Electrochemical noise analysis of the corrosion of high-purity Mg-Al alloys

被引:22
|
作者
Casajus, Paula [1 ]
Winzer, Nicholas [1 ]
机构
[1] Fraunhofer Inst Mech Mat IWM, D-79108 Freiburg, Germany
关键词
Magnesium; Alloy; Pitting corrosion; Passive films; AZ91D MAGNESIUM ALLOY; ATMOSPHERIC CORROSION; LOCALIZED CORROSION; BETA-PHASE; BEHAVIOR; MICROSTRUCTURE; RESISTANCE; AM50; AZ31; ND;
D O I
10.1016/j.corsci.2015.02.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Corrosion of high-purity Mg-Al alloys containing 3, 6 and 9 wt.% Al was investigated using electrochemical noise (EN) analysis. Changes in the EN signals were correlated with macroscopically observable events on the sample surfaces, which were recorded using time-lapse photography. Steady-state corrosion in all alloys was highly localised. For the Mg3%Al alloy, localised corrosion was preceeded by a period of general corrosion. The corrosion rate of the as-cast Mg9%Al alloy was less than those of the other materials but increased with solution annealing time. The results are consistent with strong galvanic coupling between Al-depleted and -enriched zones of the a-phase. (C) 2015 Elsevier Ltd. All rights reserved.
引用
收藏
页码:316 / 326
页数:11
相关论文
共 50 条
  • [41] Anelastic Phenomena in Mg-Al Alloys
    Nagarajan, D.
    Caceres, C. H.
    Griffiths, J. R.
    ACTA PHYSICA POLONICA A, 2012, 122 (03) : 501 - 504
  • [42] LASER CLADDING OF MG-AL ALLOYS
    WANG, AA
    SIRCAR, S
    MAZUMDER, J
    JOURNAL OF MATERIALS SCIENCE, 1993, 28 (19) : 5113 - 5122
  • [43] Calculated phase diagrams and the corrosion of die-cast Mg-Al alloys
    Liu, Ming
    Uggowitzer, Peter J.
    Nagasekhar, A. V.
    Schmutz, Patrik
    Easton, Mark
    Song, Guang-Ling
    Atrens, Andrej
    CORROSION SCIENCE, 2009, 51 (03) : 602 - 619
  • [44] Calculated phase diagrams, iron tolerance limits, and corrosion of Mg-Al alloys
    Ming Liu
    Peter J. Uggowitzer
    Patrik Schmutz
    Andrej Atrens
    JOM, 2008, 60 : 39 - 44
  • [45] Calculated phase diagrams, iron tolerance limits, and corrosion of Mg-Al alloys
    Liu, Ming
    Uggowitzer, Peter J.
    Schmutz, Patrik
    Atrens, Andrej
    JOM, 2008, 60 (12) : 39 - 44
  • [46] Corrosion products of field-exposed Mg-Al series magnesium alloys
    Liao, Jinsun
    Hotta, Makoto
    CORROSION SCIENCE, 2016, 112 : 276 - 288
  • [47] Grain refinement of high-purity Mg-Al alloy ingots and influences of minor amounts of iron and manganese on cast grain size
    Tamura, Y
    Haitani, T
    Yano, E
    Motegi, T
    Kono, N
    Sato, E
    MATERIALS TRANSACTIONS, 2002, 43 (11) : 2784 - 2788
  • [48] Effect of variations of Al content on microstructure and corrosion resistance of PEO coatings on Mg-Al alloys
    Wei, Fangfang
    Zhang, Wei
    Zhang, Tao
    Wang, Fuhui
    JOURNAL OF ALLOYS AND COMPOUNDS, 2017, 690 : 195 - 205
  • [49] THE ROLE OF HYDROGEN IN CORROSION FATIGUE OF HIGH-PURITY AL-ZN-MG EXPOSED TO WATER-VAPOR
    RICKER, RE
    DUQUETTE, DJ
    METALLURGICAL TRANSACTIONS A-PHYSICAL METALLURGY AND MATERIALS SCIENCE, 1988, 19 (07): : 1775 - 1783
  • [50] Corrosion behaviour of Mg-Al alloys with Al-11Si thermal spray coatings
    Pardo, A.
    Merino, M. C.
    Casajus, P.
    Mohedano, M.
    Arrabal, R.
    Matykina, E.
    MATERIALS AND CORROSION-WERKSTOFFE UND KORROSION, 2009, 60 (12): : 939 - 948