Development of benchmark reduced activation ferritic/martensitic steels for fusion energy applications

被引:136
作者
Tanigawa, H. [1 ]
Gaganidze, E. [2 ]
Hirose, T. [1 ]
Ando, M. [1 ]
Zinkle, S. J. [3 ]
Lindau, R. [2 ]
Diegele, E. [4 ]
机构
[1] Natl Inst Quantum & Radiol Sci & Technol, Aomori, Japan
[2] Karlsruhe Inst Technol, Karlsruhe, Germany
[3] Univ Tennessee, Knoxville, TN USA
[4] EUROfusion, Garching, Germany
关键词
reduced activation ferritic/martenssitic steel; joining technologies; irradiation effects; 14 MeV neutron irradiation effects; mitigation methodology; FERRITIC-MARTENSITIC STEEL; CYCLE FATIGUE PROPERTIES; MASTER-CURVE ANALYSIS; MATERIALS DESIGN-DATA; IN-BEAM FATIGUE; MECHANICAL-PROPERTIES; F82H STEEL; MICROSTRUCTURAL EVOLUTION; NEUTRON-IRRADIATION; CORROSION BEHAVIOR;
D O I
10.1088/1741-4326/57/9/092004
中图分类号
O35 [流体力学]; O53 [等离子体物理学];
学科分类号
070204 ; 080103 ; 080704 ;
摘要
Reduced-activation ferritic/martensitic (RAFM) steel is the benchmark structural material for in-vessel components of fusion reactor. The current status of RAFM developments and evaluations is reviewed based on two leading RAFM steels, F82H and EUROFER-97. The applicability of various joining technologies for fabrication of fusion first wall and blanket structures, such as weld or diffusion bonding, is overviewed as well. The technical challenges and potential risks of utilizing RAFM steels as the structural material of in-vessel components are discussed, and possible mitigation methodology is introduced. The discussion suggests that deuterium-tritium fusion neutron irradiation effects currently need to be treated as an ambiguity factor which could be incorporated within the safety factor. The safety factor will be defined by the engineering design criteria which are not yet developed with regard to irradiation effects and some high temperature process, and the operating time condition of the in-vessel component will be defined by the condition at which those ambiguities due to neutron irradiation become too large to be acceptable, or by the critical condition at which 14 MeV fusion neutron irradiation effects is expected to become different from fission neutron irradiation effects.
引用
收藏
页数:13
相关论文
共 101 条
[91]   Effect of heat treatments on tensile properties of F82H steel irradiated by neutrons [J].
Wakai, E. ;
Ando, M. ;
Sawai, T. ;
Tanigawa, H. ;
Taguchi, T. ;
Stoller, R. E. ;
Yamamoto, T. ;
Kato, Y. ;
Takada, F. .
JOURNAL OF NUCLEAR MATERIALS, 2007, 367 (SPEC. ISS.) :74-80
[92]   Swelling behavior of F82H steel irradiated by triple/dual ion beams [J].
Wakai, E ;
Kikuchi, K ;
Yamamoto, S ;
Aruga, T ;
Ando, M ;
Tanigawa, H ;
Taguchi, T ;
Sawai, T ;
Oka, K ;
Ohnuki, S .
JOURNAL OF NUCLEAR MATERIALS, 2003, 318 :267-273
[93]   Effect of helium production on swelling of F82H irradiated in HFIR [J].
Wakai, E ;
Hashimoto, N ;
Miwa, Y ;
Robertson, JP ;
Klueh, RL ;
Shiba, K ;
Jistukawa, S .
JOURNAL OF NUCLEAR MATERIALS, 2000, 283 :799-805
[94]   Applicability of miniature size bend specimens to determine the master curve reference temperature T0 [J].
Wallin, K ;
Planman, T ;
Valo, M ;
Rintamaa, R .
ENGINEERING FRACTURE MECHANICS, 2001, 68 (11) :1265-1296
[95]   Failure behaviour of EUROFER 97 in the low-cycle fatigue region under multi-step loading [J].
Walter, M. ;
Aktaa, J. ;
Lerch, M. .
INTERNATIONAL JOURNAL OF FATIGUE, 2008, 30 (03) :568-573
[96]   An evaluation of helium embrittlement resistance of reduced activation martensitic steels [J].
Yamamoto, N ;
Murase, Y ;
Nagakawa, J .
FUSION ENGINEERING AND DESIGN, 2006, 81 (8-14) :1085-1090
[97]   Helium effects on microstructural evolution in tempered martensitic steels: In situ helium implanter studies in HFIR [J].
Yamamoto, T. ;
Odette, G. R. ;
Miao, P. ;
Edwards, D. J. ;
Kurtz, R. J. .
JOURNAL OF NUCLEAR MATERIALS, 2009, 386-88 :338-341
[98]   Multimodal options for materials research to advance the basis for fusion energy in the ITER era [J].
Zinkle, S. J. ;
Moeslang, A. ;
Muroga, T. ;
Tanigawa, H. .
NUCLEAR FUSION, 2013, 53 (10)
[99]  
[No title captured]
[100]  
[No title captured]