Zn isotopes fractionation during slags' weathering: One source of contamination, multiple isotopic signatures

被引:14
作者
Yin, Nang-Htay [1 ,2 ,3 ]
van Hullebusch, Eric D. [1 ,3 ]
Benedetti, Marc [2 ]
Lens, Piet N. L. [3 ]
Sivry, Yann [2 ]
机构
[1] Univ Paris Est, Lab Geomat & Environm, EA 4508, UPEM, F-77454 Marne La Vallee, France
[2] Univ Paris Diderot, Sorbonne Paris Cite, Inst Phys Globe Paris, UMR 7154,CNRS, F-75005 Paris, France
[3] IHE Delft Inst Water Educ, POB 3015, NL-2601 DA Delft, Netherlands
关键词
Zn isotopes; Fractionation; Dissolution; Precipitation; Slags; Alteration; LBF; ISF; PRIMARY LEAD; AQUEOUS-SOLUTIONS; TRACE-ELEMENTS; ICP-MS; ZINC; PB; CU; METAL; DEPOSITIONS; ADSORPTION;
D O I
10.1016/j.chemosphere.2017.11.184
中图分类号
X [环境科学、安全科学];
学科分类号
08 ; 0830 ;
摘要
During the chemical weathering of lead blast furnace (LBF) and imperial smelting furnace (ISF) slags, possible Zn isotopes fractionation was studied as a function of pH, atmosphere (open air vs nitrogen), and time. Bulk LBF and ISF displayed heavier signatures compared to Johnson Matthey Company (JMC) Zn standard solution (i.e. 0.13 +/- 0.06 parts per thousand and 0.78 +/- 0.13 parts per thousand for LBF and ISF, resp). The Zn signatures vary greatly by changes in solution pH; heavier signatures at low pH and lighter signature at high pH. Smithsonite (ZnCO3) formation could induce a big delta Delta Zn-66(Nitro-Open.atm) of 1.13 parts per thousand at pH 10 and rapid zinc hydroxide precipitation could induce Delta Zn-66(Nitro-Open.atm) of 0.13-0.2 parts per thousand at pH 8.5. In addition, slags contain many mineral phases: similar to 80-84% of amorphous glassy phase (in v/v) and similar to 16-20% of many other crystalline phases. Zn isotope signatures in primary mineral phases can be extrapolated where the signature of the amorphous glassy phase lies between-035 parts per thousand and -0.42 parts per thousand, and that of the overall crystalline phases was estimated to be 2.12 parts per thousand for LBF and 5.74 parts per thousand for ISF. Therefore, un-weathered slags with many mineral phases can host distinct Zn isotope signatures, which further evolve significantly during chemical weathering. One should thus carefully consider the heterogeneity of slags and the low-temperature chemical processes which lead to diverse Zn isotopic signature in the end, when using Zn isotopes as tracer of smelter's contamination. (C) 2017 Elsevier Ltd. All rights reserved.
引用
收藏
页码:483 / 490
页数:8
相关论文
共 38 条
  • [1] Fifty-year sedimentary record of heavy metal pollution (Cd, Zn, Cu, Pb) in the Lot River reservoirs (France)
    Audry, S
    Schäfer, J
    Blanc, G
    Jouanneau, JM
    [J]. ENVIRONMENTAL POLLUTION, 2004, 132 (03) : 413 - 426
  • [2] Leaching assessment of road materials containing primary lead and zinc slags
    Barna, R
    Moszkowicz, P
    Gervais, C
    [J]. WASTE MANAGEMENT, 2004, 24 (09) : 945 - 955
  • [3] Separation of copper, iron, and zinc from complex aqueous solutions for isotopic measurement
    Borrok, D. M.
    Wanty, R. B.
    Ridley, W. I.
    Wolf, R.
    Lamothe, P. J.
    Adams, M.
    [J]. CHEMICAL GEOLOGY, 2007, 242 (3-4) : 400 - 414
  • [4] Evaluation of silica-water surface chemistry using NMR spectroscopy
    Carroll, SA
    Maxwell, RS
    Bourcier, W
    Martin, S
    Hulsey, S
    [J]. GEOCHIMICA ET COSMOCHIMICA ACTA, 2002, 66 (06) : 913 - 926
  • [5] Direct separation of Zn from dilute aqueous solutions for isotope composition determination using multi-collector ICP-MS
    Chen, Jiu-Bin
    Louvat, Pascale
    Gaillardet, Jerome
    Birck, Jean-Louis
    [J]. CHEMICAL GEOLOGY, 2009, 259 (3-4) : 120 - 130
  • [6] Isotopic composition of Zn and Pb atmospheric depositions in an urban/periurban area of northeastern France
    Cloquet, Christophe
    Carignan, Jean
    Libourel, Guy
    [J]. ENVIRONMENTAL SCIENCE & TECHNOLOGY, 2006, 40 (21) : 6594 - 6600
  • [7] de Andrade Lima LR. P., 2012, ENVIRON EARTH SCI, V68, P1033
  • [8] Use of isotope ratios to assess sources of Pb and Zn dispersed in the environment during mining and ore processing within the Orlovka-Spokoinoe mining site (Russia)
    Dolgopolova, A
    Weiss, DJ
    Seltmann, R
    Kober, B
    Mason, TFD
    Coles, B
    Stanley, CJ
    [J]. APPLIED GEOCHEMISTRY, 2006, 21 (04) : 563 - 579
  • [9] Zinc isotope fractionation during adsorption to calcite at high and low ionic strength
    Dong, Shuofei
    Wasylenki, Laura E.
    [J]. CHEMICAL GEOLOGY, 2016, 447 : 70 - 78
  • [10] Leaching of lead metallurgical slag in citric solutions -: implications for disposal and weathering in soil environments
    Ettler, V
    Komárková, M
    Jehlicka, J
    Coufal, P
    Hradil, D
    Machovic, V
    Delorme, F
    [J]. CHEMOSPHERE, 2004, 57 (07) : 567 - 577