Objectives. Resin bonding to yttrium-oxide-partially-stabilized zirconia ceramic (YPSZ) cannot be established by standard methods that are utilized for conventional silica-based dental ceramics. It was our hypothesis that adhesive bonding methods suitable for glass-infiltrated alumina ceramic can also be used to bond successfully to YPSZ. To prove this hypothesis, bonding methods suitable for alumina ceramic were used on YPSZ and the tensile bond strength and their durability evaluated in vitro. Methods. Plexiglass tubes filled with resin composite were bonded to YPSZ discs following Various adhesion protocols. Groups of 16 samples were bonded using seven different bonding methods. Subgroups of eight bonded samples were tested for tensile strength following storage in distilled water (37 degrees C) for either 3 or 150 days. In addition, the 150 day samples were thermal cycled 37 500 times as a method to stress the bond interface. The statistical analysis was made with the Kruskal-Wallis test followed by multiple pair-wise comparisons of the groups using the Wilcoxon rank sum test. Results. Sandblasting alone, the additional use of a silane or acrylizing resulted in an initial bond of a conventional BisGMA resin composite to YPSZ which failed spontaneously over storage time. The use of the BisGMA resin composite after tribochemical silica coating of YPSZ and the use of a polyacid-modified resin composite after sandblasting of YPSZ resulted in an initial bond which decreased significantly over storage time (p=0.05). A durable resin bond to YPSZ was achieved only after sandblasting the ceramic and using one of two resin composites containing a special phosphate monomer. Significance. A durable bond to YPSZ was achieved only by using resin composites with a special adhesive monomer. Therefore, the hypothesis of the study was partially proved as a durable bond to alumina ceramic is achieved with the same resin composites. However, it was partially disproved as tribochemical silica coating of YPSZ did not result in a durable resin bond as it does on glass-infiltrated alumina ceramic. (C) 1998 Academy of Dental Materials. Published by Elsevier Science Ltd.
引用
收藏
页码:64 / 71
页数:8
相关论文
共 33 条
  • [1] INTERFACE HISTOLOGY OF UNLOADED AND EARLY LOADED PARTIALLY-STABILIZED ZIRCONIA ENDOSSEOUS IMPLANT IN INITIAL BONE HEALING
    AKAGAWA, Y
    ICHIKAWA, Y
    NIKAI, H
    TSURU, H
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 1993, 69 (06) : 599 - 604
  • [2] [Anonymous], 1989, Transformation toughening of ceramics
  • [3] BOND STRENGTHS OF 3 CHEMICAL ADHESIVE CEMENTS ADHERED TO A NICKEL-CHROMIUM ALLOY FOR DIRECT BONDED RETAINERS
    ATTA, MO
    SMITH, BGN
    BROWN, D
    [J]. JOURNAL OF PROSTHETIC DENTISTRY, 1990, 63 (02) : 137 - 143
  • [4] DICOR SURFACE TREATMENTS FOR ENHANCED BONDING
    BAILEY, LF
    BENNETT, RJ
    [J]. JOURNAL OF DENTAL RESEARCH, 1988, 67 (06) : 925 - 931
  • [5] LONG-TERM IN-VIVO AND IN-VITRO AGING OF A ZIRCONIA CERAMIC USED IN ORTHOPAEDY
    CALES, B
    STEFANI, Y
    LILLEY, E
    [J]. JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1994, 28 (05): : 619 - 624
  • [6] Chang J C, 1993, J Prosthodont, V2, P110, DOI 10.1111/j.1532-849X.1993.tb00391.x
  • [7] CHRISTEL PS, 1989, B HOSP JOINT DIS ORT, V49, P170
  • [8] Dietschi D, 1997, INT J PROSTHODONT, V10, P498
  • [9] HEIDE S, 1996, P 20 ANN C EUR PROST, P94
  • [10] HOLM S, 1979, SCAND J STAT, V6, P65