Brazing of 6061 aluminum alloy/Ti-6Al-4V using Al-Si-Cu-Ge filler metals

被引:69
|
作者
Chang, S. Y. [1 ]
Tsao, L. C. [2 ]
Lei, Y. H. [1 ]
Mao, S. M. [1 ]
Huang, C. H. [3 ]
机构
[1] Natl Yunlin Univ Sci & Technol, Dept Mech Engn, Touliu 64002, Yunlin, Taiwan
[2] Natl Pingtung Univ Sci & Technol, Dept Mat Engn, Neipu 91201, Pingtung, Taiwan
[3] Met Ind Res & Dev Ctr, Kaohsiung 81160, Taiwan
关键词
Brazing; Aluminum alloys; Ti-6Al-4V; Al-Si-Cu-Ge alloys; Rare-earth elements; MICROSTRUCTURE;
D O I
10.1016/j.jmatprotec.2011.07.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al-8.4Si-20Cu-10Ge and mixed rare-earth elements (Re) containing Al-8.4Si-20Cu-10Ge-0.1Re filler metals were used for brazing of 6061 aluminum alloy/Ti-6Al-4V. The addition of 20 wt.% copper and 10 wt.% germanium into the Al-12Si filler metal lowered the solidus temperature from 586 degrees C to 489 degrees C and the liquidus temperature from 592 degrees C to 513 degrees C. The addition of 0.1 wt.% rare-earth elements into Al-8.4Si-20Cu-10Ge alloy caused remarkable Al-rich phase refinement and transformed the needle-like Al2Cu intermetallic compounds into block-like shapes. Shear strengths of the 6061 aluminum alloy/Ti-6AI-4V joints with the two brazing filler metals. Al-8.4Si-20Cu-10Ge and Al-8.4S-20Cu-10Ge-0.1Re, varied insignificantly with brazing periods of 10-60 min. The average shear strength of the 6061 aluminum alloy/Ti-6Al-4V joints brazed with Al-8.4Si-20Cu-10Ge at 530 degrees C was about 20 MPa. Rare-earth elements appeared to improve the reaction of the Al-8.45i-20Cu-10Ge filler metal with Ti-6Al-4V. The joint shear strength of the 6061 aluminum alloy/TI-6Al-4V with Al-8.4Si-20Cu-10Ge-0.1 Re reached about 51 MPa. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:8 / 14
页数:7
相关论文
共 50 条
  • [41] The bonding of nickel foam to Ti-6Al-4V using Ti-Cu-Ni braze alloy
    Jarvis, T.
    Voice, W.
    Goodall, R.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2011, 528 (06): : 2592 - 2601
  • [42] Infrared vacuum brazing of Ti-6Al-4V and Nb using the Ti-15Cu-15Ni foil
    Liaw, D. W.
    Wu, Z. Y.
    Shiue, R. K.
    Chang, C. S.
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2007, 454 : 104 - 113
  • [43] Brazing of Al2O3 to Ti-6Al-4V alloy with in situ synthesized TiB-whisker-reinforced active brazing alloy
    Yang, Minxuan
    Lin, Tiesong
    He, Peng
    Huang, Yudong
    CERAMICS INTERNATIONAL, 2011, 37 (08) : 3029 - 3035
  • [44] Stress relaxation behavior of Ti-6Al-4V alloy
    Liu, Y
    Yin, ZD
    Zhu, JC
    Li, MW
    TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA, 2003, 13 (04) : 881 - 884
  • [45] Stress relaxation behavior of Ti-6Al-4V alloy
    刘勇
    尹钟大
    朱景川
    李明伟
    TransactionsofNonferrousMetalsSocietyofChina, 2003, (04) : 881 - 884
  • [46] Microstructural aspects of superplasticity in Ti-6Al-4V alloy
    Motyka, Maciej
    Sieniawski, Jan
    Ziaja, Waldemar
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2014, 599 : 57 - 63
  • [47] Laser Powder Cladding of Ti-6Al-4V / Alloy
    Ali, Samar Reda Al-Sayed
    Hussein, Abdel Hamid Ahmed
    Nofal, Adel Abdel Menam Saleh
    Elnaby, Salah Elden Ibrahim Hasseb
    Elgazzar, Haytham Abdelrafea
    Sabour, Hassan Abdel
    MATERIALS, 2017, 10 (10):
  • [48] Microstructure and properties of the oxynitrided Ti-6Al-4V alloy
    Moskalewicz, T.
    Zimowski, S.
    Kitano, Y.
    Wierzchon, T.
    Czyrska-Filemonowicz, A.
    KOVOVE MATERIALY-METALLIC MATERIALS, 2006, 44 (03): : 133 - 138
  • [49] Hydrogen Treatment of Cast Ti-6Al-4V Alloy
    张少卿
    潘峰
    JournalofMaterialsScience&Technology, 1990, (03) : 187 - 192
  • [50] BOUND METAL DEPOSITION OF Ti-6Al-4V ALLOY
    Tuncer, Nihan
    Reidy, John P.
    Jorgensen, Luke
    Bose, Animesh
    INTERNATIONAL JOURNAL OF POWDER METALLURGY, 2024, 60 (01):