Microstructure and Tribology of Spark Plasma Sintered Fe-Cr-B Metamorphic Alloy Powder

被引:14
|
作者
Sorour, Ahmad A. [1 ]
Strauss, Holger W. [1 ]
Chromik, Richard R. [1 ]
Brochu, Mathieu [1 ]
机构
[1] McGill Univ, Dept Min & Mat Engn, Montreal, PQ H3A 2B2, Canada
关键词
Unlubricated wear; Adhesive wear; Oxidative wear; Borides; Ferrous alloys; Hardness; HIGH-CARBON STEELS; WEAR-RESISTANCE; METALLOGRAPHIC BEHAVIOR; HARDNESS; FRICTION;
D O I
10.1007/s11249-011-9845-z
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
The spark plasma sintering (SPS) process was used to fabricate a bulk Fe-Cr-B alloy (known as Armacor M) from gas-atomized powders. The purpose of this work is to study the microstructure, hardness and tribology of this sintered bulk alloy. Post microstructure and mechanical characterizations were performed to investigate the effects of wear on the microstructure and mechanical properties. Microstructural analysis using X-ray diffraction (XRD), scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) showed that SPS successfully produced a fully dense bulk material containing 67 vol.% Cr1.65Fe0.35B0.96 particles dispersed in 33 vol.% solid solution matrix consisting of Fe, Cr and Si. Using nanoindentation, the hardness of the Cr1.65Fe0.35B0.96 particles and the matrix was found to be 24 and 6 GPa, respectively. From microindentation, the bulk hardness of the sintered alloy was 9.7 GPa (991 HV). Dry sliding wear testing under mild conditions (i.e., initial Hertzian mean contact pressure of 280 MPa) was conducted against a stainless steel pin. The steady state coefficient of friction against Armacor M was about 0.82. The wear of Armacor M proceeded primarily by adhesive and mild oxidative wear. The wear volume for Armacor M was 80% less than that of carbon steel and its wear rate was 5.53 x 10(-6) mm(3) N-1 m(-1).
引用
收藏
页码:269 / 278
页数:10
相关论文
共 50 条
  • [41] Wear behavior of Fe-Cr-B alloys under dry sliding condition
    Cui, Gongjun
    Wei, Jin
    Wu, Gongxiong
    INDUSTRIAL LUBRICATION AND TRIBOLOGY, 2015, 67 (04) : 336 - 343
  • [42] Effect of Alloying Method on Microstructure and Wear Resistance of Fe-Cr-V-B Based Alloy
    Ma, Yu
    Liu, Ying
    Li, Jun
    Zhang, Hui
    Yang, Hao
    JOURNAL OF IRON AND STEEL RESEARCH INTERNATIONAL, 2016, 23 (06) : 625 - 632
  • [43] Microstructure, mechanical properties and toughening mechanism of directional Fe2B crystal in Fe-B alloy with trace Cr addition
    Jian, Yongxin
    Huang, Zhifu
    Liu, Xiaoting
    Sun, Jialin
    Xing, Jiandong
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2020, 57 : 172 - 179
  • [44] Grain growth kinetics and mechanical properties of spark plasma sintered Fe-15Cr-2W powders
    Verma, Lekhraj
    Dabhade, Vikram V.
    MATERIALS TODAY COMMUNICATIONS, 2023, 37
  • [45] The effect of Si on the microstructure and mechanical properties of spark plasma sintered boron carbide
    Ma, Luoning
    Xie, Kelvin Y.
    Toksoy, Muhammet F.
    Kuwelkar, Kanak
    Haber, Richard A.
    Hemker, Kevin J.
    MATERIALS CHARACTERIZATION, 2017, 134 : 274 - 278
  • [46] Effects of B contents on the microstructure and wear resistance of hypereutectic Fe-Cr-C hardfacing alloy coating
    Wang, Jibo
    Lu, Jianxiang
    Xing, Xiaolei
    Zhou, Yefei
    Liu, Shaocun
    Qi, Xiaowen
    Yang, Qingxiang
    MATERIALS RESEARCH EXPRESS, 2019, 6 (10)
  • [47] Improved corrosion resistance of Ni-modified Fe-Cr-B steel in molten zinc via phase transformation and microstructure control
    Wang, Mengmeng
    Gao, Rui
    Gao, Haiyan
    Zhou, Yang
    Fan, Yangyang
    Zhao, Yangyong
    Ju, Jiang
    Liu, Yahui
    Kang, Maodong
    Wang, Jun
    SURFACE & COATINGS TECHNOLOGY, 2019, 374 : 975 - 986
  • [48] Electric Erosion Induced Microstructure and Mechanical Properties in Spark Plasma Sintered Al-4.5 wt. % Cu Alloy
    Devaraj, S.
    Kumar, R.
    Sankaran, S.
    MATERIALS PERFORMANCE AND CHARACTERIZATION, 2016, 5 (01) : 54 - 65
  • [49] Influence of TiN dopant on microstructure of TiB2 ceramic sintered by spark plasma
    Shayesteh, Farzad
    Delbari, Seyed Ali
    Ahmadi, Zohre
    Shokouhimehr, Mohammadreza
    Asl, Mehdi Shahedi
    CERAMICS INTERNATIONAL, 2019, 45 (05) : 5306 - 5311
  • [50] Effect of quenching on microstructure and wear-resistance of Fe-10Cr-1.5B-2Al alloy
    Jiang, J.
    Fu, H.
    Zheng, L.
    Shu-Qi, G.
    Yue, M.
    Yong-ping, L.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2016, 47 (09) : 822 - 830