EFFECT OF DIFFERENT MIG WELDING MODES ON HARD-FACING OF INCONEL 718 ON 321 STAINLESS STEEL

被引:9
作者
Anbalagan, Karpagaraj [1 ]
Sarala, R. [2 ]
Manivannan [3 ]
Rosemary, Shobin Loukkose [4 ]
Priyadarshi, Hemant [5 ]
Cheepu, Muralimohan [6 ]
机构
[1] Natl Inst Technol Puducherry, Dept Mech Engn, Karaikal 609609, Puducherry, India
[2] Alagappa Chettiar Govt Coll Engn & Technol, Dept Mech Engn, Karaikkudi 630003, Tamil Nadu, India
[3] Karpagam Acad Higher Educ, Ctr Mat Sci, Coimbatore 641021, Tamil Nadu, India
[4] SRM Inst Sci & Technol SRMIST, Dept Phys, Tiruchirappalli Campus, Tiruchirappalli 621105, Tamil Nadu, India
[5] Natl Inst Technol Patna, Dept Mech Engn, Patna 800005, Bihar, India
[6] Super TIG Welding Co Ltd, Busan 46722, South Korea
关键词
Hard-facing; MIG welding; Inconel; 718; Overlay; HOT CRACKING; MECHANICAL-PROPERTIES; CORROSION; WIRE; SUPERALLOY; DILUTION; GTAW; MICROSTRUCTURE; PARAMETERS; GEOMETRY;
D O I
10.1142/S0218625X22501074
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In this study, the metal inert gas (MIG) welding process is taken to deposit the Inconel 718 material on 321 stainless steel. Various modes like the DC, DC-pulsed, and DC-wave-pulsed modes in MIG welding are used for depositing Inconel 718. The primary parameters such as the welding current (90-120 A) and speed (150-350 mm/min) are varied within the range for making the layer deposition over 321 stainless steel. After performing the layer deposition, the dilution, contact angle, and peak temperature are analyzed to find the optimal MIG welding mode. From the macrograph, very low dilution (7.44%) is identified for the DC mode. The most inferior contact angle (theta) of 49 degrees was measured for the DC-wave-pulsed mode. The simulation work predicted a peak temperature of 2800 degrees C for the DC mode. Considerable microstructure changes have occurred at the weld deposition (dendritic structure) and HAZ (grain coarsening) for all the three modes. At the top, interface, and HAZ locations, the microhardness obtained from the DC-pulsed mode is in between those of the DC and DC-wave-pulsed modes. Overall, the DC-pulsed mode is qualified for making the metal deposition and further work. For 50% overlap, defect-free 2-mm-thick layer depositions are made on the 321 stainless steel surfaces.
引用
收藏
页数:11
相关论文
共 44 条
[1]   Laser cladding of Inconel 625 wire for corrosion protection [J].
Abioye, T. E. ;
McCartney, D. G. ;
Clare, A. T. .
JOURNAL OF MATERIALS PROCESSING TECHNOLOGY, 2015, 217 :232-240
[2]   EFFECTS OF OVERLAP AND DEPOSITION TECHNIQUE ON WELD-BEAD SHAPE [J].
ALLEN, DJ ;
EARL, C .
METALS TECHNOLOGY, 1984, 11 (JUN) :242-248
[3]  
Anupamadev A.P., 2020, T INDIAN NATL ACAD E, V5, P581
[4]  
Bagger C., 2003, ICALEO, V2003, P302
[5]   Effect of dilution on micro hardness of Ni-Cr-B-Si alloy hardfaced on austenitic stainless steel plate for sodium-cooled fast reactor applications [J].
Balaguru, S. ;
Murali, Vela ;
Chellapandi, P. ;
Gupta, Manoj .
NUCLEAR ENGINEERING AND TECHNOLOGY, 2020, 52 (03) :589-596
[6]   Selection of welding process for hardfacing on carbon steels based on quantitative and qualitative factors [J].
Balasubramanian, V. ;
Varahamoorthy, R. ;
Ramachandran, C. S. ;
Muralidharan, C. .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2009, 40 (9-10) :887-897
[7]   Current mode effects on weld bead geometry and heat affected zone in pulsed wire arc additive manufacturing of Ti-6-4 and Inconel 718 [J].
Benakis, Michalis ;
Costanzo, Davide ;
Patran, Alin .
JOURNAL OF MANUFACTURING PROCESSES, 2020, 60 (60) :61-74
[8]   Study on Microstructure and Mechanical Properties of Laser Welded Dissimilar Joint of P91 Steel and INCOLOY 800HT Nickel Alloy [J].
Bhanu, Vishwa ;
Fydrych, Dariusz ;
Gupta, Ankur ;
Pandey, Chandan .
MATERIALS, 2021, 14 (19)
[9]   Fibre laser welding of dissimilar alloys of Ti-6Al-4V and Inconel 718 for aerospace applications [J].
Chen, Hui-Chi ;
Pinkerton, Andrew J. ;
Li, Lin .
INTERNATIONAL JOURNAL OF ADVANCED MANUFACTURING TECHNOLOGY, 2011, 52 (9-12) :977-987
[10]   Dendritic microstructure and hot cracking of laser additive manufactured Inconel 718 under improved base cooling [J].
Chen, Yuan ;
Lu, Fenggui ;
Zhang, Ke ;
Nie, Pulin ;
Hosseini, Seyed Reza Elmi ;
Feng, Kai ;
Li, Zhuguo .
JOURNAL OF ALLOYS AND COMPOUNDS, 2016, 670 :312-321