Defective Carbon Nanotubes with Stone-Wales Defect Arrays

被引:1
|
作者
Jeong, Jinwoo [1 ]
Yoon, Young-Gui [1 ]
机构
[1] Chung Ang Univ, Dept Phys, Seoul 156756, South Korea
关键词
Carbon Nanotube; Stone-Wales; Defect; ION-BEAMS; ELECTRON; TUBULES;
D O I
10.1166/jnn.2011.4465
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Presented herein are the structural and electronic properties of defective (n, n) carbon nanotubes (CNTs) (n = 3, 4, 5, 6) and of a defective graphene sheet, obtained form first-principles calculations of their electronic band strucutres. CNTs are newly discovered nanostructures with promising electronic and structural properties desired for nanoscale device applications. To enhance their functionality, various methods, such as ion implantation and ion irradiation, have been suggested for the manipulation of single-wall CNTs (SWNTs). In this study, periodic Stone-Wales defect arrays were considered. Defective (n, n) CNTs and a defective graphene sheet were analyzed in terms of their geometries and defect formation energies. In particular, the defective (5, 5) CNT was compared with the C-60 fullerene and the perfect (5, 5) CNT in polygon structures and total energies. The electronic band structures via first-principles calculations were also analyzed. A significant difference was found between the electronic band structures determined via first-principles calculations and those determined with the use of a one-parameter tight-binding model.
引用
收藏
页码:6227 / 6232
页数:6
相关论文
共 50 条
  • [1] Conductance of carbon nanotubes with a Stone-Wales defect
    Matsumura, H
    Ando, T
    JOURNAL OF THE PHYSICAL SOCIETY OF JAPAN, 2001, 70 (09) : 2657 - 2665
  • [2] Antiresonance effect due to Stone-Wales defect in carbon nanotubes
    Yang, HT
    Yang, LF
    Chen, JW
    Dong, JM
    PHYSICS LETTERS A, 2004, 325 (3-4) : 287 - 293
  • [3] Silicon doping of defect sites in Stone-Wales defective carbon nanotubes: A density functional theory study
    Anafcheh, Maryam
    Ghafouri, Reza
    SUPERLATTICES AND MICROSTRUCTURES, 2013, 60 : 1 - 9
  • [4] Defect nucleation in carbon nanotubes under tension and torsion: Stone-Wales transformation
    Jiang, H
    Feng, XQ
    Huang, Y
    Hwang, KC
    Wu, PD
    COMPUTER METHODS IN APPLIED MECHANICS AND ENGINEERING, 2004, 193 (30-32) : 3419 - 3429
  • [5] Kinetics of Topological Stone-Wales Defect Formation in Single Walled Carbon Nanotubes
    Kabir, Mukul
    Van Vliet, Krystyn J.
    JOURNAL OF PHYSICAL CHEMISTRY C, 2016, 120 (03): : 1989 - 1993
  • [6] Topological description of the Stone-Wales defect formation energy in carbon nanotubes and graphene
    Ertekin, Elif
    Chrzan, D. C.
    Daw, Murray S.
    PHYSICAL REVIEW B, 2009, 79 (15):
  • [7] Carbon Doping of Defect Sites in Stone-Wales Defective Boron-nitride Nanotubes: A Density Functional Theory Study
    Anafcheh, Maryam
    Ghafouri, Reza
    JOURNAL OF CLUSTER SCIENCE, 2013, 24 (03) : 865 - 879
  • [8] Ni adsorption on Stone-Wales defect sites in single-wall carbon nanotubes
    Yang, Seong Ho
    Shin, Weon Ho
    Kang, Jeung Ku
    JOURNAL OF CHEMICAL PHYSICS, 2006, 125 (08):
  • [9] Theoretical investigation on nonlinear optical properties of carbon nanotubes with Stone-Wales defect rings
    Zhou, Zhong-Jun
    Yu, Guang-Tao
    Ma, Fang
    Huang, Xu-Ri
    Wu, Zhi-Jian
    Li, Zhi-Ru
    JOURNAL OF MATERIALS CHEMISTRY C, 2014, 2 (02) : 306 - 311
  • [10] Energetics of Stone-Wales Defects in 4 Å Carbon Nanotubes
    Wen, Y. W.
    Liu, H. J.
    Tan, X. J.
    Pan, L.
    Shi, J.
    JOURNAL OF NANOSCIENCE AND NANOTECHNOLOGY, 2010, 10 (04) : 2332 - 2335