Properties of elastomeric calcium phosphate cement-chitosan composites

被引:74
作者
Takagi, S [1 ]
Chow, LC
Hirayama, S
Eichmiller, FC
机构
[1] Natl Inst Stand & Technol, Amer Dent Assoc Hlth Fdn, Paffenbarger Res Ctr, Div Polymers, Gaithersburg, MD 20899 USA
[2] Nihon Univ, Sch Dent, Tokyo 101, Japan
关键词
calcium phosphate cement; chitosan; chitosan derivatives; non-rigid; mechanical properties; tetracalcium phosphate; dicalcium phosphate anhydrous; hydroxyapatite;
D O I
10.1016/S0109-5641(03)00028-9
中图分类号
R78 [口腔科学];
学科分类号
1003 ;
摘要
Objective. Self-hardening calcium phosphate cements (CPC) have been shown to be efficacious in a number of clinical applications. For some applications it is desirable to have CPC in a non-rigid resorbable elastomeric matrix. In the present study, chitosan was evaluated as the matrix for preparing CPC-chitosan composites. Methods. Cement specimens were prepared by mixing CPC powder (an equimolar mixture of tetracalcium phosphate and dicalcium phosphate anhydrous) with a chitosan solution at a powder/liquid ratio of 2-2.5. The setting time was measured by a Gilmore needle method. A standard three-point flexural test was used to fracture the specimens at a crosshead speed of 0.5 mm/min. Powder X-ray diffraction analysis was used to determine the conversion of the CPC to hydroxyapatite. Results. The CPC-chitosan composites were more stable in water than conventional CPC. They did not disintegrate even when placed in water immediately after mixing. The CPC-chitosan paste hardened within 10 min in all cases. The 1 d mean flexural modulus (GPa) for the control CPC was 5.3 (0.3) (mean (standard deviation); n = 5), and that for CPC-chitosan composites were between 2.7 (0.3) and 4.7 (0.3). The 1 d mean flexural strength (MPa) for the control was 16.6 (1.9), and that for the CPC-chitosan ranged from 4.5 (0.5) and 12.0 (1.0) (n = 5). Chitosan did not interfere the conversion of CPC components to hydroxyapatite. Significance. This study demonstrates that CPC-chitosan composites are stable in a wet environment and have acceptable mechanical strengths for clinical applications. Published by Elsevier Ltd on behalf of Academy of Dental Materials.
引用
收藏
页码:797 / 804
页数:8
相关论文
共 30 条
[1]   OSTEOGENIC POTENTIAL OF NONVITAL TISSUES AND SYNTHETIC IMPLANT MATERIALS [J].
AMLER, MH .
JOURNAL OF PERIODONTOLOGY, 1987, 58 (11) :758-761
[2]  
*ASTM, 1984, F41778 ASTM
[3]   AN EVALUATION OF TRICALCIUM PHOSPHATE IMPLANTS IN HUMAN PERIODONTAL OSSEOUS DEFECTS OF 2 PATIENTS [J].
BALDOCK, WT ;
HUTCHENS, LH ;
MCFALL, WT ;
SIMPSON, DM .
JOURNAL OF PERIODONTOLOGY, 1985, 56 (01) :1-7
[4]   Hydroxyapatite cement implant for regeneration of periodontal osseous defects in humans [J].
Brown, GD ;
Mealey, BL ;
Nummikoski, PV ;
Bifano, SL ;
Waldrop, TC .
JOURNAL OF PERIODONTOLOGY, 1998, 69 (02) :146-157
[5]  
Cherng A, 1997, J BIOMED MATER RES, V35, P273, DOI 10.1002/(SICI)1097-4636(19970605)35:3<273::AID-JBM1>3.0.CO
[6]  
2-E
[7]   RIDGE AUGMENTATION USING SOLID AND POROUS HYDROXYLAPATITE PARTICLES WITH AND WITHOUT AUTOGENOUS BONE OR PLASTER [J].
FRAME, JW ;
ROUT, PGJ ;
BROWNE, RM .
JOURNAL OF ORAL AND MAXILLOFACIAL SURGERY, 1987, 45 (09) :771-777
[9]  
Fujikawa K, 1995, Dent Mater J, V14, P45
[10]   THE MECHANICAL-BEHAVIOR OF CANCELLOUS BONE [J].
GIBSON, LJ .
JOURNAL OF BIOMECHANICS, 1985, 18 (05) :317-&