Brazing of 6061 aluminum alloy/Ti-6Al-4V using Al-Si-Cu-Ge filler metals

被引:69
|
作者
Chang, S. Y. [1 ]
Tsao, L. C. [2 ]
Lei, Y. H. [1 ]
Mao, S. M. [1 ]
Huang, C. H. [3 ]
机构
[1] Natl Yunlin Univ Sci & Technol, Dept Mech Engn, Touliu 64002, Yunlin, Taiwan
[2] Natl Pingtung Univ Sci & Technol, Dept Mat Engn, Neipu 91201, Pingtung, Taiwan
[3] Met Ind Res & Dev Ctr, Kaohsiung 81160, Taiwan
关键词
Brazing; Aluminum alloys; Ti-6Al-4V; Al-Si-Cu-Ge alloys; Rare-earth elements; MICROSTRUCTURE;
D O I
10.1016/j.jmatprotec.2011.07.014
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Al-8.4Si-20Cu-10Ge and mixed rare-earth elements (Re) containing Al-8.4Si-20Cu-10Ge-0.1Re filler metals were used for brazing of 6061 aluminum alloy/Ti-6Al-4V. The addition of 20 wt.% copper and 10 wt.% germanium into the Al-12Si filler metal lowered the solidus temperature from 586 degrees C to 489 degrees C and the liquidus temperature from 592 degrees C to 513 degrees C. The addition of 0.1 wt.% rare-earth elements into Al-8.4Si-20Cu-10Ge alloy caused remarkable Al-rich phase refinement and transformed the needle-like Al2Cu intermetallic compounds into block-like shapes. Shear strengths of the 6061 aluminum alloy/Ti-6AI-4V joints with the two brazing filler metals. Al-8.4Si-20Cu-10Ge and Al-8.4S-20Cu-10Ge-0.1Re, varied insignificantly with brazing periods of 10-60 min. The average shear strength of the 6061 aluminum alloy/Ti-6Al-4V joints brazed with Al-8.4Si-20Cu-10Ge at 530 degrees C was about 20 MPa. Rare-earth elements appeared to improve the reaction of the Al-8.45i-20Cu-10Ge filler metal with Ti-6Al-4V. The joint shear strength of the 6061 aluminum alloy/TI-6Al-4V with Al-8.4Si-20Cu-10Ge-0.1 Re reached about 51 MPa. (C) 2011 Elsevier B.V. All rights reserved.
引用
收藏
页码:8 / 14
页数:7
相关论文
共 50 条
  • [21] Development of Zn-15Al-xZr filler metals for Brazing 6061 aluminum alloy to stainless steel
    Yang, Jinlong
    Xue, Songbai
    Xue, Peng
    Lv, Zhaoping
    Long, Weimin
    Zhang, Guanxing
    Zhang, Qingke
    He, Peng
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2016, 651 : 425 - 434
  • [22] Influence of Sr additions on microstructure and properties of Al-Si-Ge-Zn filler metal for brazing 6061 aluminum alloy
    Niu, Zhiwei
    Huang, Jihua
    Chen, Shuhai
    Zhao, Xingke
    JOURNAL OF MATERIALS RESEARCH, 2017, 32 (04) : 822 - 830
  • [23] Brazing of 5A01 aluminum alloy using Al-Cu-Si-Ni filler metal
    元琳琳
    史秀梅
    柳旭
    齐岳峰
    黄晓猛
    China Welding, 2018, 27 (04) : 41 - 45
  • [24] The microstructural observation of brazing Ti-6Al-4V and TZM using the BAg-8 braze alloy
    Chan, HY
    Liaw, DW
    Shiue, RK
    INTERNATIONAL JOURNAL OF REFRACTORY METALS & HARD MATERIALS, 2004, 22 (01) : 27 - 33
  • [25] Microstructural evolution of brazing Ti-6Al-4V and TZM using silver-based braze alloy
    Chan, HY
    Liaw, DW
    Shiue, RK
    MATERIALS LETTERS, 2004, 58 (7-8) : 1141 - 1146
  • [27] Joining of Zirconia and Ti-6Al-4V Using a Ti-based Amorphous Filler
    Liu, Yuhua
    Hu, Jiandong
    Zhang, Yaping
    Guo, Zuoxing
    Yang, Yue
    JOURNAL OF MATERIALS SCIENCE & TECHNOLOGY, 2011, 27 (07) : 653 - 658
  • [28] Microstructure of Ti-6Al-4V alloy
    Kim, Tae Wan
    Yoon, Yo Han
    Oh, Ho Ra
    Park, Jong Bum
    Lee, Jung-Il
    Ryu, Jeong Ho
    JOURNAL OF THE KOREAN CRYSTAL GROWTH AND CRYSTAL TECHNOLOGY, 2016, 26 (03): : 126 - 130
  • [29] Joining of Zirconia to Ti6Al4V Using Ag-Cu Sputter-Coated Ti Brazing Filler
    Simoes, Sonia
    Emadinia, Omid
    Tavares, Carlos Jose
    Guedes, Anibal
    METALS, 2022, 12 (02)
  • [30] Material characterization and corrosion behavior of hybrid coating Ti-Al-Si-Cu/Ti-6Al-4V compositeMaterialcharakterisierung und Korrosionsverhalten von hybridbeschichtetem Ti-Al-Si-Cu/Ti-6Al-4V Verbundwerkstoff
    Naidoo, L. C.
    Fatoba, O. S.
    Akinlabi, S. A.
    Mahamood, R. M.
    Shatalov, M. Y.
    Murashkin, E. V.
    Hassan, S.
    Akinlabi, E. T.
    MATERIALWISSENSCHAFT UND WERKSTOFFTECHNIK, 2020, 51 (06) : 766 - 773