Crack nucleation and growth during dynamic indentation of chemically-strengthened glass

被引:13
|
作者
Kang, M. [1 ,2 ]
Li, W. [1 ,2 ]
Leong, A. F. T. [1 ]
Guan, M. [3 ]
Fezzaa, K. [4 ]
Harris, J. T. [5 ]
Ramesh, K. T. [1 ,2 ,3 ]
Hufnagel, T. C. [1 ,2 ,3 ]
机构
[1] Johns Hopkins Univ, Hopkins Extreme Mat Inst, Baltimore, MD 21218 USA
[2] Johns Hopkins Univ, Dept Mech Engn, Baltimore, MD 21218 USA
[3] Johns Hopkins Univ, Dept Mat Sci & Engn, Baltimore, MD 21218 USA
[4] Argonne Natl Lab, Xray Sci Div, Argonne, IL 60439 USA
[5] Corning Inc, Corning, NY 14831 USA
关键词
Indentation; X-ray phase contrast imaging; Chemically-strengthened glass; BRITTLE SOLIDS; IN-SITU; DEFORMATION; INITIATION; FRACTURE; STRESS;
D O I
10.1016/j.eml.2020.100754
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Dynamic point impact loading is a primary cause of fracture of glass screens on mobile devices. An improved understanding of crack initiation and evolution under high-speed indentation could contribute to the development of materials with better performance, but experimental observations are challenging due to the short timescales and limited depth-of-field of optical microscopy. To address this need, we have observed fracture of a chemically-strengthened glass during dynamic indentation using in situ x-ray phase-contrast imaging (XPCI). Median cracks initiate below the surface of the glass, at a depth approximately corresponding to the depth at which the surface residual compressive stress diminishes to zero. These cracks initially propagate at similar to 10 m s(-1), rapidly accelerating to > 100 m s(-1). We also observe some evidence for rate-dependent behavior, in that indentation at the lowest rates studied here (below about similar to 0.15 m s(-1)) fails to initiate cracks regardless of the depth of the indentation (up to 18 mu m), while indentation at higher rates produces median cracks that either arrest or cause complete fracture, depending on the depth of indentation. (C) 2020 Elsevier Ltd. All rights reserved.
引用
收藏
页数:6
相关论文
共 50 条
  • [1] PRODUCTION OF CHEMICALLY-STRENGTHENED GLASS CONTAINERS.
    Ono, H.
    Glass, 1983, 60 (10): : 380 - 383
  • [2] Subcritical crack growth and lifetime prediction of chemically strengthened aluminosilicate glass
    Jiang, Liangbao
    Wang, Yi
    Mohagheghian, Iman
    Li, Xiaoyu
    Guo, Xintao
    Li, Lei
    Dear, John P.
    Yan, Yue
    MATERIALS & DESIGN, 2017, 122 : 128 - 135
  • [3] SLOW SURFACE CRACK GROWTH DURING VICKERS INDENTATION ON GLASS
    PHILLIPS, K
    JOURNAL OF MATERIALS SCIENCE, 1976, 11 (12) : 2354 - 2356
  • [4] Analysis of macroscopic crack branching patterns in chemically strengthened glass
    J.E. Kooi
    R. Tandon
    S.J. Glass
    J.J. Mecholsky
    Journal of Materials Research, 2008, 23 : 214 - 225
  • [5] Analysis of macroscopic crack branching patterns in chemically strengthened glass
    Kooi, J. E.
    Tandon, R.
    Glass, S. J.
    Mecholsky, J. J., Jr.
    JOURNAL OF MATERIALS RESEARCH, 2008, 23 (01) : 214 - 225
  • [6] Influence of ultra-high residual compressive stress on the static and dynamic indentation response of a chemically strengthened glass
    Jannotti, Phillip
    Subhash, Ghatu
    Ifju, Peter
    Kreski, Patrick K.
    Varshneya, Arun K.
    JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2012, 32 (08) : 1551 - 1559
  • [7] INVESTIGATION OF CRACK GROWTH DURING DYNAMIC FRACTURE OF GLASS
    FINKEL, VM
    KUTKIN, IA
    SOVIET PHYSICS-SOLID STATE, 1962, 4 (06): : 1038 - 1042
  • [8] Indentation deformation and cracking in oxide glass –toward understanding of crack nucleation
    Yoshida S.
    Journal of Non-Crystalline Solids: X, 2019, 1
  • [9] Hybridizing Shear-Stiffening Gel and Chemically-Strengthened Ultrathin Glass Sheets for Flexible Impact-Resistant Armor
    Wang, Xuchao
    Zhang, Zijing
    Liang, Zhihua
    Yao, Haimin
    ADVANCED SCIENCE, 2024, 11 (33)
  • [10] RELATION BETWEEN MULTIREGION CRACK-GROWTH AND DYNAMIC FATIGUE OF GLASS USING INDENTATION FLAWS
    CHANTIKUL, P
    LAWN, BR
    RICHTER, H
    FREIMAN, SW
    JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1983, 66 (07) : 515 - 518