Chemical Passivation Stabilizes Zn Anode

被引:114
作者
He, Pan [1 ,2 ,3 ]
Huang, Jiaxing [1 ,2 ,3 ]
机构
[1] Westlake Inst Adv Study, Hangzhou 310024, Zhejiang, Peoples R China
[2] Westlake Univ, Sch Engn, Hangzhou 310024, Zhejiang, Peoples R China
[3] Northwestern Univ, Dept Mat Sci & Engn, Evanston, IL 60208 USA
关键词
cycling stability; defect-tolerant; surface passivation; Zn anodes; ZINC; ELECTRODEPOSITION; DEPOSITION; DISSOLUTION; REDOX;
D O I
10.1002/adma.202109872
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Aqueous zinc ion batteries are an attractive option for grid-scale energy storage, which is vital to the integration of renewable energy resources with the electric energy infrastructure. The cycling stability of aqueous ZIBs is determined by the electrochemical reversibility of Zn anode, which is often deteriorated by its corrosion and dendritic Zn deposition. Here, a simple and rapid surface passivation strategy that can drastically improve the cycling stability of Zn anodes is demonstrated. For example, a dip in KMnO4 solution readily forms a continuous, conformal, and robust protective layer on the native Zn surface, leading to a more uniform plating/stripping process, increased corrosion resistance, and tolerance to manufacturing and processing defects on Zn metal electrodes. The Zn electrode cycling stabilities at 1 mA cm(-2) and 1 mA h cm(-2) are extended by approximate to 40 times. In full battery tests in the configuration of Zn||beta-MnO2, the full cell with passivated Zn anode exhibited a capacity retention of 68.7% after 300 cycles at a current density of 1.0 A g(-1), while the cell with untreated Zn anode can only retain 7.4% of capacity under the same conditions.
引用
收藏
页数:9
相关论文
共 46 条
  • [1] Ethoxylated fatty alcohols as corrosion inhibitors for dissolution of zinc in hydrochloric acid
    Abdallah, M
    [J]. CORROSION SCIENCE, 2003, 45 (12) : 2705 - 2716
  • [2] Surface characterisation of cerium layers on galvanised steel
    Arenas, MA
    de Damborenea, JJ
    [J]. SURFACE & COATINGS TECHNOLOGY, 2004, 187 (2-3) : 320 - 325
  • [3] Zinc electrodeposition in the presence of polyethylene glycol 20000
    Ballesteros, J. C.
    Diaz-Arista, P.
    Meas, Y.
    Ortega, R.
    Trejo, G.
    [J]. ELECTROCHIMICA ACTA, 2007, 52 (11) : 3686 - 3696
  • [4] Revised Pourbaix diagrams for zinc at 25-300 degrees C
    Beverskog, B
    Puigdomenech, I
    [J]. CORROSION SCIENCE, 1997, 39 (01) : 107 - 114
  • [5] Scientific Challenges for the Implementation of Zn-Ion Batteries
    Blanc, Lauren E.
    Kundu, Dipan
    Nazar, Linda F.
    [J]. JOULE, 2020, 4 (04) : 771 - 799
  • [6] Chemically resistant Cu-Zn/Zn composite anode for long cycling aqueous batteries
    Cai, Zhao
    Ou, Yangtao
    Wang, Jindi
    Xiao, Run
    Fu, Lin
    Yuan, Zhu
    Zhan, Renmin
    Sun, Yongming
    [J]. ENERGY STORAGE MATERIALS, 2020, 27 : 205 - 211
  • [7] Quantitative phase-field modeling of dendritic electrodeposition
    Cogswell, Daniel A.
    [J]. PHYSICAL REVIEW E, 2015, 92 (01):
  • [8] Quasi-Isolated Au Particles as Heterogeneous Seeds To Guide Uniform Zn Deposition for Aqueous Zinc-Ion Batteries
    Cui, Mangwei
    Xiao, Yan
    Kang, Litao
    Du, Wei
    Gao, Yanfeng
    Sun, Xueqin
    Zhou, Yanli
    Li, Xiangming
    Li, Hongfei
    Jiang, Fuyi
    Zhi, Chunyi
    [J]. ACS APPLIED ENERGY MATERIALS, 2019, 2 (09) : 6490 - 6496
  • [9] Oxygen Defects in β-MnO2 Enabling High-Performance Rechargeable Aqueous Zinc/Manganese Dioxide Battery
    Han, Mingming
    Huang, Jiwu
    Liang, Shuquan
    Shan, Lutong
    Xie, Xuesong
    Yi, Zhenyu
    Wang, Yiren
    Guo, Shan
    Zhou, Jiang
    [J]. ISCIENCE, 2020, 23 (01)
  • [10] Detrimental Effects of Surface Imperfections and Unpolished Edges on the Cycling Stability of a Zinc Foil Anode
    He, Pan
    Huang, Jiaxing
    [J]. ACS ENERGY LETTERS, 2021, 6 (05): : 1990 - 1995