Reducing Negative Effects of Oxidation on Flotation of Complex Cu-Zn Sulfide Ores

被引:5
作者
Ozcelik, Seda [1 ]
Ekmekci, Zafir [1 ]
机构
[1] Hacettepe Univ, Dept Min Engn, TR-06800 Ankara, Turkey
关键词
oxidation; flotation; depressants; CHALCOPYRITE CUFES2; SURFACE OXIDATION; PRODUCTS; SPHALERITE; ACTIVATION; MINERALS; PULP;
D O I
10.3390/min12081016
中图分类号
P3 [地球物理学]; P59 [地球化学];
学科分类号
0708 ; 070902 ;
摘要
Surface oxidation of the sulfide minerals negatively affects the flotation performance, i.e., the selectivity and even the recoveries at heavy oxidation conditions. Oxidation may take place during the formation of the ore, during mining and stockpiling, and during the flotation process. Stockpiling of large amounts of ore is a common practice in mine sites for blending the process-plant feed. However, a long stockpiling time may cause severe surface oxidation of the complex sulfide ores, particularly the complex Cu-Zn sulfide ores containing secondary copper minerals, which resulted in loss of Cu-Zn selectivity and copper recovery. A complex Cu-Zn sulfide ore was used to investigate effects of stockpile time on flotation performance and to determine the most efficient mitigation method to restore the flotation performance. Batch-scale flotation tests were performed on a heavily oxidized sample using sulfidization, high intensity conditioning, and their combination. The results showed that sulfidization desliming and stage addition of depressants during flotation was the most effective method for producing a copper concentrate from oxidized ores.
引用
收藏
页数:13
相关论文
共 38 条
  • [31] Dual effects of sodium sulfide on the flotation behavior of chalcopyrite: I. Effect of pulp potential
    Taheri, Bijan
    Abdollahy, Mahmoud
    Tonkaboni, Sied Ziaedin Shafaei
    Javadian, Soheyla
    Yarahmadi, Mohammadreza
    [J]. INTERNATIONAL JOURNAL OF MINERALS METALLURGY AND MATERIALS, 2014, 21 (05) : 415 - 422
  • [32] Tayebi-Khorami M., 2018, P IMPC 2018 29 INT M
  • [33] Surface oxidation of chalcopyrite (CuFeS2) under ambient atmospheric and aqueous (pH 2-10) conditions:: Cu, Fe L- and OK-edge X-ray spectroscopy
    Todd, EC
    Sherman, DM
    Purton, JA
    [J]. GEOCHIMICA ET COSMOCHIMICA ACTA, 2003, 67 (12) : 2137 - 2146
  • [34] VAUGHAN DJ, 1995, AM MINERAL, V80, P725
  • [35] Cu adsorption on pyrite (100):: Ab initio and spectroscopic studies
    von Oertzen, G. U.
    Skinner, W. M.
    Nesbitt, H. W.
    Pratt, A. R.
    Buckley, A. N.
    [J]. SURFACE SCIENCE, 2007, 601 (24) : 5794 - 5799
  • [36] Wills B.A, 2015, WILLS MINERAL PROCES, DOI 10.1016/B978-0-08-097053-0.00004-2
  • [37] COLLECTORLESS FLOTATION OF CHALCOPYRITE AND SPHALERITE ORES BY USING SODIUM SULFIDE
    YOON, RH
    [J]. INTERNATIONAL JOURNAL OF MINERAL PROCESSING, 1981, 8 (01) : 31 - 48
  • [38] The role of surface cleaning in high intensity conditioning
    Yu, Yuexian
    Ma, Liqiang
    Wu, Lun
    Ye, Guichuan
    Sun, Xianfeng
    [J]. POWDER TECHNOLOGY, 2017, 319 : 26 - 33