Enhancement of oxidation resistance of CVD SiC coated Cf/C-SiC hybrid composite tubes processed through Si-infiltration

被引:20
作者
Mubina, Shaik [1 ,2 ]
Khanra, Asit Kumar [2 ]
Saha, Bhaskar Prasad [1 ]
机构
[1] Int Adv Res Ctr Powder Met & New Mat, Hyderabad, Telangana, India
[2] Natl Inst Technol, Dept Met & Mat Engn, Warangal, Telangana, India
关键词
C-f/C-SiC; SiC(CNF); Hybrid composite tubes; Liquid silicon infiltration; Chemical vapour deposition; Oxidation resistance; C/SIC COMPOSITES; MECHANICAL-PROPERTIES; ELECTROPHORETIC DEPOSITION; TRIBOLOGICAL PROPERTIES; SIC/SIC COMPOSITES; PASSIVE-OXIDATION; SILICON-CARBIDE; C/C COMPOSITES; MICROSTRUCTURE; FABRICATION;
D O I
10.1016/j.jallcom.2020.154107
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Carbon fiber reinforced SiC based composites show an excellent combination of physical, mechanical and thermal properties. The combination of these properties makes C-f/SiC composites a material of choice for high-temperature load-bearing applications. However, the high-temperature oxidation has been an issue for structural ceramic composites. The combined effect of passive and active oxidation at a different temperature, influencing the overall oxidation behavior of C-f/SiC composites, which is mainly influenced by the partial pressure of oxygen. Although constant research is ongoing to improve the oxidation resistance of C-f/SiC composites, the literature on the in-depth oxidation mechanism of SiC based composites is scant. In the present study, three different types of C-f/C-SiC hybrid composite tubes were fabricated by the liquid silicon infiltration process (LSI) to study the high temperatures oxidation behavior. The dense carbon nanofibers (CNF) containing silicon carbide composite tubes (SiC(CNF)) braided with long carbon fabric (C-f) of different braiding patterns were used as a base matrix material for LSI. Further, a dense and uniform cubic beta-SiC coating was applied on the surface of the above-mentioned hybrid composite tubes by using the chemical vapour deposition (CVD) technique to improve its oxidation resistance property. The oxidation behavior of bare C-f, C-f/C-SiC (LSI) composite and CVD- SiC coated C-f/C-SiC hybrid composite samples were examined separately from room temperature to 1450 degrees C in the air using thermogravimetric analysis (TGA). The exhibited residual mass of LSI composite and SiC coated hybrid composite samples was found to be 24% and 0.7% respectively. It is evident from the TG analysis that SiC coated hybrid composite samples exhibited the highest oxidation resistance amongst all the composites due to the formation of highly dense uniform coating. (C) 2020 Elsevier B.V. All rights reserved.
引用
收藏
页数:10
相关论文
共 45 条
[1]   Oxidation behaviour of SiC/SiC ceramic matrix composites in air [J].
Al Nasiri, Nasrin ;
Patra, Niranjan ;
Ni, Na ;
Jayaseelan, Daniel D. ;
Lee, William E. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2016, 36 (14) :3293-3302
[2]   Electroplating chromium on CVD SiC and SiCf-SiC advanced cladding via PyC compatibility coating [J].
Ang, Caen ;
Kemery, Craig ;
Katoh, Yutai .
JOURNAL OF NUCLEAR MATERIALS, 2018, 503 :245-249
[3]   A CRITICAL-EVALUATION OF INDENTATION TECHNIQUES FOR MEASURING FRACTURE-TOUGHNESS .1. DIRECT CRACK MEASUREMENTS [J].
ANSTIS, GR ;
CHANTIKUL, P ;
LAWN, BR ;
MARSHALL, DB .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1981, 64 (09) :533-538
[4]  
Anthony C.J., 2009, CHEM VAPOUR DEPOSITI
[5]  
Antonio V., 2017, CORROS SCI, V123, P129
[6]   A SiCnw/PyC-toughened ZrB2-SiC coating for protecting Si-SiC coated C/C composites against oxidation [J].
Cheng, Chunyu ;
Li, Hejun ;
Fu, Qiangang ;
Guo, Liping .
APPLIED SURFACE SCIENCE, 2018, 457 :360-366
[7]   Oxidation protection of C/C composites with a multilayer coating of SiC and Si plus SiC plus SiC nanowires [J].
Chu Yanhui ;
Li Hejun ;
Fu Qiangang ;
Wang Haipeng ;
Hou Xianghui ;
Zou Xu ;
Shang Gunan .
CARBON, 2012, 50 (03) :1280-1288
[8]   Electrophoretic deposition: From traditional ceramics to nanotechnology [J].
Corni, Ilaria ;
Ryan, Mary P. ;
Boccaccini, Aldo R. .
JOURNAL OF THE EUROPEAN CERAMIC SOCIETY, 2008, 28 (07) :1353-1367
[9]   In-situ growth of SiC nanostructures and their influence on anti-oxidation capability of C/SiC composites [J].
Dai, Jixiang ;
Sha, Jianjun ;
Shao, Junqi ;
Zu, Yufei ;
Lei, Mingkai ;
Flauder, Stefan ;
Langhof, Nico ;
Krenkel, Walter .
CORROSION SCIENCE, 2017, 124 :71-79
[10]   Ultra-high temperature ceramics: Materials for extreme environments [J].
Fahrenholtz, William G. ;
Hilmas, Greg E. .
SCRIPTA MATERIALIA, 2017, 129 :94-99