Formation, Evolution and Final Structure of Interface in 2024Al Joints Fabricated by Explosive Welding

被引:4
|
作者
Xia Meng [1 ]
Fu Yanshu [1 ]
Hu Xiaowu [1 ]
机构
[1] Nanchang Univ, Sch Mech & Elect Engn, Nanchang 330031, Jiangxi, Peoples R China
来源
JOURNAL OF WUHAN UNIVERSITY OF TECHNOLOGY-MATERIALS SCIENCE EDITION | 2017年 / 32卷 / 05期
基金
中国国家自然科学基金;
关键词
explosive welding; instability; interface morphology; fractal dimensions; INSTABILITY;
D O I
10.1007/s11595-017-1727-2
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
The wavy interface for similar or the same metal explosive welding (EXW) and the universal mechanism of wavy interface formation in EXW were studied in this work. Based on a new established model, it was deduced that the evolution frequencies of the instability were constrained in a limited range. Then experiments of identical metal EXW were performed and welding interfaces were characterized for examining the final morphology. By calculating the fractal dimensions and multifractal spectra of welding interface, the fractal characteristics of interface were revealed and a quantitative description was achieved for EXW interface structure. Thus, the formation, evolution and final morphology of wavy interface were systemically researched.
引用
收藏
页码:1171 / 1178
页数:8
相关论文
共 50 条
  • [1] Formation, Evolution and Final Structure of Interface in 2024Al Joints Fabricated by Explosive Welding
    夏萌
    付艳恕
    HU Xiaowu
    Journal of Wuhan University of Technology(Materials Science), 2017, (05) : 1171 - 1178
  • [2] Formation, evolution and final structure of interface in 2024Al joints fabricated by explosive welding
    Meng Xia
    Yanshu Fu
    Xiaowu Hu
    Journal of Wuhan University of Technology-Mater. Sci. Ed., 2017, 32 : 1171 - 1178
  • [3] Laser welding of SiCp/2024Al composites with novel TiB2/2024Al composite filler
    Han, Ke
    Han, Rui
    Li, Xiaopeng
    Zhang, Xingyue
    Li, Hongliang
    Wang, Jianhao
    Wang, Kehong
    MATERIALS LETTERS, 2023, 349
  • [4] Interface microstructure morphology and formation evolution mechanism of Al-1060/Cu-T2 composites fabricated by explosive welding method
    Liang Hanliang
    Luo Ning
    Chen Yanlong
    Wang Jinxiang
    Wang Guiji
    Zhai Cheng
    Li Xiaojie
    COMPOSITE INTERFACES, 2022, 29 (05) : 465 - 485
  • [5] HRTEM Study of Interface Structure in Al2O3/2024Al Composite
    Bai Pucun
    Pei Jie
    Dai Xiongjie
    Zhao Chunwang
    Xing Yongming
    RARE METAL MATERIALS AND ENGINEERING, 2009, 38 : 1 - 5
  • [6] Microstructure and texture distribution in the bonding interface of Cu/Al composite tube fabricated by explosive welding
    Jiang, Li
    Luo, Ning
    Liang, Hanliang
    Zhao, Yang
    INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2022, 123 (9-10): : 3021 - 3031
  • [7] Microstructure and texture distribution in the bonding interface of Cu/Al composite tube fabricated by explosive welding
    Li Jiang
    Ning Luo
    Hanliang Liang
    Yang Zhao
    The International Journal of Advanced Manufacturing Technology, 2022, 123 : 3021 - 3031
  • [8] Aging behavior of AlNp/2024Al composites fabricated by squeeze casting
    School of Materials Science and Engineering, Harbin Institute of Technology, Harbin 150001, China
    不详
    Trans Nonferrous Met Soc China, 2006, SUPPL. 3 (1450-1454):
  • [9] Weldability window and the effect of interface morphology on the properties of Al/Cu/Al laminated composites fabricated by explosive welding
    Athar, M. M. Hoseini
    Tolaminejad, Behzad
    MATERIALS & DESIGN, 2015, 86 : 516 - 525
  • [10] Aging behavior of AlNp/2024Al composites fabricated by squeeze casting
    Wu Gao-hui
    Chen Guo-qin
    Jiang Long-tao
    Luan Bai-feng
    Kono, N.
    Haitani, T.
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2006, 16 : S1450 - S1454