Corrosion evaluation of eutectic chloride molten salt for new generation of CSP plants. Part 1: Thermal treatment assessment

被引:53
作者
Fernandez, Angel G. [1 ]
Cabeza, Luisa F. [1 ]
机构
[1] Univ Lleida, INSPIRES Res Ctr, GREiA Res Grp, Pere De Cabrera S-N, Lleida 25001, Spain
基金
欧盟地平线“2020”;
关键词
Concentrated solar power; Thermal energy storage; Corrosion mitigation; Chloride molten salt; Thermal purification treatment; ALUMINA-FORMING ALLOYS; SOLAR POWER-PLANTS; DECOMPOSITION; RESISTANCE; BEHAVIOR; METALS;
D O I
10.1016/j.est.2019.101125
中图分类号
TE [石油、天然气工业]; TK [能源与动力工程];
学科分类号
0807 ; 0820 ;
摘要
The operating temperature of a steam turbine is limited to 565 degrees C by the molten nitrate heat-transfer fluid; therefore, a new molten salt chemistry is needed to increase the maximum operating temperature in the new generation of CSP plants and improve the thermal-to-electrical energy conversion efficiency in the turbine block, such as chloride molten salts. Nevertheless, the prevention of high-temperature corrosion on containment materials using chlorides plays a critical role and a corrosion mitigation plan is needed to achieve the target plant lifetime of 30 years. This paper presents a corrosion mitigation strategy focused on different thermal treatments performed in the eutectic ternary chloride molten salt composed by MgCl2/NaCl/KCl (55.1 wt.%/24.5 wt. %/20.4 wt.%). Corrosion rates were obtained through linear polarization resistance technique in a conventional commercial stainless steel (AISI 304) at 720 degrees C during 5 h of immersion after the different thermal treatments carried out. Scanning electron microscopy and XRD analysis were used to confirm the corrosion rates and corrosion layer proposed by electrochemical techniques, obtaining a minimum corrosion rate of 6.033 mm/year for the best thermal treatment performed.
引用
收藏
页数:7
相关论文
共 25 条
  • [1] Cole Galen, 2019, POTENTIAL ROLE CONCE
  • [2] Thermal decomposition studies on magnesium hydroxychlorides
    de Bakker, J.
    Peacey, J.
    Davis, B.
    [J]. CANADIAN METALLURGICAL QUARTERLY, 2012, 51 (04) : 419 - 423
  • [3] Ding W., 2018, SOLAR ENERGY MAT SOL, V184
  • [4] Molten chloride salts for next generation concentrated solar power plants: Mitigation strategies against corrosion of structural materials
    Ding, Wenjin
    Shi, Hao
    Jianu, Adrian
    Xiu, Yanlei
    Bonk, Alexander
    Weisenburger, Alfons
    Bauer, Thomas
    [J]. SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2019, 193 : 298 - 313
  • [5] Corrosion behavior of metallic alloys in molten chloride salts for thermal energy storage in concentrated solar power plants: A review
    Ding, Wenjin
    Bonk, Alexander
    Bauer, Thomas
    [J]. FRONTIERS OF CHEMICAL SCIENCE AND ENGINEERING, 2018, 12 (03) : 564 - 576
  • [6] Preparation of anhydrous magnesium chloride from ammonium magnesium chloride hexahydrate
    Eom, Hyoung-Choon
    Park, Hyungkyu
    Yoon, Ho-Sung
    [J]. ADVANCED POWDER TECHNOLOGY, 2010, 21 (02) : 125 - 130
  • [7] ANODIC CORROSION AND PASSIVATION BEHAVIOR OF SOME METALS IN MOLTEN LICL-KCL CONTAINING OXIDE IONS
    FENG, XK
    MELENDRES, CA
    [J]. JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1982, 129 (06) : 1245 - 1249
  • [8] Corrosion resistance of alumina forming alloys against molten chlorides for energy production. II: Electrochemical impedance spectroscopy under thermal cycling conditions
    Gomez-Vidal, J. C.
    Fernandez, A. G.
    Tirawat, R.
    Turchi, C.
    Huddleston, W.
    [J]. SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2017, 166 : 234 - 245
  • [9] Corrosion resistance of alumina-forming alloys against molten chlorides for energy production. I: Pre-oxidation treatment and isothermal corrosion tests
    Gomez-Vidal, J. C.
    Fernandez, A. G.
    Tirawat, R.
    Turchi, C.
    Huddleston, W.
    [J]. SOLAR ENERGY MATERIALS AND SOLAR CELLS, 2017, 166 : 222 - 233
  • [10] THE EFFECTS OF CHLORIDES, HYDROGEN-CHLORIDE, AND SULFUR-DIOXIDE IN THE OXIDATION OF STEELS BELOW DEPOSITS
    GRABKE, HJ
    REESE, E
    SPIEGEL, M
    [J]. CORROSION SCIENCE, 1995, 37 (07) : 1023 - 1043