Effect of silicon content on the microstructure evolution, mechanical properties, and biocompatibility of β-type TiNbZrTa alloys fabricated by laser powder bed fusion

被引:18
|
作者
Luo, X. [1 ,4 ]
Yang, C. [1 ]
Li, R. Y. [3 ]
Wang, H. [3 ]
Lu, H. Z. [1 ]
Song, T. [1 ]
Ma, H. W. [1 ]
Li, D. D. [2 ]
Gebert, A. [4 ]
Li, Y. Y. [1 ,2 ]
机构
[1] South China Univ Technol, Guangdong Prov Key Lab Proc & Forming Adv Metall, Natl Engn Res Ctr Nearnetshape Forming Metall Mat, Guangzhou 510640, Peoples R China
[2] Huazhong Univ Sci & Technol, State Key Lab Mat Proc & Mould Technol, Wuhan 430074, Peoples R China
[3] Jilin Univ, Second Hosp Jilin Univ, Dept Orthoped, Changchun 130041, Peoples R China
[4] Leibniz IFW Dresden, Inst Complex Mat, Helmholtzstr 20, D-01069 Dresden, Germany
来源
BIOMATERIALS ADVANCES | 2022年 / 133卷
基金
中国国家自然科学基金;
关键词
beta-Type titanium alloys; Laser powder bed fusion; Microstructure; Mechanical properties; Biocompatibility; TITANIUM-ALLOYS; SI; PHASE; STRENGTH; TRANSITION; HIP;
D O I
10.1016/j.msec.2021.112625
中图分类号
TB3 [工程材料学]; R318.08 [生物材料学];
学科分类号
0805 ; 080501 ; 080502 ;
摘要
Beta-type titanium alloys are excellent candidates for biomedical applications because of their very low elastic modulus, excellent corrosion resistance, and biocompatibility. However, many traditional beta-type titanium alloys exhibit low yield strength. In this study, a small amount of Si (3 and 5 at.%) was added to a Ti-35Nb-7Zr-5Ta (wt%, TNZT) biomedical alloy prepared via laser powder bed fusion (LPBF) to increase its yield strength. The Si addition resulted in a significant increase in the compression yield strength of the alloy (from 802 to 1282 MPa). Meanwhile, the elastic moduli of the TNZT alloys (48.7-60.6 GPa) with 3 and 5 at.% Si were much lower than that of the Ti-6Al-4 V alloy (110 GPa), which is used extensively in clinical applications. The microstructural analyses indicated that the ultrahigh-strength of the TNZT alloy containing Si was due to the presence of ultrafine (Ti, Nb, Zr)(5)Si-3 (S1) grains in the beta-Ti matrix. In addition, thin shell-shaped S1 and (Ti, Nb, Zr)(2)Si (S2) grains precipitated along the columnar beta-Ti grain boundaries in the TNZT alloys containing 3 and 5 at.% Si, respectively. Moreover, the introduction of Si to the TNZT alloy significantly refined the grains, weakened the cubic texture, decreased surface roughness, and improved Vickers hardness. The ultrahigh strength of the Si-containing TNZT alloys was due to grain boundary strengthening and precipitation strengthening. In addition, in vitro studies with MC3T3-E1 cells revealed that the cytocompatibilities of the LPBF-fabricated TNZT and Si-containing TNZT alloys were equivalent and were better than that of the LPBF-fabricated Ti-6Al-4 V alloy. In particular, the TNZT alloy with 3 at.% Si showed the best elastic modulus (48.7 +/- 1.0 GPa), yield strength (1151 +/- 17 MPa), and cell biological response among all the alloys investigated in this study, and hence was found to be a suitable candidate for application in load-bearing bone implants.
引用
收藏
页数:12
相关论文
共 50 条
  • [31] Effect of Scanning Speed on Microstructure and Properties of Inconel 718 Fabricated by Laser Powder Bed Fusion
    Qin Cheng
    Xue Yan
    Transactions of the Indian Institute of Metals, 2023, 76 : 997 - 1006
  • [32] Microstructure and mechanical properties of Al10SiMg fabricated by pulsed laser powder bed fusion
    Chou, R.
    Ghosh, A.
    Chou, S. C.
    Paliwal, M.
    Brochu, M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 689 : 53 - 62
  • [33] Microstructure and mechanical properties of crack-free Inconel 738 fabricated by laser powder bed fusion
    Jena, Ashutosh
    Atabay, Sila Ece
    Brochu, Mathieu
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2022, 850
  • [34] Microstructure development of Ti scaffold by laser powder bed fusion with chemical polishing and its mechanical properties, biocompatibility
    Lu, Changfu
    Chen, Jing
    Ma, Teng
    Chen, Yuxin
    Zeng, Da
    Gan, Yiliang
    Yang, Youwen
    BIOSURFACE AND BIOTRIBOLOGY, 2024, 10 (02) : 52 - 62
  • [35] Microstructure and mechanical evolution behavior of LPBF (laser powder bed fusion)-fabricated TA15 alloy
    Wu, Xuping
    Zhang, Dongyun
    Guo, Yanwu
    Zhang, Tai
    Liu, Zhiyuan
    JOURNAL OF ALLOYS AND COMPOUNDS, 2021, 873
  • [36] Microstructure and mechanical evolution behavior of LPBF (laser powder bed fusion)-fabricated TA15 alloy
    Zhang, Dongyun (zhangdy@bjut.edu.cn), 1600, Elsevier Ltd (873):
  • [37] Characteristics of β-type Ti-41Nb alloy produced by laser powder bed fusion: Microstructure, mechanical properties and in vitro biocompatibility
    Zhongjie Li
    Jiajun Qiu
    Hao Xu
    Anping Dong
    Lin He
    Guoliang Zhu
    Dafan Du
    Hui Xing
    Xuanyong Liu
    Baode Sun
    Journal of Materials Science & Technology, 2022, 124 (29) : 260 - 272
  • [38] Improving the microstructure and mechanical properties of laser powder bed fusion-fabricated tantalum by high laser energy density
    Du, Jingguang
    Ren, Yaojia
    Zhang, Mingming
    Liang, Luxin
    Chen, Chao
    Zhou, Kechao
    Liu, Xinyan
    Xu, Feng
    Baker, Ian
    Wu, Hong
    MATERIALS LETTERS, 2023, 333
  • [39] Effect of solution treatment on microstructure and mechanical properties of AZ91D alloy fabricated by laser powder bed fusion
    Xu W.-H.
    Zhang Z.-W.
    Li J.-K.
    Yuan H.-W.
    An G.-J.
    Shi H.
    Li W.
    Wei Q.-S.
    Zhongguo Youse Jinshu Xuebao/Chinese Journal of Nonferrous Metals, 2023, 33 (11): : 3638 - 3649
  • [40] Effect of heat treatment on microstructure and mechanical properties of AlSi10Mg fabricated using laser powder bed fusion
    Huang, Nancy
    Luo, Qixiang
    Bartles, Dean L.
    Simpson, Timothy W.
    Beese, Allison M.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2024, 895