Ten-year observation of dentin bonding durability of 4-META/MMA-TBB resin cement -a SEM and TEM study

被引:12
作者
Aoki, Kanako [1 ]
Kitasako, Yuichi [1 ]
Ichinose, Shizuko [2 ]
Burrow, Michael F. [3 ]
Ariyoshi, Meu [1 ]
Nikaido, Toru [1 ]
Tagami, Junji [1 ,4 ]
机构
[1] Tokyo Med & Dent Univ, Dept Restorat Sci, Grad Sch Med & Dent Sci, Bunkyo Ku, Tokyo 1138549, Japan
[2] Tokyo Med & Dent Univ, Instrumental Anal Res Ctr, Bunkyo Ku, Tokyo 1138510, Japan
[3] Univ Hong Kong, Fac Dent, Prince Philip Dent Hosp, Pokfulam, Hong Kong, Peoples R China
[4] Tokyo Med & Dent Univ, Global Ctr Excellence Program, Int Res Ctr Mol Sci Tooth & Bone Dis, Bunkyo Ku, Tokyo 1138549, Japan
基金
日本学术振兴会;
关键词
Bond durability; Resin cement; Tensile bond test; SEM; TEM; LONG-TERM DURABILITY; IN-VIVO; DEGRADATION; STRENGTH; ADHESION; NANOLEAKAGE; INTERFACE; COLLAGEN;
D O I
10.4012/dmj.2011-003
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
This study aimed to assess dentin bond durability of 4-META/MMA-TBB resin cement over ten years, by evaluating the tensile bond strength, and SEM. and TEM observations. Tensile bond strength of Super Bond C&B (SB) to bovine dentin was evaluated at 1 day and after 10 years. The mode of failure after debonding was observed by SEM. Interfacial ultrastructure and nanoleakage was observed by TEM at the baseline and after 10 y. The tensile bond strength significantly dropped after 10 y. The failure pattern shifted from cohesive failure in resin towards adhesive failure or cohesive failure in dentin. TEM observation revealed degradation of both resin and collagen networks within the hybrid layer and nanoleakage at the base of the hybrid layer after 10 y. The bond strength of SB to dentin significantly decreased, and the hybrid layer degraded, while the overlying hydrophobic resin layer showed little disintegration over 10 y.
引用
收藏
页码:438 / 447
页数:10
相关论文
共 38 条
  • [1] Akimoto T, 1991, J JPN SOC DENT MAT D, V10, P42
  • [2] Adhesion to tooth structure: A critical review of "macro" test methods
    Braga, Roberto R.
    Meira, Josete B. C.
    Boaro, Leticia C. C.
    Xavier, Tathy A.
    [J]. DENTAL MATERIALS, 2010, 26 (02) : E38 - E49
  • [3] Dentin bond durability after three years using a dentin bonding agent with and without priming
    Burrow, MF
    Satoh, M
    Tagami, J
    [J]. DENTAL MATERIALS, 1996, 12 (5-6) : 302 - 307
  • [4] Seven-year dentin bond strengths of a total- and self-etch system
    Burrow, MF
    Harada, N
    Kitasako, Y
    Nikaido, T
    Tagami, J
    [J]. EUROPEAN JOURNAL OF ORAL SCIENCES, 2005, 113 (03) : 265 - 270
  • [5] Burrow Michael F., 1993, Bulletin of Tokyo Medical and Dental University, V40, P173
  • [6] Adhesive permeability affects coupling of resin cements that utilise self-etching primers to dentine
    Carvalho, RM
    Pegoraro, TA
    Tay, FR
    Pegoraro, LF
    Silva, NRFA
    Pashley, DH
    [J]. JOURNAL OF DENTISTRY, 2004, 32 (01) : 55 - 65
  • [7] INFLUENCE OF SELECTED VARIABLES ON ADHESION TESTING
    FOWLER, CS
    SWARTZ, ML
    MOORE, BK
    RHODES, BF
    [J]. DENTAL MATERIALS, 1992, 8 (04) : 265 - 269
  • [8] NON-PRESSURE ADHESION OF A NEW ADHESIVE RESTORATIVE RESIN
    FUSAYAMA, T
    NAKAMURA, M
    KUROSAKI, N
    IWAKU, M
    [J]. JOURNAL OF DENTAL RESEARCH, 1979, 58 (04) : 1364 - 1370
  • [9] Evaluation of physical properties and surface degradation of self-adhesive resin cements
    Han, Linlin
    Okamoto, Akira
    Fukushima, Masayoshi
    Okiji, Takashi
    [J]. DENTAL MATERIALS JOURNAL, 2007, 26 (06) : 906 - 914
  • [10] SEM and TEM analysis of water degradation of human dentinal collagen
    Hashimoto, M
    Tay, FR
    Ohno, H
    Sano, H
    Kaga, M
    Yiu, C
    Kumagai, H
    Kudou, Y
    Kubota, M
    Oguchi, H
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2003, 66B (01): : 287 - 298