ZrB2-SiC as a protective coating for C/SiC composites: Effect of high temperature oxidation on thermal shock property and protection mechanism

被引:21
作者
Yang, Xiang [1 ]
Feng, Cao [1 ]
Qing, Wang [1 ]
机构
[1] Natl Univ Def Technol, Sci & Technol Adv Ceram Fibers & Composites Lab, Changsha 410073, Hunan, Peoples R China
来源
JOURNAL OF ASIAN CERAMIC SOCIETIES | 2016年 / 4卷 / 02期
基金
中国国家自然科学基金;
关键词
Ceramic-matrix composites (CMCs); Corrosion; Fracture; Mechanical properties; High-temperature properties; CERAMIC COMPOSITES; MATRIX COMPOSITES; BEHAVIOR; INFILTRATION; FIBER; POLYCARBOSILANE;
D O I
10.1016/j.jascer.2016.02.001
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
ZrB2-SiC coating was prepared on C/SiC composites surface by slurry method, and then the thermal fatigue behavior of ZrB2-SiC coated C/SiC composites was studied. The composition of the coating layers was characterized by XRD, SEM and EDS. With the thickness was 200 tun, the coating was ZrB2 and SiC. During thermal cycle between 1773 K in air and 373 K in boiling water, the weight of the ZrB2-SiC coated composites decreased lightly. The decrease of the flexural strength during the thermal cycle was primarily due to the debonding of the fiber-matrix interfaces and the oxidation of the coated samples. Compared with the uncoated C/SiC composites, the coating played an important role in enhancing the resistance to the thermal shock. (C) 2016 The Ceramic Society of Japan and the Korean Ceramic Society. Production and hosting by Elsevier B.V.
引用
收藏
页码:159 / 163
页数:5
相关论文
共 50 条
[31]   Wear damage tolerance and high temperature oxidation behavior of HfB2:ZrB2-SiC composites [J].
Nisar, Ambreen ;
Bajpai, Shipra ;
Khan, Mohammad Mohsin ;
Balani, Kantesh .
CERAMICS INTERNATIONAL, 2020, 46 (13) :21689-21698
[32]   Effect of SiC Nanowires on the Mechanical and Oxidation Protective Ability of SiC Coating for C/C Composites [J].
Chu Yanhui ;
Fu Qiangang ;
Li Hejun ;
Shi Xiaohong ;
Li Kezhi ;
Wen Xue ;
Shang Gunan .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2012, 95 (02) :739-745
[33]   Thermal shock behavior of ZrB2-SiC ultra-high temperature ceramics with addition of zirconia [J].
Li, Weijie ;
Zhang, Yong ;
Zhang, Xinghong ;
Hong, Changqing ;
Han, Wenbo .
JOURNAL OF ALLOYS AND COMPOUNDS, 2009, 478 (1-2) :386-391
[34]   Role of TiC and WC Addition on the Mechanism and Kinetics of Isothermal Oxidation and High-Temperature Stability of ZrB2-SiC Composites [J].
Sengupta, Pradyut ;
Manna, Indranil .
HIGH TEMPERATURE CORROSION OF MATERIALS, 2024, 101 (SUPPL 1) :57-83
[35]   The effect of a graphite addition on oxidation of ZrB2-SiC in air at 1500°C [J].
Rezaie, Alireza ;
Fahrenholtz, William G. ;
Hilmas, Gregory E. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2013, 33 (02) :413-421
[36]   ZrB2-SiC(Al) ceramics with high resistance to oxidation at 1500 °C [J].
Wang, Yiguang ;
Luo, Lei ;
Sun, Jing ;
An, Linan .
CORROSION SCIENCE, 2013, 74 :154-158
[37]   Oxidation and ablation resistance of the ZrB2-CrSi2-Si/SiC coating for C/C composites at high temperature [J].
Feng, Tao ;
Li, Hejun ;
Hu, Manhong ;
Lin, Hongjiao ;
Li, Lu .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 662 :302-307
[38]   Influence of angle of incidence, temperature and SiC content on erosive wear behavior of ZrB2-SiC composites [J].
Gupta, Yashpal ;
Venkateswaran, T. ;
Kumar, B. Venkata Manoj .
INTERNATIONAL JOURNAL OF APPLIED CERAMIC TECHNOLOGY, 2020, 17 (02) :459-467
[39]   Preparation and ablation properties of ZrB2-SiC protective laminae for carbon/carbon composites [J].
Wang, Dini ;
Zeng, Yi ;
Xiong, Xiang ;
Li, Guodong ;
Chen, Zhaoke ;
Sun, Wei ;
Wang, Yalei .
CERAMICS INTERNATIONAL, 2014, 40 (09) :14215-14222
[40]   Research Progress of ZrB2-SiC Based Anti-oxidation Coatings of Cf/C Composites [J].
Fang, Yaohua ;
Zhang, Zhi ;
Wang, Yongxin ;
Peng, Jie ;
Zhang, Haijun ;
Liu, Jianghao .
RARE METAL MATERIALS AND ENGINEERING, 2024, 53 (11) :3259-3270