Reinforcement of a PMMA resin for fixed interim prostheses with nanodiamonds

被引:52
作者
Protopapa, Popi [2 ]
Kontonasaki, Eleana [2 ]
Bikiaris, Dimitrios [3 ]
Paraskevopoulos, Konstantinos M. [1 ]
Koidis, Petros [2 ]
机构
[1] Aristotle Univ Thessaloniki, Solid State Phys Sect, Sch Phys, GR-54124 Thessaloniki, Macedonia, Greece
[2] Aristotle Univ Thessaloniki, Dept Fixed Prostheses & Implants Prosthodont, Sch Dent, GR-54124 Thessaloniki, Macedonia, Greece
[3] Aristotle Univ Thessaloniki, Lab Polymer Chem & Technol, Dept Chem, GR-54124 Thessaloniki, Macedonia, Greece
关键词
Polymethyl methacrylate; Dental fixed interim prostheses; Nanocomposites; Nanodiamonds; Reinforcement; MASTICATORY MUSCLE-ACTIVITY; FRACTURE-TOUGHNESS; POLY(METHYL METHACRYLATE); MECHANICAL-PROPERTIES; DENTAL COMPOSITES; IMPACT STRENGTH; ACRYLIC RESINS; FPD MATERIALS; GLASS-FIBER; POLYMER;
D O I
10.4012/dmj.2010-135
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
The aim of this study was to investigate the possible reinforcement of Nanodiamonds (ND) in a PMMA resin for fixed interim restorations. The fracture toughness (K-1c), impact strength and the dynamic thermomechanical properties (T-g, E', E '', tan delta) of a series of PMMA-ND nanocomposites with different amounts of ND were evaluated. The fracture toughness increased as the ND percentage increased up to 0.38% wt but a greater amount of ND induced a decrease in K-1c. Impact strength and Young's modulus were also increased by increasing nanoparticles content, indicating the reinforcing effect of ND. Dynamic mechanical properties were also affected. By increasing the ND content an increase of storage modulus was recorded, while glass transition was shifted at higher temperatures. Under the limitations of this study, it can be suggested that reinforcing PMMA with ND nanoparticles-especially at low concentrations-may increase the overall performance of fixed interim prostheses.
引用
收藏
页码:222 / 231
页数:10
相关论文
共 62 条
[1]  
ASTM, D256 ASTM
[2]   Nanodiamond-Polymer Composite Fibers and Coatings [J].
Behler, Kristopher D. ;
Stravato, Antonella ;
Mochalin, Vadym ;
Korneva, Guzeliya ;
Yushin, Gleb ;
Gogotsi, Yury .
ACS NANO, 2009, 3 (02) :363-369
[3]   Preparation bv melt mixing and characterization of isotactic polypropylene/SiO2 nanocomposites containing untreated and surface-treated nanoparticles [J].
Bikiaris, DN ;
Papageorgiou, GZ ;
Pavlidou, E ;
Vouroutzis, N ;
Palatzoglou, P ;
Karayannidis, GP .
JOURNAL OF APPLIED POLYMER SCIENCE, 2006, 100 (04) :2684-2696
[4]  
*BS EN ISO, 2005, 127372005 BS EN ISO
[5]   The thermal stability of nanodiamond surface groups and onset of nanodiamond graphitization [J].
Butenko, Yu. V. ;
Kuznetsov, V. L. ;
Paukshtis, E. A. ;
Stadnichenko, A. I. ;
Mazov, I. N. ;
Moseenkov, S. I. ;
Boronin, A. I. ;
Kosheev, S. V. .
FULLERENES NANOTUBES AND CARBON NANOSTRUCTURES, 2006, 14 (2-3) :557-564
[6]  
Callister WD, 2006, MAT SCI ENG INTRO, V7th, P232
[7]  
CHARTOFF RP, 1994, AM SOC TEST MATER, V1249, P88, DOI 10.1520/STP15367S
[8]   Nanoconfinement revealed in degradation and relaxation studies of two structurally different polystyrene-clay systems [J].
Chen, Kai ;
Wilkie, Charles A. ;
Vyazovkin, Sergey .
JOURNAL OF PHYSICAL CHEMISTRY B, 2007, 111 (44) :12685-12692
[9]  
Craig R., 2002, RESTORATIVE DENT MAT, V11th, P640
[10]  
CULBERTSON T, 1999, TECHNOLOGY, V10, P275