条
[1]   Surface modification of magnesium by NaHCO3 and corrosion behavior in Hank's solution for new biomaterial applications [J].
Al-Abdullat, Y ;
Tsutsumi, S ;
Nakajima, N ;
Ohta, M ;
Kuwahara, H ;
Ikeuchi, K .
MATERIALS TRANSACTIONS, 2001, 42 (08) :1777-1780
[2]   Anodizing treatments for magnesium alloys and their effecton corrosion resistance in various environments [J].
Blawert, Carsten ;
Dietzel, Wolfgang ;
Ghali, Edward ;
Song, Guangling .
ADVANCED ENGINEERING MATERIALS, 2006, 8 (06) :511-533
[3]  
Di Mario Carlo, 2004, J Interv Cardiol, V17, P391, DOI 10.1111/j.1540-8183.2004.04081.x
[4]   Temporary scaffolding of coronary arteries with bioabsorbable magnesium stents:: a prospective, non-randomised multicentre trial [J].
Erbel, Raimund ;
Di Mario, Carlo ;
Bartunek, Jozef ;
Bonnier, Johann ;
de Bruyne, Bernard ;
Eberli, Franz R. ;
Erne, Paul ;
Haude, Michael ;
Heublein, Bernd ;
Horrigan, Mark ;
Ilsley, Charles ;
Boese, Dirk ;
Koolen, Jacques ;
Luescher, Thomas F. ;
Weissman, Neil ;
Waksman, Ron .
LANCET, 2007, 369 (9576) :1869-1875
[5]   On the biodegradation performance of an Mg-Y-RE alloy with various surface conditions in simulated body fluid [J].
Haenzi, Anja C. ;
Gunde, Petra ;
Schinhammer, Michael ;
Uggowitzer, Peter J. .
ACTA BIOMATERIALIA, 2009, 5 (01) :162-171
[6]   Biocorrosion of magnesium alloys: a new principle in cardiovascular implant technology? [J].
Heublein, B ;
Rohde, R ;
Kaese, V ;
Niemeyer, M ;
Hartung, W ;
Haverich, A .
HEART, 2003, 89 (06) :651-656
[7]   Precipitation control of calcium phosphate on pure magnesium by anodization [J].
Hiromoto, Sachiko ;
Shishido, Tamao ;
Yamamoto, Akiko ;
Maruyama, Norio ;
Somekawa, Hidetoshi ;
Mukai, Toshiji .
CORROSION SCIENCE, 2008, 50 (10) :2906-2913
[8]   Polarization behavior of pure magnesium under a controlled flow in a NaCl solution [J].
Hiromoto, Sachiko ;
Yamamoto, Akiko ;
Maruyama, Norio ;
Somekawa, Hidetoshi ;
Mukai, Toshiji .
MATERIALS TRANSACTIONS, 2008, 49 (06) :1456-1461
[9]   Corrosion product formation during NaCl induced atmospheric corrosion of magnesium alloy AZ91D [J].
Jonsson, Martin ;
Persson, Dan ;
Thierry, Dominique .
CORROSION SCIENCE, 2007, 49 (03) :1540-1558
[10]  
KANAZAWA T, 1985, INORGANIC PHOSPHORUS, P4