A comparative study on constraint parameters for characterizing fracture toughness of X60 and X100 pipe steels

被引:4
|
作者
Qian, Cheng [1 ]
Liang, Jie [1 ]
Huang, Yifan [2 ]
Kang, Jidong [1 ]
Gianetto, James [1 ]
机构
[1] CanmetMATERIALS, 183 Longwood Rd South, Hamilton, ON L8P 0A5, Canada
[2] Candu Energy Inc, 2251 Speakman Dr, Mississauga, ON L5K 1B2, Canada
关键词
Fracture toughness; J-R curve; CTOD-R curve; Constraint effect; X60 and X100 pipe steels; CRACK BORDER FIELD; J-R CURVES; TIP FIELDS; TRIAXIALITY PARAMETER; INPLANE; SPECIMENS; FAMILY;
D O I
10.1016/j.engfailanal.2022.106617
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The fracture toughness resistance curve (e.g., J -R curve and crack tip opening displacement (CTOD) or delta-R curve) is important in facilitating strain-based design and integrity assessment of oil and gas pipelines, where influence of ground movement and presence of planar weld flaws must be accounted for. In the present study, duplicate single edge notched bend (SE(B)) and clamped single edge notched tension (SE(T)) specimens with two different initial crack lengths were tested at room temperature for longitudinally-oriented specimens machined from X60 and X100 pipe steels where the notch is along the through-thickness direction. The results showed the expected trends of higher fracture toughness resistance curves for shallow-cracked over deep -cracked specimen types and tension over bending loading modes. Eleven constraint parameters (i.e., Q(HRR), Q(SSY), Q(LM), Q(BM), A(2), A(2BM), h, T-z, C-p, A(p), V-p) were calculated based on 3-D finite element analysis for all tested SE(B) and SE(T) specimens. The results indicated that the shallow-cracked SE(B) specimens exhibit a constraint condition similar to the intrinsically low-constraint deep-cracked SE(T) specimens made of the X60 pipe steel. Among all of the constraint parameters, the A(p) parameter based on the equivalent plastic strain isoline was found to correlate the best to the material fracture toughness for currently tested specimens. Furthermore, a linear master curve between various critical fracture toughness values and A(p) parameter was obtained for all the tested specimens with different crack lengths, loading modes and pipe steels.
引用
收藏
页数:22
相关论文
共 12 条
  • [1] Constraint effect on fracture toughness resistance curves of an X60 pipe steel
    Qian, Cheng
    Liang, Jie
    Huang, Yifan
    Kang, Jidong
    Gianetto, James
    4TH INTERNATIONAL CONFERENCE ON STRUCTURAL INTEGRITY (ICSI 2021), 2022, 37 : 926 - 933
  • [2] Study on uniform parameters characterizing the crack-tip constraint effect of fracture toughness
    He, Guangwei
    Bao, Chen
    Cai, Lixun
    ENGINEERING FRACTURE MECHANICS, 2019, 222
  • [3] Influence of Constraint on J-resistance Curves for an X100 Pipe Steel
    Kang, Jidong
    Shen, Guowu
    Liang, Jie
    Gianetto, James
    20TH EUROPEAN CONFERENCE ON FRACTURE, 2014, 3 : 239 - 244
  • [4] SENSITIVITY TO HYDROGEN EMBRITTLEMENT OF X52, X70 and X100 PIPE STEELS
    Capelle, J.
    Pluvinage, G.
    NEW DEVELOPMENTS ON METALLURGY AND APPLICATIONS OF HIGH STRENGTH STEELS: BUENOS AIRES 2008, VOLS 1 AND 2, PROCEEDINGS,, 2008, : 1255 - 1262
  • [5] Role of crystallographic texture, delamination and constraint on anisotropy in fracture toughness of API X70 line pipe steels
    Chatterjee, Soumya
    Koley, Soumyajit
    Das Bakshi, Subhankar
    Shome, Mahadev
    MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2017, 708 : 254 - 266
  • [6] FRACTURE TOUGHNESS OF WELDED JOINTS OF X100 HIGH-STRENGTH PIPELINE STEEL
    Bi Zongyue
    Yang Jun
    Niu Jing
    Zhang Jianxun
    ACTA METALLURGICA SINICA, 2013, 49 (05) : 576 - 582
  • [7] Effects of Temperature and Crack Tip Constraint on Cleavage Fracture Toughness in the Weld Thermal Simulated X80 Pipeline Steels
    Xu, Jie
    Fan, Yu
    NEW AND ADVANCED MATERIALS, PTS 1 AND 2, 2011, 197-198 : 1595 - 1598
  • [8] Study on fracture of non-through crack bodies of X60 pipeline steel
    Dong, HR
    Guo, WL
    Yang, Z
    Lu, MX
    Zhao, XW
    Luo, JH
    ACTA METALLURGICA SINICA, 2001, 37 (06) : 579 - 584
  • [9] Determination of Fracture Toughness and KIC-CVN Correlations for BM, HAZ, and WB in API 5L X60 Pipeline
    S. Capula-Colindres
    G. Terán
    D. Angeles-Herrera
    J. C. Velázquez
    E. Torres-Santillán
    Arabian Journal for Science and Engineering, 2021, 46 : 7461 - 7469
  • [10] Assessing the effects of loading rate on fracture toughness of AISI 1020 and API 5L X80 steels with hydrogen charging: experimental and numeric simulation study
    Wang, Hantong
    Zhang, Ci
    Ma, Haonan
    Tong, Zhi
    Huang, Yibai
    Jin, Ying
    Su, Cheng
    Zheng, Wenyue
    ENGINEERING FRACTURE MECHANICS, 2025, 314