关键词
hemp fiber; thermogravimetric analysis; epoxy resin; mechanical properties; activation energy; REINFORCED POLYESTER; EPOXY COMPOSITES; THERMAL-BEHAVIOR; BOND STRENGTH; JUTE FIBERS; HEMP; FLAX; CELLULOSE; LIGNIN; RESIN;
D O I
10.1002/app.31335
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Industrial hemp fibers were treated with a 5 wt % NaOH, 2 wt % Na2SO3 solution at 120 degrees C for 60 min to remove noncellulosic fiber components. Analysis of fibers by lignin analysis, scanning electron microscopy (SEM), zeta potential, Fourier transform infrared (FTIR) spectroscopy, wide angle X-ray diffraction (WAXRD) and differential thermal/thermogravimetric analysis (DTA/TGA), supported that alkali treatment had (i) removed lignin, (ii) separated fibers from their fiber bundles, (iii) exposed cellulose hydroxyl groups, (iv) made the fiber surface cleaner, and (v) enhanced thermal stability of the fibers by increasing cellulose crystallinity through better packing of cellulose chains. Untreated and alkali treated short (random and aligned) and long (aligned) hemp fiber/epoxy composites were produced with fiber contents between 40 and 65 wt %. Although alkali treatment generally improved composite strength, better strength at high fiber contents for long fiber composites was achieved with untreated fiber, which appeared to be due to less fiber/fiber contact between alkali treated fibers. Composites with 65 wt % untreated, long aligned fiber were the strongest with a tensile strength (TS) of 165 MPa, Young's modulus (YM) of 17 GPa, flexural strength of 180 MPa, flexural modulus of 9 GPa, impact energy (IE) of 14.5 kJ/m(2), and fracture toughness (K-Ic) of 5 MPa m(1/2). (C) 2010 Wiley Periodicals, Inc. J Appl Polym Sci 119: 3696-3707, 2011
引用
收藏
页码:3696 / 3707
页数:12
相关论文
共 47 条
[1]   Physical and mechanical characterization of jute fabric composites [J].
Acha, BA ;
Marcovich, NE ;
Reboredo, MM .
JOURNAL OF APPLIED POLYMER SCIENCE, 2005, 98 (02) :639-650
[2]  
BECKERMANN GW, 2004, 2 INT C STRUCT P PRO, P257
[3]   Influence of chemical modifications on water-sorption and mechanical properties of Agave fibres [J].
Bessadok, A. ;
Marais, S. ;
Roudesli, S. ;
Lixon, C. ;
Metayer, M. .
COMPOSITES PART A-APPLIED SCIENCE AND MANUFACTURING, 2008, 39 (01) :29-45
[4]   Surface characterization of flax, hemp and cellulose fibers; Surface properties and the water uptake behavior [J].
Bismarck, A ;
Aranberri-Askargorta, I ;
Springer, J ;
Lampke, T ;
Wielage, B ;
Stamboulis, A ;
Shenderovich, I ;
Limbach, HH .
POLYMER COMPOSITES, 2002, 23 (05) :872-894
[5]   Unidirectional hemp and flax EP- and PP-composites: Influence of defined fiber treatments [J].
Bledzki, AK ;
Fink, HP ;
Specht, K .
JOURNAL OF APPLIED POLYMER SCIENCE, 2004, 93 (05) :2150-2156
[6]  
Bledzki AK, 1996, J APPL POLYM SCI, V59, P1329, DOI 10.1002/(SICI)1097-4628(19960222)59:8<1329::AID-APP17>3.0.CO
[7]  
2-0
[9]   COMPARATIVE STUDIES ON CELLULOLYTIC ENZYME LIGNIN AND MILLED WOOD LIGNIN OF SWEETGUM AND SPRUCE [J].
CHANG, HM ;
COWLING, EB ;
BROWN, W ;
ADLER, E ;
MIKSCHE, G .
HOLZFORSCHUNG, 1975, 29 (05) :153-159
[10]  
CLARK JA, 1985, PULP TECHN TREATM PA