Microstructure and mechanical properties of laser additive repaired Ti17 titanium alloy

被引:36
作者
Zhao, Zhuang [1 ,2 ]
Chen, Jing [1 ,2 ]
Zhang, Qiang [1 ,2 ]
Tan, Hua [1 ,2 ]
Lin, Xin [1 ,2 ]
Huang, Wei-dong [1 ,2 ]
机构
[1] Northwestern Polytech Univ, State Key Lab Solidificat Proc, Xian 710072, Shaanxi, Peoples R China
[2] Northwestern Polytech Univ, Key Lab Met High Performance Addit Mfg & Innovat, Minist Ind & Informat Technol, Xian 710072, Shaanxi, Peoples R China
基金
中国国家自然科学基金;
关键词
laser additive repair; Ti17 titanium alloy; microstructure; mechanical properties; deformation behavior; TI-5AL-2SN-2ZR-4MO-4CR ALLOY; MELTING DEPOSITION; FATIGUE BEHAVIOR; TI-6AL-4V ALLOY; EVOLUTION; STEEL; TRANSFORMATION; COMPONENTS;
D O I
10.1016/S1003-6326(17)60289-9
中图分类号
TF [冶金工业];
学科分类号
0806 ;
摘要
Laser additive manufacturing technology with powder feeding was employed to repair wrought Ti17 titanium alloy with small surface defects. The microstructure, micro-hardness and room temperature tensile properties of laser additive repaired (LARed) specimen were investigated. The results show that, cellular substructures are observed in the laser deposited zone (LDZ), rather than the typical alpha laths morphology due to lack of enough subsequent thermal cycles. The cellular substructures lead to lower micro-hardness in the LDZ compared with the wrought substrate zone which consists of duplex microstructure. The tensile test results indicate that the tensile deformation process of the LARed specimen exhibits a characteristic of dramatic plastic strain heterogeneity and fracture in the laser repaired zone with a mixed dimple and cleavage mode. The tensile strength of the LARed specimen is slightly higher than that of the wrought specimen and the elongation of 11.7% is lower.
引用
收藏
页码:2613 / 2621
页数:9
相关论文
共 29 条
[1]   Experimental and numerical study of strength mismatch in cross-weld tensile testing [J].
Acar, Murat O. ;
Gungor, Salih .
JOURNAL OF STRAIN ANALYSIS FOR ENGINEERING DESIGN, 2015, 50 (06) :349-365
[2]  
[Anonymous], 2004, P 23 INT C APPL LAS
[3]   The mechanical and microstructural characteristics of laser-deposited IN718 [J].
Blackwell, PL .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2005, 170 (1-2) :240-246
[4]  
Chen J, 2006, T NONFERR METAL SOC, V16, pS2104
[5]  
CHEN Jing, 2011, CHINESE J LASERS, V38
[6]   Laser metal deposition as repair technology for stainless steel and titanium alloys [J].
Graf, Benjamin ;
Gumenyuk, Andrey ;
Rethmeier, Michael .
LASER ASSISTED NET SHAPE ENGINEERING 7 (LANE 2012), 2012, 39 :376-381
[7]   A comparison of tool-repair methods using CO2 laser surfacing and arc surfacing [J].
Grum, J ;
Slabe, JM .
APPLIED SURFACE SCIENCE, 2003, 208 :424-431
[8]   Low cycle fatigue behavior of laser melting deposited TC18 titanium alloy [J].
Li, Zhen ;
Tian, Xiang-jun ;
Tang, Hai-bo ;
Wang, Hua-ming .
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2013, 23 (09) :2591-2597
[9]   Microstructure and mechanical behavior of commercial purity Ti/Ti-6Al-2Zr-1Mo-1V structurally graded material fabricated by laser additive manufacturing [J].
Liang, Yao-Jian ;
Liu, Dong ;
Wang, Hua-Ming .
SCRIPTA MATERIALIA, 2014, 74 :80-83
[10]   Microstructure and mechanical properties of laser forming repaired 17-4PH stainless steel [J].
Lin, Xin ;
Cao, Yongqing ;
Wu, Xiaoyu ;
Yang, Haiou ;
Chen, Jing ;
Huang, Weidong .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2012, 553 :80-88